Modulating the extent of fast and slow boron-oxygen related degradation in Czochralski silicon by thermal annealing: Evidence of a single defect

The fast and slow boron-oxygen related degradation in p-type Czochralski silicon is often attributed to two separate defects due to the different time constants and the determination of different capture cross section ratios (k). However, a recent study using high lifetime samples demonstrated ident...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of applied physics 2017-02, Vol.121 (5)
Hauptverfasser: Kim, Moonyong, Abbott, Malcolm, Nampalli, Nitin, Wenham, Stuart, Stefani, Bruno, Hallam, Brett
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue 5
container_start_page
container_title Journal of applied physics
container_volume 121
creator Kim, Moonyong
Abbott, Malcolm
Nampalli, Nitin
Wenham, Stuart
Stefani, Bruno
Hallam, Brett
description The fast and slow boron-oxygen related degradation in p-type Czochralski silicon is often attributed to two separate defects due to the different time constants and the determination of different capture cross section ratios (k). However, a recent study using high lifetime samples demonstrated identical recombination properties for the fast and slow degradation and proposed an alternative hypothesis that these were in fact due to a single defect. The study presented in this article provides further experimental evidence to support the single defect hypothesis. Thermal annealing after light soaking is used to investigate the behaviour of subsequent boron-oxygen related degradation. Modifying the temperature and duration of dark annealing on pre-degraded samples is observed to alter the fraction of fast and slow degradation during subsequent illumination. Dark annealing at 173 °C for 60 s is shown to result in almost all degradation occurring during the fast time-scale, whereas annealing at 155 °C for 7 h causes all degradation to occur during the slow time-scale. This modulation occurs without changing the total extent of degradation or changing the capture cross-section ratio. The results are consistent with the fast decay being caused by defect formation from immediately available defect precursors after dark annealing, whereas the slow degradation is caused by the slow transformation of another species into the defect precursor species before the more rapid reaction of defect formation can proceed.
doi_str_mv 10.1063/1.4975685
format Article
fullrecord <record><control><sourceid>proquest_scita</sourceid><recordid>TN_cdi_scitation_primary_10_1063_1_4975685</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>2124541040</sourcerecordid><originalsourceid>FETCH-LOGICAL-c393t-8d620cb9d8239de57338c24aa77f4a65ee7042c991134b7b27d8b288b32782073</originalsourceid><addsrcrecordid>eNqdkM1KAzEUhYMoWKsL3yDgSmE0PzNN4k5K_YGKG10PmeROHR2TmqS19Sl8ZFMruHd14fKd78BB6JiSc0pG_IKel0pUI1ntoAElUhWiqsguGhDCaCGVUPvoIMYXQiiVXA3Q1723i16nzs1wegYMqwQuYd_iVseEtbM49v4DNz54V_jVegYOB8gJsNjCLGibw97hzuHxpzfPQffxtcOx6zuT3816ow1vus8uB7rPRZd4suwsOAObHp1ZN-sh21ow6RDttVkBR793iJ6uJ4_j22L6cHM3vpoWhiueCmlHjJhGWcm4slAJzqVhpdZCtKUeVQCClMwoRSkvG9EwYWXDpGw4E5IRwYfoZOudB_--gJjqF78ILlfWjLKyKikpSaZOt5QJPsYAbT0P3ZsO65qSejN4TevfwTN7tmWj6dLPKP-Dlz78gfXctvwbmaeP9w</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>2124541040</pqid></control><display><type>article</type><title>Modulating the extent of fast and slow boron-oxygen related degradation in Czochralski silicon by thermal annealing: Evidence of a single defect</title><source>Scitation (American Institute of Physics)</source><source>Alma/SFX Local Collection</source><creator>Kim, Moonyong ; Abbott, Malcolm ; Nampalli, Nitin ; Wenham, Stuart ; Stefani, Bruno ; Hallam, Brett</creator><creatorcontrib>Kim, Moonyong ; Abbott, Malcolm ; Nampalli, Nitin ; Wenham, Stuart ; Stefani, Bruno ; Hallam, Brett</creatorcontrib><description>The fast and slow boron-oxygen related degradation in p-type Czochralski silicon is often attributed to two separate defects due to the different time constants and the determination of different capture cross section ratios (k). However, a recent study using high lifetime samples demonstrated identical recombination properties for the fast and slow degradation and proposed an alternative hypothesis that these were in fact due to a single defect. The study presented in this article provides further experimental evidence to support the single defect hypothesis. Thermal annealing after light soaking is used to investigate the behaviour of subsequent boron-oxygen related degradation. Modifying the temperature and duration of dark annealing on pre-degraded samples is observed to alter the fraction of fast and slow degradation during subsequent illumination. Dark annealing at 173 °C for 60 s is shown to result in almost all degradation occurring during the fast time-scale, whereas annealing at 155 °C for 7 h causes all degradation to occur during the slow time-scale. This modulation occurs without changing the total extent of degradation or changing the capture cross-section ratio. The results are consistent with the fast decay being caused by defect formation from immediately available defect precursors after dark annealing, whereas the slow degradation is caused by the slow transformation of another species into the defect precursor species before the more rapid reaction of defect formation can proceed.