Surface wrinkling by chemical modification of poly(dimethylsiloxane)-based networks during sputtering

Wrinkling is an important mechanical phenomenon that generates periodic topographical patterns across a surface. This paper presents experimental evidence that surface wrinkles, which form consequent to thin film magnetron sputtering of either indium tin oxide (ITO) or aluminum on poly(dimethylsilox...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Soft matter 2013-01, Vol.9 (32), p.7797-783
Hauptverfasser: Casper, Michelle D, Gzen, Arif, Dickey, Michael D, Genzer, Jan, Maria, Jon-Paul
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 783
container_issue 32
container_start_page 7797
container_title Soft matter
container_volume 9
creator Casper, Michelle D
Gzen, Arif
Dickey, Michael D
Genzer, Jan
Maria, Jon-Paul
description Wrinkling is an important mechanical phenomenon that generates periodic topographical patterns across a surface. This paper presents experimental evidence that surface wrinkles, which form consequent to thin film magnetron sputtering of either indium tin oxide (ITO) or aluminum on poly(dimethylsiloxane) networks (PDMS-N) made from a commercial Sylgard-184 kit, result from chemical modification of the PDMS-N surface as opposed to extrinsic thermomechanical stresses originating from differential thermal expansion. X-ray photoelectron spectroscopy results reveal that the PDMS-N surface becomes depleted in carbon and concurrently enriched in oxygen relative to silicon due to sputtering. This silica-like surface layer possesses intrinsic compressive stress that leads to wrinkle formation during the first 5 seconds of sputtering. The wrinkles maintain their periodicity irrespective of the thickness of the ITO film formed during subsequent deposition. Furthermore, upon removal of the ITO layer, the wrinkles persist with their periodicity unchanged. A narrow sputtering pressure window between 2 and 12 mTorr generates wrinkles. Pressures below this range cannot sustain a radio frequency plasma, while pressures above this range provide sufficient thermalization of kinetic energy as to eliminate the energetic bombardment that modifies the PDMS-N. This study provides a new understanding of the origins of wrinkling in sputtered films on polymeric substrates and creates opportunities to manipulate the topography produced by spontaneous surface wrinkling. Wrinkling is an important mechanical phenomenon that generates periodic topographical patterns across a surface.
doi_str_mv 10.1039/c3sm50966d
format Article
fullrecord <record><control><sourceid>proquest_rsc_p</sourceid><recordid>TN_cdi_rsc_primary_c3sm50966d</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>1429892615</sourcerecordid><originalsourceid>FETCH-LOGICAL-c378t-a4142faebdf6ff948c0883a660162b7e84e51e672a2105dbc41338b52a305b4d3</originalsourceid><addsrcrecordid>eNp9kM1LwzAYxoMoOKcX70K8TaGaNGmaHmX4BQMPKngraT5cXNrUpGX2v7djMvHi6f3B8-Ph5QHgFKMrjEhxLUmsM1QwpvbABOeUJoxTvr9j8nYIjmL8QIhwitkE6Oc-GCE1XAfbrJxt3mE1QLnUtZXCwdora0bqrG-gN7D1bpgpW-tuObhonf8Sjb5IKhG1go3u1j6sIlR92BTFtu86vcFjcGCEi_rk507B693ty_whWTzdP85vFokkOe8SQTFNjdCVMsyYgnKJOCeCMYRZWuWaU51hzfJUpBhlqpIUE8KrLBUEZRVVZApm2942-M9ex66sbZTaufFL38dyrC94kTKcjerlVpXBxxi0KdtgaxGGEqNys2X5u-Uon23lEOXO-5Of_5eXrTLkG2A2fx4</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1429892615</pqid></control><display><type>article</type><title>Surface wrinkling by chemical modification of poly(dimethylsiloxane)-based networks during sputtering</title><source>Royal Society Of Chemistry Journals 2008-</source><source>Alma/SFX Local Collection</source><creator>Casper, Michelle D ; Gzen, Arif ; Dickey, Michael D ; Genzer, Jan ; Maria, Jon-Paul</creator><creatorcontrib>Casper, Michelle D ; Gzen, Arif ; Dickey, Michael D ; Genzer, Jan ; Maria, Jon-Paul</creatorcontrib><description>Wrinkling is an important mechanical phenomenon that generates periodic topographical patterns across a surface. This paper presents experimental evidence that surface wrinkles, which form consequent to thin film magnetron sputtering of either indium tin oxide (ITO) or aluminum on poly(dimethylsiloxane) networks (PDMS-N) made from a commercial Sylgard-184 kit, result from chemical modification of the PDMS-N surface as opposed to extrinsic thermomechanical stresses originating from differential thermal expansion. X-ray photoelectron spectroscopy results reveal that the PDMS-N surface becomes depleted in carbon and concurrently enriched in oxygen relative to silicon due to sputtering. This silica-like surface layer possesses intrinsic compressive stress that leads to wrinkle formation during the first 5 seconds of sputtering. The wrinkles maintain their