The Physical Simulation On Extrusion Process Of Glass Fiber Composite Wire Coated By Lead

The method of manufacturing the composite wire by extruding lead to coated glass fiber is described. The different composite wire that diameter is from 0.5 to 1.0mm has been produced by two kinds of different extruding technology (getting wire along horizontal direction and getting wire along perpen...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Acta metallurgica sinica : English letters 2004-12, Vol.17 (6), p.940-944
Hauptverfasser: Sun, H F, Fang, W B, Han, F, He, W X, Wang, E D
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 944
container_issue 6
container_start_page 940
container_title Acta metallurgica sinica : English letters
container_volume 17
creator Sun, H F
Fang, W B
Han, F
He, W X
Wang, E D
description The method of manufacturing the composite wire by extruding lead to coated glass fiber is described. The different composite wire that diameter is from 0.5 to 1.0mm has been produced by two kinds of different extruding technology (getting wire along horizontal direction and getting wire along perpendicular direction). The optimal extruding technological parameter has been given in different extruding technology by the physical simulation (H: 300DGC, 550kN, 0.16mm. P. 300DGC, 215kN, 0.16mm). The effect on the coating, speed by other extruding technological parameters in the different extruding technology has been discussed. The extruding temperature and extruding force is higher, the coating speed is faster. It has been pointed, that the affection on the extruding technology by the extruding, temperature has also behaved as the extruding temperature rising up spontaneously. The reason for exiting the minimum extruding force and maximum extruding force also has been discussion in this paper. It is also important to the extruding process and coating speed that is the coating clearance.
format Article
fullrecord <record><control><sourceid>wanfang_jour_proqu</sourceid><recordid>TN_cdi_wanfang_journals_jsxb_e200406027</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><wanfj_id>jsxb_e200406027</wanfj_id><sourcerecordid>jsxb_e200406027</sourcerecordid><originalsourceid>FETCH-LOGICAL-p1647-9c259e5dbef81f232f48cc68e7524ac5ba402055168c52ddb2b1bf56de095afd3</originalsourceid><addsrcrecordid>eNqFjU9LwzAchntQcE6_Q056KiRpkjZHHdsUCh04EU8lf35xKV0zmxa3b7_KvHt63wce3vcqmRGMRZoTSW6S2xibiSjj-Sz53O4AbXan6I1q0Zvfj60afOhQ1aHlcejH-AubPhiIEVUOrVs1lZXX0KNF2B9C9AOgD9_DhGoAi55PqARl75Jrp9oI9385T95Xy-3iJS2r9eviqUwPRLA8lYZyCdxqcAVxNKOOFcaIAnJOmTJcK4Yp5pyIwnBqraaaaMeFBSy5cjabJ4-X3R_VOdV91U0Y-256rJt41DVQjBkWmOaT-XAxD334HiEO9d5HA22rOghjrKkURYal_F8sGMs5wdkZeJRo9g</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>28447510</pqid></control><display><type>article</type><title>The Physical Simulation On Extrusion Process Of Glass Fiber Composite Wire Coated By Lead</title><source>Alma/SFX Local Collection</source><creator>Sun, H F ; Fang, W B ; Han, F ; He, W X ; Wang, E D</creator><creatorcontrib>Sun, H F ; Fang, W B ; Han, F ; He, W X ; Wang, E D</creatorcontrib><description>The method of manufacturing the composite wire by extruding lead to coated glass fiber is described. The different composite wire that diameter is from 0.5 to 1.0mm has been produced by two kinds of different extruding technology (getting wire along horizontal direction and getting wire along perpendicular direction). The optimal extruding technological parameter has been given in different extruding technology by the physical simulation (H: 300DGC, 550kN, 0.16mm. P. 300DGC, 215kN, 0.16mm). The effect on the coating, speed by other extruding technological parameters in the different extruding technology has been discussed. The extruding temperature and extruding force is higher, the coating speed is faster. It has been pointed, that the affection on the extruding technology by the extruding, temperature has also behaved as the extruding temperature rising up spontaneously. The reason for exiting the minimum extruding force and maximum extruding force also has been discussion in this paper. It is also important to the extruding process and coating speed that is the coating clearance.</description><identifier>ISSN: 1006-7191</identifier><language>eng</language><publisher>School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China</publisher><ispartof>Acta metallurgica sinica : English letters, 2004-12, Vol.17 (6), p.940-944</ispartof><rights>Copyright © Wanfang Data Co. Ltd. All Rights Reserved.</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Uhttp://www.wanfangdata.com.cn/images/PeriodicalImages/jsxb-e/jsxb-e.jpg</thumbnail><link.rule.ids>314,776,780</link.rule.ids></links><search><creatorcontrib>Sun, H F</creatorcontrib><creatorcontrib>Fang, W B</creatorcontrib><creatorcontrib>Han, F</creatorcontrib><creatorcontrib>He, W X</creatorcontrib><creatorcontrib>Wang, E D</creatorcontrib><title>The Physical Simulation On Extrusion Process Of Glass Fiber Composite Wire Coated By Lead</title><title>Acta metallurgica sinica : English letters</title><description>The method of manufacturing the composite wire by extruding lead to coated glass fiber is described. The different composite wire that diameter is from 0.5 to 1.0mm has been produced by two kinds of different extruding technology (getting wire along horizontal direction and getting wire along perpendicular direction). The optimal extruding technological parameter has been given in different extruding technology by the physical simulation (H: 300DGC, 550kN, 0.16mm. P. 300DGC, 215kN, 0.16mm). The effect on the coating, speed by other extruding technological parameters in the different extruding technology has been discussed. The extruding temperature and extruding force is higher, the coating speed is faster. It has been pointed, that the affection on the extruding technology by the extruding, temperature has also behaved as the extruding temperature rising up spontaneously. The reason for exiting the minimum extruding force and maximum extruding force also has been discussion in this paper. It is also important to the extruding process and coating speed that is the coating clearance.