</description><identifier>ISSN: 0021-8979</identifier><identifier>EISSN: 1089-7550</identifier><identifier>DOI: 10.1063/1.4975685</identifier><identifier>CODEN: JAPIAU</identifier><language>eng</language><publisher>Melville: American Institute of Physics</publisher><subject>Absorption cross sections ; Annealing ; Applied physics ; Boron ; Decay rate ; Defects ; Degradation ; Hypotheses ; Light ; Oxygen ; Precursors ; Silicon</subject><ispartof>Journal of applied physics, 2017-02, Vol.121 (5)</ispartof><rights>Author(s)</rights><rights>2017 Author(s). Published by AIP Publishing.</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c393t-8d620cb9d8239de57338c24aa77f4a65ee7042c991134b7b27d8b288b32782073</citedby><cites>FETCH-LOGICAL-c393t-8d620cb9d8239de57338c24aa77f4a65ee7042c991134b7b27d8b288b32782073</cites><orcidid>0000-0002-3860-5633</orcidid></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://pubs.aip.org/jap/article-lookup/doi/10.1063/1.4975685$$EHTML$$P50$$Gscitation$$H</linktohtml><link.rule.ids>314,776,780,790,4498,27901,27902,76126</link.rule.ids></links><search><creatorcontrib>Kim, Moonyong</creatorcontrib><creatorcontrib>Abbott, Malcolm</creatorcontrib><creatorcontrib>Nampalli, Nitin</creatorcontrib><creatorcontrib>Wenham, Stuart</creatorcontrib><creatorcontrib>Stefani, Bruno</creatorcontrib><creatorcontrib>Hallam, Brett</creatorcontrib><title>Modulating the extent of fast and slow boron-oxygen related degradation in Czochralski silicon by thermal annealing: Evidence of a single defect</title><title>Journal of applied physics</title><description>The fast and slow boron-oxygen related degradation in p-type Czochralski silicon is often attributed to two separate defects due to the different time constants and the determination of different capture cross section ratios (k). However, a recent study using high lifetime samples demonstrated identical recombination properties for the fast and slow degradation and proposed an alternative hypothesis that these were in fact due to a single defect. The study presented in this article provides further experimental evidence to support the single defect hypothesis. Thermal annealing after light soaking is used to investigate the behaviour of subsequent boron-oxygen related degradation. Modifying the temperature and duration of dark annealing on pre-degraded samples is observed to alter the fraction of fast and slow degradation during subsequent illumination. Dark annealing at 173 °C for 60 s is shown to result in almost all degradation occurring during the fast time-scale, whereas annealing at 155 °C for 7 h causes all degradation to occur during the slow time-scale. This modulation occurs without changing the total extent of degradation or changing the capture cross-section ratio. The results are consistent with the fast decay being caused by defect formation from immediately available defect precursors after dark annealing, whereas the slow degradation is caused by the slow transformation of another species into the defect precursor species before the more rapid reaction of defect formation can proceed.</description><subject>Absorption cross sections</subject><subject>Annealing</subject><subject>Applied physics</subject><subject>Boron</subject><subject>Decay rate</subject><subject>Defects</subject><subject>Degradation</subject><subject>Hypotheses</subject><subject>Light</subject><subject>Oxygen</subject><subject>Precursors</subject><subject>Silicon</subject><issn>0021-8979</issn><issn>1089-7550</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2017</creationdate><recordtype>article</recordtype><recordid>eNqdkM1KAzEUhYMoWKsL3yDgSmE0PzNN4k5K_YGKG10PmeROHR2TmqS19Sl8ZFMruHd14fKd78BB6JiSc0pG_IKel0pUI1ntoAElUhWiqsguGhDCaCGVUPvoIMYXQiiVXA3Q1723i16nzs1wegYMqwQuYd_iVseEtbM49v4DNz54V_jVegYOB8gJsNjCLGibw97hzuHxpzfPQffxtcOx6zuT3816ow1vus8uB7rPRZd4suwsOAObHp1ZN-sh21ow6RDttVkBR793iJ6uJ4_j22L6cHM3vpoWhiueCmlHjJhGWcm4slAJzqVhpdZCtKUeVQCClMwoRSkvG9EwYWXDpGw4E5IRwYfoZOudB_--gJjqF78ILlfWjLKyKikpSaZOt5QJPsYAbT0P3ZsO65qSejN4TevfwTN7tmWj6dLPKP-Dlz78gfXctvwbmaeP9w</recordid><startdate>20170207</startdate><enddate>20170207</enddate><creator>Kim, Moonyong</creator><creator>Abbott, Malcolm</creator><creator>Nampalli, Nitin</creator><creator>Wenham, Stuart</creator><creator>Stefani, Bruno</creator><creator>Hallam, Brett</creator><general>American Institute of Physics</general><scope>AAYXX</scope><scope>CITATION</scope><scope>8FD</scope><scope>H8D</scope><scope>L7M</scope><orcidid>https://orcid.org/0000-0002-3860-5633</orcidid></search><sort><creationdate>20170207</creationdate><title>Modulating