Influence of Lanthanum-Doped Tungsten Wire Drawing Process on Microstructure and Properties
A reasonable preparation processing of Lanthanum-doped tungsten wire plays a decisive role in the final properties of the wire. This paper gives the optimum drawing process parameters of lanthanum-doped tungsten wire with φ1.00 mm–φ0.50 mm and explains the phenomenon of coarsening of fiber-like grai...
Gespeichert in:
Veröffentlicht in: | Materials 2022-07, Vol.15 (14), p.4979 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | 14 |
container_start_page | 4979 |
container_title | Materials |
container_volume | 15 |
creator | Wang, Luyan Yu, Yueguang Zhang, Peng Yang, Jiancan |
description | A reasonable preparation processing of Lanthanum-doped tungsten wire plays a decisive role in the final properties of the wire. This paper gives the optimum drawing process parameters of lanthanum-doped tungsten wire with φ1.00 mm–φ0.50 mm and explains the phenomenon of coarsening of fiber-like grains in the preparation processing of tungsten wire. The final optimum process parameters of lanthanum-doped tungsten wire are given: the temperature is 950 °C (the first pass temperature is 950 °C, and the temperature decreases by about 20 °C for each pass), the compression ratio is 15%, mold temperature is 550 °C, because of the limitation of equipment conditions, the wire drawing speed is fixed at 0.19 m/s. It is found that the fiber-like grains of the tungsten wire coarsen when the temperature is too high, and it is prone to breakage when the temperature is too low during the drawing process. When the compression ratio is too high (for example, 22%), there is a negative impact on the surface quality and the straightness of the tungsten wire. When the compression ratio is too low, the processing die time is increased, and the production cost is increased. |
doi_str_mv | 10.3390/ma15144979 |
format | Article |
fullrecord | <record><control><sourceid>proquest_pubme</sourceid><recordid>TN_cdi_pubmedcentral_primary_oai_pubmedcentral_nih_gov_9323575</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>2694039655</sourcerecordid><originalsourceid>FETCH-LOGICAL-c383t-ea3a38354b9d341e9e3db12bbf3035e0b007d0f8f3d2a1d3f92b3c173db082733</originalsourceid><addsrcrecordid>eNpdkU1LxDAQhoMoKqsXf0HBiwjVpJO2yUUQ14-FFT0oHjyEtJ2ulTZZk0bx39uyi19zmYH34WVmXkIOGD0BkPS00yxlnMtcbpBdJmUWM8n55q95h-x7_0qHAmAikdtkB1IhBOfZLnmemboNaEqMbB3NtelftAldPLVLrKKHYBa-RxM9NQ6jqdMfjVlE986W6H1kTXTblM763oWyDwOhTTWqS3R9g36PbNW69bi_7hPyeHX5cHETz--uZxfn87gEAX2MGvQwpLyQFXCGEqEqWFIUNVBIkRaU5hWtRQ1VolkFtUwKKFk-UFQkOcCEnK18l6HosCrR9E63aumaTrtPZXWj_iqmeVEL-64kJJDm6WBwtDZw9i2g71XX-BLbVhu0waskk2kieCbEgB7-Q19tcGY4b6Q4BZmlo-Hxihq_4x3W38swqsbY1E9s8AVHbYmx</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>2694039655</pqid></control><display><type>article</type><title>Influence of Lanthanum-Doped Tungsten Wire Drawing Process on Microstructure and Properties</title><source>PubMed Central Open Access</source><source>MDPI - Multidisciplinary Digital Publishing Institute</source><source>EZB-FREE-00999 freely available EZB journals</source><source>PubMed Central</source><source>Free Full-Text Journals in Chemistry</source><creator>Wang, Luyan ; Yu, Yueguang ; Zhang, Peng ; Yang, Jiancan</creator><creatorcontrib>Wang, Luyan ; Yu, Yueguang ; Zhang, Peng ; Yang, Jiancan</creatorcontrib><description>A reasonable preparation processing of Lanthanum-doped tungsten wire plays a decisive role in the final properties of the wire. This paper gives the optimum drawing process parameters of lanthanum-doped tungsten wire with φ1.00 mm–φ0.50 mm and explains the phenomenon of coarsening of fiber-like grains in the preparation processing of tungsten wire. The final optimum process parameters of lanthanum-doped