</description><issn>1006-7191</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2004</creationdate><recordtype>article</recordtype><recordid>eNqFjU9LwzAchntQcE6_Q056KiRpkjZHHdsUCh04EU8lf35xKV0zmxa3b7_KvHt63wce3vcqmRGMRZoTSW6S2xibiSjj-Sz53O4AbXan6I1q0Zvfj60afOhQ1aHlcejH-AubPhiIEVUOrVs1lZXX0KNF2B9C9AOgD9_DhGoAi55PqARl75Jrp9oI9385T95Xy-3iJS2r9eviqUwPRLA8lYZyCdxqcAVxNKOOFcaIAnJOmTJcK4Yp5pyIwnBqraaaaMeFBSy5cjabJ4-X3R_VOdV91U0Y-256rJt41DVQjBkWmOaT-XAxD334HiEO9d5HA22rOghjrKkURYal_F8sGMs5wdkZeJRo9g</recordid><startdate>200412</startdate><enddate>200412</enddate><creator>Sun, H F</creator><creator>Fang, W B</creator><creator>Han, F</creator><creator>He, W X</creator><creator>Wang, E D</creator><general>School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China</general><scope>7QQ</scope><scope>7SR</scope><scope>8FD</scope><scope>JG9</scope><scope>7TB</scope><scope>FR3</scope><scope>2B.</scope><scope>4A8</scope><scope>92I</scope><scope>93N</scope><scope>PSX</scope><scope>TCJ</scope></search><sort><creationdate>200412</creationdate><title>The Physical Simulation On Extrusion Process Of Glass Fiber Composite Wire Coated By Lead</title><author>Sun, H F ; Fang, W B ; Han, F ; He, W X ; Wang, E D</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-p1647-9c259e5dbef81f232f48cc68e7524ac5ba402055168c52ddb2b1bf56de095afd3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2004</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Sun, H F</creatorcontrib><creatorcontrib>Fang, W B</creatorcontrib><creatorcontrib>Han, F</creatorcontrib><creatorcontrib>He, W X</creatorcontrib><creatorcontrib>Wang, E D</creatorcontrib><collection>Ceramic Abstracts</collection><collection>Engineered Materials Abstracts</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><collection>Mechanical &amp; Transportation Engineering Abstracts</collection><collection>Engineering Research Database</collection><collection>Wanfang Data Journals - Hong Kong</collection><collection>WANFANG Data Centre</collection><collection>Wanfang Data Journals</collection><collection>万方数据期刊 - 香港版</collection><collection>China Online Journals (COJ)</collection><collection>China Online Journals (COJ)</collection><jtitle>Acta metallurgica sinica : English letters</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Sun, H F</au><au>Fang, W B</au><au>Han, F</au><au>He, W X</au><au>Wang, E D</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>The Physical Simulation On Extrusion Process Of Glass Fiber Composite Wire Coated By Lead</atitle><jtitle>Acta metallurgica sinica : English letters</jtitle><date>2004-12</date><risdate>2004</risdate><volume>17</volume><issue>6</issue><spage>940</spage><epage>944</epage><pages>940-944</pages><issn>1006-7191</issn><abstract>The method of manufacturing the composite wire by extruding lead to coated glass fiber is described. The different composite wire that diameter is from 0.5 to 1.0mm has been produced by two kinds of different extruding technology (getting wire along horizontal direction and getting wire along perpendicular direction). The optimal extruding technological parameter has been given in different extruding technology by the physical simulation (H: 300DGC, 550kN, 0.16mm. P. 300DGC, 215kN, 0.16mm). The effect on the coating, speed by other extruding technological parameters in the different extruding technology has been discussed. The extruding temperature and extruding force is higher, the coating speed is faster. It has been pointed, that the affection on the extruding technology by the extruding, temperature has also behaved as the extruding temperature rising up spontaneously. The reason for exiting the minimum extruding force and maximum extruding force also has been discussion in this paper. It is also important to the extruding process and coating speed that is the coating clearance.</abstract><pub>School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China</pub><tpages>5</tpages></addata></record>
fulltext fulltext
identifier ISSN: 1006-7191
ispartof Acta metallurgica sinica : English letters, 2004-12, Vol.17 (6), p.940-944
issn 1006-7191
language eng
recordid cdi_wanfang_journals_jsxb_e200406027
source Alma/SFX Local Collection
title The Physical Simulation On Extrusion Process Of Glass Fiber Composite Wire Coated By Lead
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-21T10%3A19%3A26IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-wanfang_jour_proqu&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=The%20Physical%20Simulation%20On%20Extrusion%20Process%20Of%20Glass%20Fiber%20Composite%20Wire%20Coated%20By%20Lead&rft.jtitle=Acta%20metallurgica%20sinica%20:%20English%20letters&rft.au=Sun,%20H%20F&rft.date=2004-12&rft.volume=17&rft.issue=6&rft.spage=940&rft.epage=944&rft.pages=940-944&rft.issn=1006-7191&rft_id=info:doi/&rft_dat=%3Cwanfang_jour_proqu%3Ejsxb_e200406027%3C/wanfang_jour_proqu%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=28447510&rft_id=info:pmid/&rft_wanfj_id=jsxb_e200406027&rfr_iscdi=true