Air-hardening, low to medium carbon steel for improved heat treatment

A steel to be air-hardened as part of heat treatments such as hardening-and-tempering, induction hardening, carburizing, carbonitriding or nitriding comprising, in weight %: 1 C 0.10-0.55; Si 0.97-2.03; Mn 1.14-1.83; Cr 0.00-1.65; Mo 0.36-0.58; and the balance Fe + impurities

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Olund, Patrik, Lund, Thore, Larsson, Staffan, Neuman, Peter, Rosch, Oliver
Format: Patent
Sprache:eng
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A steel to be air-hardened as part of heat treatments such as hardening-and-tempering, induction hardening, carburizing, carbonitriding or nitriding comprising, in weight %: 1 C 0.10-0.55; Si 0.97-2.03; Mn 1.14-1.83; Cr 0.00-1.65; Mo 0.36-0.58; and the balance Fe + impurities