METHOD FOR PREPARING Li4NbxTi5-xO12/C NANOCOMPOSITE AS AN ANODE MATERIAL FOR LI-ION BATTERIES

4x5-x1224x5-x12A method for preparing a LiNbTiO/C nanocomposite as anode material for lithium-ion batteries is disclosed, which includes the following steps: (a) obtaining a mixture of a lithium salt, niobium pentaoxide, titanium dioxide (TiO), and a carbon source in a selected stoichiometric ratio;...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: Hefei Guoxuan High-Tech Power Energy Co., Ltd
Format: Patent
Sprache:eng
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Hefei Guoxuan High-Tech Power Energy Co., Ltd
description 4x5-x1224x5-x12A method for preparing a LiNbTiO/C nanocomposite as anode material for lithium-ion batteries is disclosed, which includes the following steps: (a) obtaining a mixture of a lithium salt, niobium pentaoxide, titanium dioxide (TiO), and a carbon source in a selected stoichiometric ratio; (b) mixing the mixture in a dispersant to produce a slurry; (c) drying the slurry to produce a dried mixture; (d) treating the dried mixture under a protective atmosphere, according to a heating program to produce the LiNbTiO/C nanocomposite, wherein the heating program comprises: calcining the dried mixture at 600° C. for 2-6 hours, heating it at a rate of 2-20° C. per minute to 950-980° C., cooling it by natural cooling to 800-850° C., maintaining the temperature at 800-850° C. for 16 hours, and cooling it by natural cooling to room temperature.
format Patent
fullrecord <record><control><sourceid>uspatents_EFI</sourceid><recordid>TN_cdi_uspatents_applications_13485523</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>20120305856</sourcerecordid><originalsourceid>FETCH-uspatents_applications_134855233</originalsourceid><addsrcrecordid>eNrjZIj1dQ3x8HdRcPMPUggIcg1wDPL0c1fwyTTxS6oIyTTVrfA3NNJ3VvBz9PN39vcN8A_2DHFVcAxWcPQDIn8XVwVfxxDXIE9HH7AJPp66nv5-Ck6OISBB12AeBta0xJziVF4ozc2g5uYa4uyhW1pckFiSmldSHJ9YUJCTmZxYkpmfVxxvaGxiYWpqZGxMtEIAgwk4kg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PREPARING Li4NbxTi5-xO12/C NANOCOMPOSITE AS AN ANODE MATERIAL FOR LI-ION BATTERIES</title><source>USPTO Published Applications</source><creator>Hefei Guoxuan High-Tech Power Energy Co., Ltd</creator><creatorcontrib>Hefei Guoxuan High-Tech Power Energy Co., Ltd</creatorcontrib><description>4x5-x1224x5-x12A method for preparing a LiNbTiO/C nanocomposite as anode material for lithium-ion batteries is disclosed, which includes the following steps: (a) obtaining a mixture of a lithium salt, niobium pentaoxide, titanium dioxide (TiO), and a carbon source in a selected stoichiometric ratio; (b) mixing the mixture in a dispersant to produce a slurry; (c) drying the slurry to produce a dried mixture; (d) treating the dried mixture under a protective atmosphere, according to a heating program to produce the LiNbTiO/C nanocomposite, wherein the heating program comprises: calcining the dried mixture at 600° C. for 2-6 hours, heating it at a rate of 2-20° C. per minute to 950-980° C., cooling it by natural cooling to 800-850° C., maintaining the temperature at 800-850° C. for 16 hours, and cooling it by natural cooling to room temperature.