Effects of WC ratios on bead size and crack initiation in forming WC-Co cemented carbides by the laser metal deposition

Enhancing the durability of molds, jigs, and tools is crucial for the industry, and one approach to achieve this is by forming a metallic layer with high hardness on their surfaces. Metallic layers with high hardness can be formed through laser metal deposition (LMD), which is one of the additive ma...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of laser applications 2023-11, Vol.35 (4)
Hauptverfasser: Yamashita, Yorihiro, Nakamura, Mitsuki, Kunimine, Takahiro, Sato, Yuji, Funada, Yoshinori, Tsukamoto, Masahiro
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue 4
container_start_page
container_title Journal of laser applications
container_volume 35
creator Yamashita, Yorihiro
Nakamura, Mitsuki
Kunimine, Takahiro
Sato, Yuji
Funada, Yoshinori
Tsukamoto, Masahiro
description Enhancing the durability of molds, jigs, and tools is crucial for the industry, and one approach to achieve this is by forming a metallic layer with high hardness on their surfaces. Metallic layers with high hardness can be formed through laser metal deposition (LMD), which is one of the additive manufacturing processes, using cemented carbide powder. However, crack initiation typically occurs inside cemented carbide layers formed by the LMD. Therefore, achieving a cladding process for cemented carbide layers without cracks is desired for practical applications. In this study, the effects of tungsten carbide (WC) ratios in WC-Co cemented carbide granulated powder on formed bead size and crack initiation during the LMD processing were investigated. The number of cracks generated during the LMD processing was evaluated using an acoustic emission (AE) technique. The number of burst-type AE signals generated was counted as the number of cracks. Seven types of WC-Co cemented carbide granulated powders with WC ratios ranging from 30.5 to 92 mass% were prepared. Beads were formed using each powder through the LMD, with AE signals being measured. In the case of a WC ratio of 42.9 mass% or less, no crack was observed. On the other hand, cracks were observed when the WC ratio was 53.9 mass% or greater, and the number of cracks increased with an increase in the WC ratio.
doi_str_mv 10.2351/7.0001101
format Article
fullrecord <record><control><sourceid>scitation_cross</sourceid><recordid>TN_cdi_scitation_primary_10_2351_7_0001101</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>jla</sourcerecordid><originalsourceid>FETCH-LOGICAL-c224t-2763d1bf997ac0ead59b78a8541feffc0965c34992c2a7e7d276a0a844056d763</originalsourceid><addsrcrecordid>eNp9kM1LxDAQxYMouK4e_A_mqtA1X23ao5T1Axa8KHoraTLR6LZdkoCsf71Zd8-e5g383mPmEXLJ6IKLkt2oBaWUMcqOyIw1oi6YqNVx1lTyQsjq7ZScxfiZGSWUnJHvpXNoUoTJwWsLQSc_5WWEHrWF6H8Q9GjBBG2-wI8--R0xZgluCoMf37OtaCcwOOCYMKM69N5ihH4L6QNhrSMGGDDpNVjcTNHvAs7JidPriBeHOScvd8vn9qFYPd0_trerwnAuU8FVJSzrXdMobWg-qWx6Veu6lMyhc4Y2VWmEbBpuuFaobDZoqmspaVnZbJ6Tq32uCVOMAV23CX7QYdsx2u0a61R3aCyz13s2Gp_-3vwH_gUcV2te</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Effects of WC ratios on bead size and crack initiation in forming WC-Co cemented carbides by the laser metal deposition</title><source>AIP Journals Complete</source><creator>Yamashita, Yorihiro ; Nakamura, Mitsuki ; Kunimine, Takahiro ; Sato, Yuji ; Funada, Yoshinori ; Tsukamoto, Masahiro</creator><creatorcontrib>Yamashita, Yorihiro ; Nakamura, Mitsuki ; Kunimine, Takahiro ; Sato, Yuji ; Funada, Yoshinori ; Tsukamoto, Masahiro</creatorcontrib><description>Enhancing the durability of molds, jigs, and tools is crucial for the industry, and one approach to achieve this is by forming a metallic layer with high hardness on their surfaces. Metallic layers with high hardness can be formed through laser metal deposition (LMD), which is one of the additive manufacturing processes, using cemented carbide powder. However, crack initiation typically occurs inside cemented carbide layers formed by the LMD. Therefore, achieving a cladding process for cemented carbide layers without cracks is desired for practical applications. In this study, the effects of tungsten carbide (WC) ratios in WC-Co cemented carbide granulated