Method of manufacturing high-crush-strength iridium catalyst for hydrazine decomposition reaction in spacecraft thrusters using bauxite
Disclosed herein is a method for manufacturing a high-crush-strength iridium catalyst for hydrazine decomposition for spacecraft and satellite propulsion using bauxite, the method including: an acid treatment step of bringing bauxite into contact with a 0.1-10 M acid solution for 10-14 hr; a filtrat...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Disclosed herein is a method for manufacturing a high-crush-strength iridium catalyst for hydrazine decomposition for spacecraft and satellite propulsion using bauxite, the method including: an acid treatment step of bringing bauxite into contact with a 0.1-10 M acid solution for 10-14 hr; a filtration step of filtering the acid-treated bauxite as a solid to remove the remaining acid and impurities; a thermal treatment step of bringing the filtered bauxite into contact with hot air at a temperature of 500-700° C. for 2-6 hr; a catalyst loading step of loading an iridium catalyst onto the thermally treated bauxite; and a reduction step of reducing the catalyst of the catalyst-loaded bauxite. |
---|