</description><language>eng</language><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://image-ppubs.uspto.gov/dirsearch-public/print/downloadPdf/20120305856$$EPDF$$P50$$Guspatents$$Hfree_for_read</linktopdf><link.rule.ids>230,308,776,869,881,64032</link.rule.ids><linktorsrc>$$Uhttps://patentcenter.uspto.gov/applications/13485523$$EView_record_in_USPTO$$FView_record_in_$$GUSPTO$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Hefei Guoxuan High-Tech Power Energy Co., Ltd</creatorcontrib><title>METHOD FOR PREPARING Li4NbxTi5-xO12/C NANOCOMPOSITE AS AN ANODE MATERIAL FOR LI-ION BATTERIES</title><description>4x5-x1224x5-x12A method for preparing a LiNbTiO/C nanocomposite as anode material for lithium-ion batteries is disclosed, which includes the following steps: (a) obtaining a mixture of a lithium salt, niobium pentaoxide, titanium dioxide (TiO), and a carbon source in a selected stoichiometric ratio; (b) mixing the mixture in a dispersant to produce a slurry; (c) drying the slurry to produce a dried mixture; (d) treating the dried mixture under a protective atmosphere, according to a heating program to produce the LiNbTiO/C nanocomposite, wherein the heating program comprises: calcining the dried mixture at 600° C. for 2-6 hours, heating it at a rate of 2-20° C. per minute to 950-980° C., cooling it by natural cooling to 800-850° C., maintaining the temperature at 800-850° C. for 16 hours, and cooling it by natural cooling to room temperature.</description><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EFI</sourceid><recordid>eNrjZIj1dQ3x8HdRcPMPUggIcg1wDPL0c1fwyTTxS6oIyTTVrfA3NNJ3VvBz9PN39vcN8A_2DHFVcAxWcPQDIn8XVwVfxxDXIE9HH7AJPp66nv5-Ck6OISBB12AeBta0xJziVF4ozc2g5uYa4uyhW1pckFiSmldSHJ9YUJCTmZxYkpmfVxxvaGxiYWpqZGxMtEIAgwk4kg</recordid><startdate>20120531</startdate><enddate>20120531</enddate><creator>Hefei Guoxuan High-Tech Power Energy Co., Ltd</creator><scope>EFI</scope></search><sort><creationdate>20120531</creationdate><title>METHOD FOR PREPARING Li4NbxTi5-xO12/C NANOCOMPOSITE AS AN ANODE MATERIAL FOR LI-ION BATTERIES</title></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-uspatents_applications_134855233</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2012</creationdate><toplevel>online_resources</toplevel><creatorcontrib>Hefei Guoxuan High-Tech Power Energy Co., Ltd</creatorcontrib><collection>USPTO Published Applications</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><aucorp>Hefei Guoxuan High-Tech Power Energy Co., Ltd</aucorp><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PREPARING Li4NbxTi5-xO12/C NANOCOMPOSITE AS AN ANODE MATERIAL FOR LI-ION BATTERIES</title><date>2012-05-31</date><risdate>2012</risdate><abstract>4x5-x1224x5-x12A method for preparing a LiNbTiO/C nanocomposite as anode material for lithium-ion batteries is disclosed, which includes the following steps: (a) obtaining a mixture of a lithium salt, niobium pentaoxide, titanium dioxide (TiO), and a carbon source in a selected stoichiometric ratio; (b) mixing the mixture in a dispersant to produce a slurry; (c) drying the slurry to produce a dried mixture; (d) treating the dried mixture under a protective atmosphere, according to a heating program to produce the LiNbTiO/C nanocomposite, wherein the heating program comprises: calcining the dried mixture at 600° C. for 2-6 hours, heating it at a rate of 2-20° C. per minute to 950-980° C., cooling it by natural cooling to 800-850° C., maintaining the temperature at 800-850° C. for 16 hours, and cooling it by natural cooling to room temperature.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_uspatents_applications_13485523
source USPTO Published Applications
title METHOD FOR PREPARING Li4NbxTi5-xO12/C NANOCOMPOSITE AS AN ANODE MATERIAL FOR LI-ION BATTERIES
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-02T14%3A16%3A26IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-uspatents_EFI&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.aucorp=Hefei%20Guoxuan%20High-Tech%20Power%20Energy%20Co.,%20Ltd&rft.date=2012-05-31&rft_id=info:doi/&rft_dat=%3Cuspatents_EFI%3E20120305856%3C/uspatents_EFI%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true