powder on formed bead size and crack initiation during the LMD processing were investigated. The number of cracks generated during the LMD processing was evaluated using an acoustic emission (AE) technique. The number of burst-type AE signals generated was counted as the number of cracks. Seven types of WC-Co cemented carbide granulated powders with WC ratios ranging from 30.5 to 92 mass% were prepared. Beads were formed using each powder through the LMD, with AE signals being measured. In the case of a WC ratio of 42.9 mass% or less, no crack was observed. On the other hand, cracks were observed when the WC ratio was 53.9 mass% or greater, and the number of cracks increased with an increase in the WC ratio.</description><identifier>ISSN: 1042-346X</identifier><identifier>EISSN: 1938-1387</identifier><identifier>DOI: 10.2351/7.0001101</identifier><identifier>CODEN: JLAPEN</identifier><language>eng</language><ispartof>Journal of laser applications, 2023-11, Vol.35 (4)</ispartof><rights>Author(s)</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><cites>FETCH-LOGICAL-c224t-2763d1bf997ac0ead59b78a8541feffc0965c34992c2a7e7d276a0a844056d763</cites><orcidid>0000-0003-4401-9638 ; 0000-0001-7225-6281</orcidid></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://pubs.aip.org/jla/article-lookup/doi/10.2351/7.0001101$$EHTML$$P50$$Gscitation$$Hfree_for_read</linktohtml><link.rule.ids>314,777,781,791,4498,27905,27906,76133</link.rule.ids></links><search><creatorcontrib>Yamashita, Yorihiro</creatorcontrib><creatorcontrib>Nakamura, Mitsuki</creatorcontrib><creatorcontrib>Kunimine, Takahiro</creatorcontrib><creatorcontrib>Sato, Yuji</creatorcontrib><creatorcontrib>Funada, Yoshinori</creatorcontrib><creatorcontrib>Tsukamoto, Masahiro</creatorcontrib><title>Effects of WC ratios on bead size and crack initiation in forming WC-Co cemented carbides by the laser metal deposition</title><title>Journal of laser applications</title><description>Enhancing the durability of molds, jigs, and tools is crucial for the industry, and one approach to achieve this is by forming a metallic layer with high hardness on their surfaces. Metallic layers with high hardness can be formed through laser metal deposition (LMD), which is one of the additive manufacturing processes, using cemented carbide powder. However, crack initiation typically occurs inside cemented carbide layers formed by the LMD. Therefore, achieving a cladding process for cemented carbide layers without cracks is desired for practical applications. In this study, the effects of tungsten carbide (WC) ratios in WC-Co cemented carbide granulated powder on formed bead size and crack initiation during the LMD processing were investigated. The number of cracks generated during the LMD processing was evaluated using an acoustic emission (AE) technique. The number of burst-type AE signals generated was counted as the number of cracks. Seven types of WC-Co cemented carbide granulated powders with WC ratios ranging from 30.5 to 92 mass% were prepared. Beads were formed using each powder through the LMD, with AE signals being measured. In the case of a WC ratio of 42.9 mass% or less, no crack was observed. On the other hand, cracks were observed when the WC ratio was 53.9 mass% or greater, and the number of cracks increased with an increase in the WC ratio.</description><issn>1042-346X</issn><issn>1938-1387</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2023</creationdate><recordtype>article</recordtype><recordid>eNp9kM1LxDAQxYMouK4e_A_mqtA1X23ao5T1Axa8KHoraTLR6LZdkoCsf71Zd8-e5g383mPmEXLJ6IKLkt2oBaWUMcqOyIw1oi6YqNVx1lTyQsjq7ZScxfiZGSWUnJHvpXNoUoTJwWsLQSc_5WWEHrWF6H8Q9GjBBG2-wI8--R0xZgluCoMf37OtaCcwOOCYMKM69N5ihH4L6QNhrSMGGDDpNVjcTNHvAs7JidPriBeHOScvd8vn9qFYPd0_trerwnAuU8FVJSzrXdMobWg-qWx6Veu6lMyhc4Y2VWmEbBpuuFaobDZoqmspaVnZbJ6Tq32uCVOMAV23CX7QYdsx2u0a61R3aCyz13s2Gp_-3vwH_gUcV2te</recordid><startdate>202311</startdate><enddate>202311</enddate><creator>Yamashita, Yorihiro</creator><creator>Nakamura, Mitsuki</creator><creator>Kunimine, Takahiro</creator><creator>Sato, Yuji</creator><creator>Funada, Yoshinori</creator><creator>Tsukamoto, Masahiro</creator><scope>AJDQP</scope><scope>AAYXX</scope><scope>CITATION</scope><orcidid>https://orcid.org/0000-0003-4401-9638</orcidid><orcidid>https://orcid.org/0000-0001-7225-6281</orcidid></search><sort><creationdate>202311</creationdate><title>Effects