Temperature-stable cast iron alloy and use of said alloy

A description is given of a temperature-stable cast-iron alloy having high wear resistance at temperatures between 500 and 900° C. The alloy is characterized in that it has the following composition expressed in weight percentages: chromium: 15.0-20.0%, carbon: 1.0-2.0%, manganese: 0.8-1.2%, silicon...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Karlsson, Asger, Kirkegaard Stage, Rasmus
Format: Patent
Sprache:eng
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Karlsson, Asger
Kirkegaard Stage, Rasmus
description A description is given of a temperature-stable cast-iron alloy having high wear resistance at temperatures between 500 and 900° C. The alloy is characterized in that it has the following composition expressed in weight percentages: chromium: 15.0-20.0%, carbon: 1.0-2.0%, manganese: 0.8-1.2%, silicon: 1.2-1.5%, nickel: 1.5-2.5%, balance iron and unavoidable metallic and non-metallic contaminants where the non-metallic contaminants comprise nitrogen, oxygen, phosphorous and sulphur. Hereby is obtained a cast-iron alloy which has a higher wear resistance and a reduced tendency to form the undesirable sigma phase when heated to temperatures between 500 and 900° C. as compared to the known allows.
format Patent
fullrecord <record><control><sourceid>uspatents_EFH</sourceid><recordid>TN_cdi_uspatents_grants_08202375</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>08202375</sourcerecordid><originalsourceid>FETCH-uspatents_grants_082023753</originalsourceid><addsrcrecordid>eNrjZLAISc0tSC1KLCktStUtLklMyklVSE4sLlHILMrPU0jMycmvVEjMS1EoLU5VyE9TKE7MTIGI8jCwpiXmFKfyQmluBgU31xBnD93S4oLEktS8kuL49KJEEGVgYWRgZGxuakyEEgC-LS7U</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Temperature-stable cast iron alloy and use of said alloy</title><source>USPTO Issued Patents</source><creator>Karlsson, Asger ; Kirkegaard Stage, Rasmus</creator><creatorcontrib>Karlsson, Asger ; Kirkegaard Stage, Rasmus ; FLSMIDTH A/S</creatorcontrib><description>A description is given of a temperature-stable cast-iron alloy having high wear resistance at temperatures between 500 and 900° C. The alloy is characterized in that it has the following composition expressed in weight percentages: chromium: 15.0-20.0%, carbon: 1.0-2.0%, manganese: 0.8-1.2%, silicon: 1.2-1.5%, nickel: 1.5-2.5%, balance iron and unavoidable metallic and non-metallic contaminants where the non-metallic contaminants comprise nitrogen, oxygen, phosphorous and sulphur. Hereby is obtained a cast-iron alloy which has a higher wear resistance and a reduced tendency to form the undesirable sigma phase when heated to temperatures between 500 and 900° C. as compared to the known allows.</description><language>eng</language><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://image-ppubs.uspto.gov/dirsearch-public/print/downloadPdf/8202375$$EPDF$$P50$$Guspatents$$Hfree_for_read</linktopdf><link.rule.ids>230,308,780,802,885,64039</link.rule.ids><linktorsrc>$$Uhttps://image-ppubs.uspto.gov/dirsearch-public/print/downloadPdf/8202375$$EView_record_in_USPTO$$FView_record_in_$$GUSPTO$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Karlsson, Asger</creatorcontrib><creatorcontrib>Kirkegaard Stage, Rasmus</creatorcontrib><creatorcontrib>FLSMIDTH A/S</creatorcontrib><title>Temperature-stable cast iron alloy and use of said alloy</title><description>A description is given of a temperature-stable cast-iron alloy having high wear resistance at temperatures between 500 and 900° C. The alloy is characterized in that it has the following composition expressed in weight percentages: chromium: 15.0-20.0%, carbon: 1.0-2.0%, manganese: 0.8-1.2%, silicon: 1.2-1.5%, nickel: 1.5-2.5%, balance iron and unavoidable metallic and non-metallic contaminants where the non-metallic contaminants comprise nitrogen, oxygen, phosphorous and sulphur. Hereby is obtained a cast-iron alloy which has a higher wear resistance and a reduced tendency to form the undesirable sigma phase when heated to temperatures between 500 and 900° C. as compared to the known allows.</description><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EFH</sourceid><recordid>eNrjZLAISc0tSC1KLCktStUtLklMyklVSE4sLlHILMrPU0jMycmvVEjMS1EoLU5VyE9TKE7MTIGI8jCwpiXmFKfyQmluBgU31xBnD93S4oLEktS8kuL49KJEEGVgYWRgZGxuakyEEgC-LS7U</recordid><startdate>20120619</startdate><enddate>20120619</enddate><creator>Karlsson, Asger</creator><creator>Kirkegaard Stage, Rasmus</creator><scope>EFH</scope></search><sort><creationdate>20120619</creationdate><title>Temperature-stable cast iron alloy and use of said alloy</title><author>Karlsson, Asger ; Kirkegaard Stage, Rasmus</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-uspatents_grants_082023753</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2012</creationdate><toplevel>online_resources</toplevel><creatorcontrib>Karlsson, Asger</creatorcontrib><creatorcontrib>Kirkegaard Stage, Rasmus</creatorcontrib><creatorcontrib>FLSMIDTH A/S</creatorcontrib><collection>USPTO Issued Patents</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Karlsson, Asger</au><au>Kirkegaard Stage, Rasmus</au><aucorp>FLSMIDTH A/S</aucorp><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Temperature-stable cast iron alloy and use of said alloy</title><date>2012-06-19</date><risdate>2012</risdate><abstract>A description is given of a temperature-stable cast-iron alloy having high wear resistance at temperatures between 500 and 900° C. The alloy is characterized in that it has the following composition expressed in weight percentages: chromium: 15.0-20.0%, carbon: 1.0-2.0%, manganese: 0.8-1.2%, silicon: 1.2-1.5%, nickel: 1.5-2.5%, balance iron and unavoidable metallic and non-metallic contaminants where the non-metallic contaminants comprise nitrogen, oxygen, phosphorous and sulphur. Hereby is obtained a cast-iron alloy which has a higher wear resistance and a reduced tendency to form the undesirable sigma phase when heated to temperatures between 500 and 900° C. as compared to the known allows.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_uspatents_grants_08202375
source USPTO Issued Patents
title Temperature-stable cast iron alloy and use of said alloy
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T17%3A09%3A30IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-uspatents_EFH&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Karlsson,%20Asger&rft.aucorp=FLSMIDTH%20A/S&rft.date=2012-06-19&rft_id=info:doi/&rft_dat=%3Cuspatents_EFH%3E08202375%3C/uspatents_EFH%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true