tungsten wire are given: the temperature is 950 °C (the first pass temperature is 950 °C, and the temperature decreases by about 20 °C for each pass), the compression ratio is 15%, mold temperature is 550 °C, because of the limitation of equipment conditions, the wire drawing speed is fixed at 0.19 m/s. It is found that the fiber-like grains of the tungsten wire coarsen when the temperature is too high, and it is prone to breakage when the temperature is too low during the drawing process. When the compression ratio is too high (for example, 22%), there is a negative impact on the surface quality and the straightness of the tungsten wire. When the compression ratio is too low, the processing die time is increased, and the production cost is increased.</description><identifier>ISSN: 1996-1944</identifier><identifier>EISSN: 1996-1944</identifier><identifier>DOI: 10.3390/ma15144979</identifier><identifier>PMID: 35888446</identifier><language>eng</language><publisher>Basel: MDPI AG</publisher><subject>Coarsening ; Compression ratio ; Grains ; Lanthanum ; Microwaves ; Pressure molding ; Process parameters ; Production costs ; Research methodology ; Shear strength ; Surface properties ; Tungsten ; Wire drawing</subject><ispartof>Materials, 2022-07, Vol.15 (14), p.4979</ispartof><rights>2022 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/). Notwithstanding the ProQuest Terms and Conditions, you may use this content in accordance with the terms of the License.</rights><rights>2022 by the authors. 2022</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c383t-ea3a38354b9d341e9e3db12bbf3035e0b007d0f8f3d2a1d3f92b3c173db082733</citedby><cites>FETCH-LOGICAL-c383t-ea3a38354b9d341e9e3db12bbf3035e0b007d0f8f3d2a1d3f92b3c173db082733</cites><orcidid>0000-0002-5015-9410 ; 0000-0002-3801-4657</orcidid></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://www.ncbi.nlm.nih.gov/pmc/articles/PMC9323575/pdf/$$EPDF$$P50$$Gpubmedcentral$$Hfree_for_read</linktopdf><linktohtml>$$Uhttps://www.ncbi.nlm.nih.gov/pmc/articles/PMC9323575/$$EHTML$$P50$$Gpubmedcentral$$Hfree_for_read</linktohtml><link.rule.ids>230,314,727,780,784,885,27924,27925,53791,53793</link.rule.ids></links><search><creatorcontrib>Wang, Luyan</creatorcontrib><creatorcontrib>Yu, Yueguang</creatorcontrib><creatorcontrib>Zhang, Peng</creatorcontrib><creatorcontrib>Yang, Jiancan</creatorcontrib><title>Influence of Lanthanum-Doped Tungsten Wire Drawing Process on Microstructure and Properties</title><title>Materials</title><description>A reasonable preparation processing of Lanthanum-doped tungsten wire plays a decisive role in the final properties of the wire. This paper gives the optimum drawing process parameters of lanthanum-doped tungsten wire with φ1.00 mm–φ0.50 mm and explains the phenomenon of coarsening of fiber-like grains in the preparation processing of tungsten wire. The final optimum process parameters of lanthanum-doped tungsten wire are given: the temperature is 950 °C (the first pass temperature is 950 °C, and the temperature decreases by about 20 °C for each pass), the compression ratio is 15%, mold temperature is 550 °C, because of the limitation of equipment conditions, the wire drawing speed is fixed at 0.19 m/s. It is found that the fiber-like grains of the tungsten wire coarsen when the temperature is too high, and it is prone to breakage when the temperature is too low during the drawing process. When the compression ratio is too high (for example, 22%), there is a negative impact on the surface quality and the straightness of the tungsten wire. When the compression ratio is too low, the processing die time is increased, and the production cost is increased.