periodicity irrespective of the thickness of the ITO film formed during subsequent deposition. Furthermore, upon removal of the ITO layer, the wrinkles persist with their periodicity unchanged. A narrow sputtering pressure window between 2 and 12 mTorr generates wrinkles. Pressures below this range cannot sustain a radio frequency plasma, while pressures above this range provide sufficient thermalization of kinetic energy as to eliminate the energetic bombardment that modifies the PDMS-N. This study provides a new understanding of the origins of wrinkling in sputtered films on polymeric substrates and creates opportunities to manipulate the topography produced by spontaneous surface wrinkling. Wrinkling is an important mechanical phenomenon that generates periodic topographical patterns across a surface.</description><identifier>ISSN: 1744-683X</identifier><identifier>EISSN: 1744-6848</identifier><identifier>DOI: 10.1039/c3sm50966d</identifier><language>eng</language><subject>Carbon ; Indium tin oxide ; Magnetron sputtering ; Networks ; Sputtering ; Stresses ; Thermal expansion ; Wrinkling</subject><ispartof>Soft matter, 2013-01, Vol.9 (32), p.7797-783</ispartof><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c378t-a4142faebdf6ff948c0883a660162b7e84e51e672a2105dbc41338b52a305b4d3</citedby><cites>FETCH-LOGICAL-c378t-a4142faebdf6ff948c0883a660162b7e84e51e672a2105dbc41338b52a305b4d3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,778,782,27907,27908</link.rule.ids></links><search><creatorcontrib>Casper, Michelle D</creatorcontrib><creatorcontrib>Gzen, Arif</creatorcontrib><creatorcontrib>Dickey, Michael D</creatorcontrib><creatorcontrib>Genzer, Jan</creatorcontrib><creatorcontrib>Maria, Jon-Paul</creatorcontrib><title>Surface wrinkling by chemical modification of poly(dimethylsiloxane)-based networks during sputtering</title><title>Soft matter</title><description>Wrinkling is an important mechanical phenomenon that generates periodic topographical patterns across a surface. This paper presents experimental evidence that surface wrinkles, which form consequent to thin film magnetron sputtering of either indium tin oxide (ITO) or aluminum on poly(dimethylsiloxane) networks (PDMS-N) made from a commercial Sylgard-184 kit, result from chemical modification of the PDMS-N surface as opposed to extrinsic thermomechanical stresses originating from differential thermal expansion. X-ray photoelectron spectroscopy results reveal that the PDMS-N surface becomes depleted in carbon and concurrently enriched in oxygen relative to silicon due to sputtering. This silica-like surface layer possesses intrinsic compressive stress that leads to wrinkle formation during the first 5 seconds of sputtering. The wrinkles maintain their periodicity irrespective of the thickness of the ITO film formed during subsequent deposition. Furthermore, upon removal of the ITO layer, the wrinkles persist with their periodicity unchanged. A narrow sputtering pressure window between 2 and 12 mTorr generates wrinkles. Pressures below this range cannot sustain a radio frequency plasma, while pressures above this range provide sufficient thermalization of kinetic energy as to eliminate the energetic bombardment that modifies the PDMS-N. This study provides a new understanding of the origins of wrinkling in sputtered films on polymeric substrates and creates opportunities to manipulate the topography produced by spontaneous surface wrinkling. Wrinkling is an important mechanical phenomenon that generates periodic topographical patterns across a surface.</description><subject>Carbon</subject><subject>Indium tin oxide</subject><subject>Magnetron sputtering</subject><subject>Networks</subject><subject>Sputtering</subject><subject>Stresses</subject><subject>Thermal expansion</subject><subject>Wrinkling</subject><issn>1744-683X</issn><issn>1744-6848</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2013</creationdate><recordtype>article</recordtype><recordid>eNp9kM1LwzAYxoMoOKcX70K8TaGaNGmaHmX4BQMPKngraT5cXNrUpGX2v7djMvHi6f3B8-Ph5QHgFKMrjEhxLUmsM1QwpvbABOeUJoxTvr9j8nYIjmL8QIhwitkE6Oc-GCE1XAfbrJxt3mE1QLnUtZXCwdora0bqrG-gN7D1bpgpW-tuObhonf8Sjb5IKhG1go3u1j6sIlR92BTFtu86vcFjcGCEi_rk507B693ty_whWTzdP85vFokkOe8SQTFNjdCVMsyYgnKJOCeCMYRZWuWaU51hzfJUpBhlqpIUE8KrLBUEZRVVZApm2942-M9ex66sbZTaufFL38dyrC94kTKcjerlVpXBxxi0KdtgaxGGEqNys2X5u-Uon23lEOXO-5Of_5eXrTLkG2A2fx4</recordid><startdate>20130101</startdate><enddate>20130101</enddate><creator>Casper, Michelle D</creator><creator>Gzen, Arif</creator><creator>Dickey, Michael D</creator><creator>Genzer, Jan</creator><creator>Maria, Jon-Paul</creator><scope>AAYXX</scope><scope>CITATION</scope><scope>7QF</scope><scope>7U5</scope><scope>8FD</scope><scope>JG9</scope><scope>L7M</scope></search><sort><creationdate>20130101</creationdate><title>Surface