of WC ratios on bead size and crack initiation in forming WC-Co cemented carbides by the laser metal deposition</title><author>Yamashita, Yorihiro ; Nakamura, Mitsuki ; Kunimine, Takahiro ; Sato, Yuji ; Funada, Yoshinori ; Tsukamoto, Masahiro</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c224t-2763d1bf997ac0ead59b78a8541feffc0965c34992c2a7e7d276a0a844056d763</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2023</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Yamashita, Yorihiro</creatorcontrib><creatorcontrib>Nakamura, Mitsuki</creatorcontrib><creatorcontrib>Kunimine, Takahiro</creatorcontrib><creatorcontrib>Sato, Yuji</creatorcontrib><creatorcontrib>Funada, Yoshinori</creatorcontrib><creatorcontrib>Tsukamoto, Masahiro</creatorcontrib><collection>AIP Open Access Journals</collection><collection>CrossRef</collection><jtitle>Journal of laser applications</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Yamashita, Yorihiro</au><au>Nakamura, Mitsuki</au><au>Kunimine, Takahiro</au><au>Sato, Yuji</au><au>Funada, Yoshinori</au><au>Tsukamoto, Masahiro</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Effects of WC ratios on bead size and crack initiation in forming WC-Co cemented carbides by the laser metal deposition</atitle><jtitle>Journal of laser applications</jtitle><date>2023-11</date><risdate>2023</risdate><volume>35</volume><issue>4</issue><issn>1042-346X</issn><eissn>1938-1387</eissn><coden>JLAPEN</coden><abstract>Enhancing the durability of molds, jigs, and tools is crucial for the industry, and one approach to achieve this is by forming a metallic layer with high hardness on their surfaces. Metallic layers with high hardness can be formed through laser metal deposition (LMD), which is one of the additive manufacturing processes, using cemented carbide powder. However, crack initiation typically occurs inside cemented carbide layers formed by the LMD. Therefore, achieving a cladding process for cemented carbide layers without cracks is desired for practical applications. In this study, the effects of tungsten carbide (WC) ratios in WC-Co cemented carbide granulated powder on formed bead size and crack initiation during the LMD processing were investigated. The number of cracks generated during the LMD processing was evaluated using an acoustic emission (AE) technique. The number of burst-type AE signals generated was counted as the number of cracks. Seven types of WC-Co cemented carbide granulated powders with WC ratios ranging from 30.5 to 92 mass% were prepared. Beads were formed using each powder through the LMD, with AE signals being measured. In the case of a WC ratio of 42.9 mass% or less, no crack was observed. On the other hand, cracks were observed when the WC ratio was 53.9 mass% or greater, and the number of cracks increased with an increase in the WC ratio.</abstract><doi>10.2351/7.0001101</doi><tpages>7</tpages><orcidid>https://orcid.org/0000-0003-4401-9638</orcidid><orcidid>https://orcid.org/0000-0001-7225-6281</orcidid><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 1042-346X
ispartof Journal of laser applications, 2023-11, Vol.35 (4)
issn 1042-346X
1938-1387
language eng
recordid cdi_scitation_primary_10_2351_7_0001101
source AIP Journals Complete
title Effects of WC ratios on bead size and crack initiation in forming WC-Co cemented carbides by the laser metal deposition
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-19T16%3A52%3A57IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-scitation_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Effects%20of%20WC%20ratios%20on%20bead%20size%20and%20crack%20initiation%20in%20forming%20WC-Co%20cemented%20carbides%20by%20the%20laser%20metal%20deposition&rft.jtitle=Journal%20of%20laser%20applications&rft.au=Yamashita,%20Yorihiro&rft.date=2023-11&rft.volume=35&rft.issue=4&rft.issn=1042-346X&rft.eissn=1938-1387&rft.coden=JLAPEN&rft_id=info:doi/10.2351/7.0001101&rft_dat=%3Cscitation_cross%3Ejla%3C/scitation_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true