</description><subject>Coarsening</subject><subject>Compression ratio</subject><subject>Grains</subject><subject>Lanthanum</subject><subject>Microwaves</subject><subject>Pressure molding</subject><subject>Process parameters</subject><subject>Production costs</subject><subject>Research methodology</subject><subject>Shear strength</subject><subject>Surface properties</subject><subject>Tungsten</subject><subject>Wire drawing</subject><issn>1996-1944</issn><issn>1996-1944</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2022</creationdate><recordtype>article</recordtype><sourceid>ABUWG</sourceid><sourceid>AFKRA</sourceid><sourceid>AZQEC</sourceid><sourceid>BENPR</sourceid><sourceid>CCPQU</sourceid><sourceid>DWQXO</sourceid><recordid>eNpdkU1LxDAQhoMoKqsXf0HBiwjVpJO2yUUQ14-FFT0oHjyEtJ2ulTZZk0bx39uyi19zmYH34WVmXkIOGD0BkPS00yxlnMtcbpBdJmUWM8n55q95h-x7_0qHAmAikdtkB1IhBOfZLnmemboNaEqMbB3NtelftAldPLVLrKKHYBa-RxM9NQ6jqdMfjVlE986W6H1kTXTblM763oWyDwOhTTWqS3R9g36PbNW69bi_7hPyeHX5cHETz--uZxfn87gEAX2MGvQwpLyQFXCGEqEqWFIUNVBIkRaU5hWtRQ1VolkFtUwKKFk-UFQkOcCEnK18l6HosCrR9E63aumaTrtPZXWj_iqmeVEL-64kJJDm6WBwtDZw9i2g71XX-BLbVhu0waskk2kieCbEgB7-Q19tcGY4b6Q4BZmlo-Hxihq_4x3W38swqsbY1E9s8AVHbYmx</recordid><startdate>20220718</startdate><enddate>20220718</enddate><creator>Wang, Luyan</creator><creator>Yu, Yueguang</creator><creator>Zhang, Peng</creator><creator>Yang, Jiancan</creator><general>MDPI AG</general><general>MDPI</general><scope>AAYXX</scope><scope>CITATION</scope><scope>7SR</scope><scope>8FD</scope><scope>8FE</scope><scope>8FG</scope><scope>ABJCF</scope><scope>ABUWG</scope><scope>AFKRA</scope><scope>AZQEC</scope><scope>BENPR</scope><scope>BGLVJ</scope><scope>CCPQU</scope><scope>D1I</scope><scope>DWQXO</scope><scope>HCIFZ</scope><scope>JG9</scope><scope>KB.</scope><scope>PDBOC</scope><scope>PIMPY</scope><scope>PQEST</scope><scope>PQQKQ</scope><scope>PQUKI</scope><scope>PRINS</scope><scope>7X8</scope><scope>5PM</scope><orcidid>https://orcid.org/0000-0002-5015-9410</orcidid><orcidid>https://orcid.org/0000-0002-3801-4657</orcidid></search><sort><creationdate>20220718</creationdate><title>Influence of Lanthanum-Doped Tungsten Wire Drawing Process on Microstructure and Properties</title><author>Wang, Luyan ; Yu, Yueguang ; Zhang, Peng ; Yang, Jiancan</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c383t-ea3a38354b9d341e9e3db12bbf3035e0b007d0f8f3d2a1d3f92b3c173db082733</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2022</creationdate><topic>Coarsening</topic><topic>Compression ratio</topic><topic>Grains</topic><topic>Lanthanum</topic><topic>Microwaves</topic><topic>Pressure molding</topic><topic>Process parameters</topic><topic>Production costs</topic><topic>Research methodology</topic><topic>Shear strength</topic><topic>Surface properties</topic><topic>Tungsten</topic><topic>Wire drawing</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Wang, Luyan</creatorcontrib><creatorcontrib>Yu, Yueguang</creatorcontrib><creatorcontrib>Zhang, Peng</creatorcontrib><creatorcontrib>Yang, Jiancan</creatorcontrib><collection>CrossRef</collection><collection>Engineered Materials Abstracts</collection><collection>Technology Research Database</collection><collection>ProQuest SciTech Collection</collection><collection>ProQuest Technology Collection</collection><collection>Materials Science & Engineering Collection</collection><collection>ProQuest Central (Alumni Edition)</collection><collection>ProQuest Central UK/Ireland</collection><collection>ProQuest Central Essentials</collection><collection>ProQuest Central</collection><collection>Technology Collection</collection><collection>ProQuest One Community College</collection><collection>ProQuest Materials Science Collection</collection><collection>ProQuest Central Korea</collection><collection>SciTech Premium Collection</collection><collection>Materials Research Database</collection><collection>Materials