the extent of fast and slow boron-oxygen related degradation in Czochralski silicon by thermal annealing: Evidence of a single defect</title><author>Kim, Moonyong ; Abbott, Malcolm ; Nampalli, Nitin ; Wenham, Stuart ; Stefani, Bruno ; Hallam, Brett</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c393t-8d620cb9d8239de57338c24aa77f4a65ee7042c991134b7b27d8b288b32782073</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2017</creationdate><topic>Absorption cross sections</topic><topic>Annealing</topic><topic>Applied physics</topic><topic>Boron</topic><topic>Decay rate</topic><topic>Defects</topic><topic>Degradation</topic><topic>Hypotheses</topic><topic>Light</topic><topic>Oxygen</topic><topic>Precursors</topic><topic>Silicon</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Kim, Moonyong</creatorcontrib><creatorcontrib>Abbott, Malcolm</creatorcontrib><creatorcontrib>Nampalli, Nitin</creatorcontrib><creatorcontrib>Wenham, Stuart</creatorcontrib><creatorcontrib>Stefani, Bruno</creatorcontrib><creatorcontrib>Hallam, Brett</creatorcontrib><collection>CrossRef</collection><collection>Technology Research Database</collection><collection>Aerospace Database</collection><collection>Advanced Technologies Database with Aerospace</collection><jtitle>Journal of applied physics</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Kim, Moonyong</au><au>Abbott, Malcolm</au><au>Nampalli, Nitin</au><au>Wenham, Stuart</au><au>Stefani, Bruno</au><au>Hallam, Brett</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Modulating the extent of fast and slow boron-oxygen related degradation in Czochralski silicon by thermal annealing: Evidence of a single defect</atitle><jtitle>Journal of applied physics</jtitle><date>2017-02-07</date><risdate>2017</risdate><volume>121</volume><issue>5</issue><issn>0021-8979</issn><eissn>1089-7550</eissn><coden>JAPIAU</coden><abstract>The fast and slow boron-oxygen related degradation in p-type Czochralski silicon is often attributed to two separate defects due to the different time constants and the determination of different capture cross section ratios (k). However, a recent study using high lifetime samples demonstrated identical recombination properties for the fast and slow degradation and proposed an alternative hypothesis that these were in fact due to a single defect. The study presented in this article provides further experimental evidence to support the single defect hypothesis. Thermal annealing after light soaking is used to investigate the behaviour of subsequent boron-oxygen related degradation. Modifying the temperature and duration of dark annealing on pre-degraded samples is observed to alter the fraction of fast and slow degradation during subsequent illumination. Dark annealing at 173 °C for 60 s is shown to result in almost all degradation occurring during the fast time-scale, whereas annealing at 155 °C for 7 h causes all degradation to occur during the slow time-scale. This modulation occurs without changing the total extent of degradation or changing the capture cross-section ratio. The results are consistent with the fast decay being caused by defect formation from immediately available defect precursors after dark annealing, whereas the slow degradation is caused by the slow transformation of another species into the defect precursor species before the more rapid reaction of defect formation can proceed.</abstract><cop>Melville</cop><pub>American Institute of Physics</pub><doi>10.1063/1.4975685</doi><tpages>10</tpages><orcidid>https://orcid.org/0000-0002-3860-5633</orcidid></addata></record>
fulltext fulltext
identifier ISSN: 0021-8979
ispartof Journal of applied physics, 2017-02, Vol.121 (5)
issn 0021-8979
1089-7550
language eng
recordid cdi_scitation_primary_10_1063_1_4975685
source Scitation (American Institute of Physics); Alma/SFX Local Collection
subjects Absorption cross sections
Annealing
Applied physics
Boron
Decay rate
Defects
Degradation
Hypotheses
Light
Oxygen
Precursors
Silicon
title Modulating the extent of fast and slow boron-oxygen related degradation in Czochralski silicon by thermal annealing: Evidence of a single defect
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-11T22%3A41%3A13IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_scita&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Modulating%20the%20extent%20of%20fast%20and%20slow%20boron-oxygen%20related%20degradation%20in%20Czochralski%20silicon%20by%20thermal%20annealing:%20Evidence%20of%20a%20single%20defect&rft.jtitle=Journal%20of%20applied%20physics&rft.au=Kim,%20Moonyong&rft.date=2017-02-07&rft.volume=121&rft.issue=5&rft.issn=0021-8979&rft.eissn=1089-7550&rft.coden=JAPIAU&rft_id=info:doi/10.1063/1.4975685&rft_dat=%3Cproquest_scita%3E2124541040%3C/proquest_scita%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=2124541040&rft_id=info:pmid/&rfr_iscdi=true