wrinkling by chemical modification of poly(dimethylsiloxane)-based networks during sputtering</title><author>Casper, Michelle D ; Gzen, Arif ; Dickey, Michael D ; Genzer, Jan ; Maria, Jon-Paul</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c378t-a4142faebdf6ff948c0883a660162b7e84e51e672a2105dbc41338b52a305b4d3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2013</creationdate><topic>Carbon</topic><topic>Indium tin oxide</topic><topic>Magnetron sputtering</topic><topic>Networks</topic><topic>Sputtering</topic><topic>Stresses</topic><topic>Thermal expansion</topic><topic>Wrinkling</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Casper, Michelle D</creatorcontrib><creatorcontrib>Gzen, Arif</creatorcontrib><creatorcontrib>Dickey, Michael D</creatorcontrib><creatorcontrib>Genzer, Jan</creatorcontrib><creatorcontrib>Maria, Jon-Paul</creatorcontrib><collection>CrossRef</collection><collection>Aluminium Industry Abstracts</collection><collection>Solid State and Superconductivity Abstracts</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><collection>Advanced Technologies Database with Aerospace</collection><jtitle>Soft matter</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Casper, Michelle D</au><au>Gzen, Arif</au><au>Dickey, Michael D</au><au>Genzer, Jan</au><au>Maria, Jon-Paul</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Surface wrinkling by chemical modification of poly(dimethylsiloxane)-based networks during sputtering</atitle><jtitle>Soft matter</jtitle><date>2013-01-01</date><risdate>2013</risdate><volume>9</volume><issue>32</issue><spage>7797</spage><epage>783</epage><pages>7797-783</pages><issn>1744-683X</issn><eissn>1744-6848</eissn><abstract>Wrinkling is an important mechanical phenomenon that generates periodic topographical patterns across a surface. This paper presents experimental evidence that surface wrinkles, which form consequent to thin film magnetron sputtering of either indium tin oxide (ITO) or aluminum on poly(dimethylsiloxane) networks (PDMS-N) made from a commercial Sylgard-184 kit, result from chemical modification of the PDMS-N surface as opposed to extrinsic thermomechanical stresses originating from differential thermal expansion. X-ray photoelectron spectroscopy results reveal that the PDMS-N surface becomes depleted in carbon and concurrently enriched in oxygen relative to silicon due to sputtering. This silica-like surface layer possesses intrinsic compressive stress that leads to wrinkle formation during the first 5 seconds of sputtering. The wrinkles maintain their periodicity irrespective of the thickness of the ITO film formed during subsequent deposition. Furthermore, upon removal of the ITO layer, the wrinkles persist with their periodicity unchanged. A narrow sputtering pressure window between 2 and 12 mTorr generates wrinkles. Pressures below this range cannot sustain a radio frequency plasma, while pressures above this range provide sufficient thermalization of kinetic energy as to eliminate the energetic bombardment that modifies the PDMS-N. This study provides a new understanding of the origins of wrinkling in sputtered films on polymeric substrates and creates opportunities to manipulate the topography produced by spontaneous surface wrinkling. Wrinkling is an important mechanical phenomenon that generates periodic topographical patterns across a surface.</abstract><doi>10.1039/c3sm50966d</doi><tpages>7</tpages></addata></record>
fulltext fulltext
identifier ISSN: 1744-683X
ispartof Soft matter, 2013-01, Vol.9 (32), p.7797-783
issn 1744-683X
1744-6848
language eng
recordid cdi_rsc_primary_c3sm50966d
source Royal Society Of Chemistry Journals 2008-; Alma/SFX Local Collection
subjects Carbon
Indium tin oxide
Magnetron sputtering
Networks
Sputtering
Stresses
Thermal expansion
Wrinkling
title Surface wrinkling by chemical modification of poly(dimethylsiloxane)-based networks during sputtering
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-17T05%3A19%3A02IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_rsc_p&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Surface%20wrinkling%20by%20chemical%20modification%20of%20poly(dimethylsiloxane)-based%20networks%20during%20sputtering&rft.jtitle=Soft%20matter&rft.au=Casper,%20Michelle%20D&rft.date=2013-01-01&rft.volume=9&rft.issue=32&rft.spage=7797&rft.epage=783&rft.pages=7797-783&rft.issn=1744-683X&rft.eissn=1744-6848&rft_id=info:doi/10.1039/c3sm50966d&rft_dat=%3Cproquest_rsc_p%3E1429892615%3C/proquest_rsc_p%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1429892615&rft_id=info:pmid/&rfr_iscdi=true