Science Database</collection><collection>Materials Science Collection</collection><collection>Access via ProQuest (Open Access)</collection><collection>ProQuest One Academic Eastern Edition (DO NOT USE)</collection><collection>ProQuest One Academic</collection><collection>ProQuest One Academic UKI Edition</collection><collection>ProQuest Central China</collection><collection>MEDLINE - Academic</collection><collection>PubMed Central (Full Participant titles)</collection><jtitle>Materials</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Wang, Luyan</au><au>Yu, Yueguang</au><au>Zhang, Peng</au><au>Yang, Jiancan</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Influence of Lanthanum-Doped Tungsten Wire Drawing Process on Microstructure and Properties</atitle><jtitle>Materials</jtitle><date>2022-07-18</date><risdate>2022</risdate><volume>15</volume><issue>14</issue><spage>4979</spage><pages>4979-</pages><issn>1996-1944</issn><eissn>1996-1944</eissn><abstract>A reasonable preparation processing of Lanthanum-doped tungsten wire plays a decisive role in the final properties of the wire. This paper gives the optimum drawing process parameters of lanthanum-doped tungsten wire with φ1.00 mm–φ0.50 mm and explains the phenomenon of coarsening of fiber-like grains in the preparation processing of tungsten wire. The final optimum process parameters of lanthanum-doped tungsten wire are given: the temperature is 950 °C (the first pass temperature is 950 °C, and the temperature decreases by about 20 °C for each pass), the compression ratio is 15%, mold temperature is 550 °C, because of the limitation of equipment conditions, the wire drawing speed is fixed at 0.19 m/s. It is found that the fiber-like grains of the tungsten wire coarsen when the temperature is too high, and it is prone to breakage when the temperature is too low during the drawing process. When the compression ratio is too high (for example, 22%), there is a negative impact on the surface quality and the straightness of the tungsten wire. When the compression ratio is too low, the processing die time is increased, and the production cost is increased.</abstract><cop>Basel</cop><pub>MDPI AG</pub><pmid>35888446</pmid><doi>10.3390/ma15144979</doi><orcidid>https://orcid.org/0000-0002-5015-9410</orcidid><orcidid>https://orcid.org/0000-0002-3801-4657</orcidid><oa>free_for_read</oa></addata></record> |
fulltext | fulltext |
identifier | ISSN: 1996-1944 |
ispartof | Materials, 2022-07, Vol.15 (14), p.4979 |
issn | 1996-1944 1996-1944 |
language | eng |
recordid | cdi_pubmedcentral_primary_oai_pubmedcentral_nih_gov_9323575 |
source | PubMed Central Open Access; MDPI - Multidisciplinary Digital Publishing Institute; EZB-FREE-00999 freely available EZB journals; PubMed Central; Free Full-Text Journals in Chemistry |
subjects | Coarsening Compression ratio Grains Lanthanum Microwaves Pressure molding Process parameters Production costs Research methodology Shear strength Surface properties Tungsten Wire drawing |
title | Influence of Lanthanum-Doped Tungsten Wire Drawing Process on Microstructure and Properties |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-27T13%3A41%3A44IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_pubme&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Influence%20of%20Lanthanum-Doped%20Tungsten%20Wire%20Drawing%20Process%20on%20Microstructure%20and%20Properties&rft.jtitle=Materials&rft.au=Wang,%20Luyan&rft.date=2022-07-18&rft.volume=15&rft.issue=14&rft.spage=4979&rft.pages=4979-&rft.issn=1996-1944&rft.eissn=1996-1944&rft_id=info:doi/10.3390/ma15144979&rft_dat=%3Cproquest_pubme%3E2694039655%3C/proquest_pubme%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=2694039655&rft_id=info:pmid/35888446&rfr_iscdi=true |