Large cohesive energy adsorbent for fluoride removal, preparation and application thereof

222633 3 3 The present disclosure provides a method for preparing a high cohesive energy adsorbent for fluoride removal, which includes the following steps: S1. adding NaHF-NiF·6HO additive to SiCO ceramic powder, and sintering at a temperature of 310-330° C. for 18-22h to obtain a sintered substanc...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: FUJIAN DEER TECHNOLOGY CO., LTD
Format: Patent
Sprache:eng
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:222633 3 3 The present disclosure provides a method for preparing a high cohesive energy adsorbent for fluoride removal, which includes the following steps: S1. adding NaHF-NiF·6HO additive to SiCO ceramic powder, and sintering at a temperature of 310-330° C. for 18-22h to obtain a sintered substance; S2. grinding the sintered substance to obtain particles with a size of 2-3 mm, and mixing the particles with polyacrylonitrile to form a composite polymer; and S3. molding the composite polymer by a vacuum baking process at a temperature of 75-85° C., then performing ball milling and sieving to obtain the high cohesive energy adsorbent for fluoride removal. The high cohesive energy adsorbent for fluoride removal may be used in the adsorption and separation of the CF-CHF-CClFmixture system, and the contents of CHFand CClFare lowered to less than 10ppmv.