Creep behavior and microstructure evolution of directionally solidified superalloy IC10 at high temperature
The creep behavior of directionally solidified (DS) superalloy IC10 was investigated under 192 MPa and 218 MPa at 980 deg C. Under the testing conditions, the marked creep characteristic of die superalloy is that the creep curve has a short primary and secondary stage and a long tertiary stage. Anot...