Ultra-thin gate oxide through post decoupled plasma nitridation anneal

DPN (decoupled plasma nitridation) is used to improve robustness of ultra thin gate oxides. Conventionally, this is followed by an anneal in pure helium to remove structural defects in the oxide. However, annealing under these conditions has been found to cause a deterioration of the electrical perf...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Zhong, Dong, Tan, Yun, Ang, Chew, Zheng, Jia
Format: Patent
Sprache:eng
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Zhong, Dong
Tan, Yun
Ang, Chew
Zheng, Jia
description DPN (decoupled plasma nitridation) is used to improve robustness of ultra thin gate oxides. Conventionally, this is followed by an anneal in pure helium to remove structural defects in the oxide. However, annealing under these conditions has been found to cause a deterioration of the electrical performance of devices. This problem has been overcome by annealing, in a 1:4 oxygen-nitrogen mixture (1,050° C. at about 10 torr) instead of in helium or nitrogen oxide. This results in a gate oxide that is resistant to boron contamination without suffering any loss in its electrical properties.
format Patent
fullrecord <record><control><sourceid>uspatents_EFI</sourceid><recordid>TN_cdi_uspatents_applications_20030170956</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>20030170956</sourcerecordid><originalsourceid>FETCH-uspatents_applications_200301709563</originalsourceid><addsrcrecordid>eNqVjEEKwjAQAHPxIOof9uqhEC1aPIvFB-i5LM3aBtZNyG7A5yviBzzNZWaWrr-zFWxsjgITGkF6xUBgc0l1miEnNQg0ppqZAmRGfSJItBIDWkwCKELIa7d4ICttfly5bX-5na9N1fy5iumAOXMcv5EOe-9bv-v86XBs_3HfKmk67w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Ultra-thin gate oxide through post decoupled plasma nitridation anneal</title><source>USPTO Published Applications</source><creator>Zhong, Dong ; Tan, Yun ; Ang, Chew ; Zheng, Jia</creator><creatorcontrib>Zhong, Dong ; Tan, Yun ; Ang, Chew ; Zheng, Jia</creatorcontrib><description>DPN (decoupled plasma nitridation) is used to improve robustness of ultra thin gate oxides. Conventionally, this is followed by an anneal in pure helium to remove structural defects in the oxide. However, annealing under these conditions has been found to cause a deterioration of the electrical performance of devices. This problem has been overcome by annealing, in a 1:4 oxygen-nitrogen mixture (1,050° C. at about 10 torr) instead of in helium or nitrogen oxide. This results in a gate oxide that is resistant to boron contamination without suffering any loss in its electrical properties.</description><language>eng</language><creationdate>2003</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://image-ppubs.uspto.gov/dirsearch-public/print/downloadPdf/20030170956$$EPDF$$P50$$Guspatents$$Hfree_for_read</linktopdf><link.rule.ids>230,309,781,874,886,64064</link.rule.ids><linktorsrc>$$Uhttps://patentcenter.uspto.gov/applications/10091983$$EView_record_in_USPTO$$FView_record_in_$$GUSPTO$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Zhong, Dong</creatorcontrib><creatorcontrib>Tan, Yun</creatorcontrib><creatorcontrib>Ang, Chew</creatorcontrib><creatorcontrib>Zheng, Jia</creatorcontrib><title>Ultra-thin gate oxide through post decoupled plasma nitridation anneal</title><description>DPN (decoupled plasma nitridation) is used to improve robustness of ultra thin gate oxides. Conventionally, this is followed by an anneal in pure helium to remove structural defects in the oxide. However, annealing under these conditions has been found to cause a deterioration of the electrical performance of devices. This problem has been overcome by annealing, in a 1:4 oxygen-nitrogen mixture (1,050° C. at about 10 torr) instead of in helium or nitrogen oxide. This results in a gate oxide that is resistant to boron contamination without suffering any loss in its electrical properties.</description><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2003</creationdate><recordtype>patent</recordtype><sourceid>EFI</sourceid><recordid>eNqVjEEKwjAQAHPxIOof9uqhEC1aPIvFB-i5LM3aBtZNyG7A5yviBzzNZWaWrr-zFWxsjgITGkF6xUBgc0l1miEnNQg0ppqZAmRGfSJItBIDWkwCKELIa7d4ICttfly5bX-5na9N1fy5iumAOXMcv5EOe-9bv-v86XBs_3HfKmk67w</recordid><startdate>20030911</startdate><enddate>20030911</enddate><creator>Zhong, Dong</creator><creator>Tan, Yun</creator><creator>Ang, Chew</creator><creator>Zheng, Jia</creator><scope>EFI</scope></search><sort><creationdate>20030911</creationdate><title>Ultra-thin gate oxide through post decoupled plasma nitridation anneal</title><author>Zhong, Dong ; Tan, Yun ; Ang, Chew ; Zheng, Jia</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-uspatents_applications_200301709563</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2003</creationdate><toplevel>online_resources</toplevel><creatorcontrib>Zhong, Dong</creatorcontrib><creatorcontrib>Tan, Yun</creatorcontrib><creatorcontrib>Ang, Chew</creatorcontrib><creatorcontrib>Zheng, Jia</creatorcontrib><collection>USPTO Published Applications</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Zhong, Dong</au><au>Tan, Yun</au><au>Ang, Chew</au><au>Zheng, Jia</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Ultra-thin gate oxide through post decoupled plasma nitridation anneal</title><date>2003-09-11</date><risdate>2003</risdate><abstract>DPN (decoupled plasma nitridation) is used to improve robustness of ultra thin gate oxides. Conventionally, this is followed by an anneal in pure helium to remove structural defects in the oxide. However, annealing under these conditions has been found to cause a deterioration of the electrical performance of devices. This problem has been overcome by annealing, in a 1:4 oxygen-nitrogen mixture (1,050° C. at about 10 torr) instead of in helium or nitrogen oxide. This results in a gate oxide that is resistant to boron contamination without suffering any loss in its electrical properties.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_uspatents_applications_20030170956
source USPTO Published Applications
title Ultra-thin gate oxide through post decoupled plasma nitridation anneal
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-16T02%3A20%3A13IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-uspatents_EFI&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Zhong,%20Dong&rft.date=2003-09-11&rft_id=info:doi/&rft_dat=%3Cuspatents_EFI%3E20030170956%3C/uspatents_EFI%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true