Optimization of dye adsorption time and film thickness for efficient ZnO dye-sensitized solar cells with high at-rest stability

Photoelectrodes for dye-sensitized solar cells were fabricated using commercially available zinc oxide (ZnO) nanoparticles and sensitized with the dye N719. This study systematically investigates the effects of two fabrication factors: the ZnO film thickness and the dye adsorption time. Results show...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Nanoscale research letters 2012-12, Vol.7 (1), p.688-688, Article 688
Hauptverfasser: Chang, Wei-Chen, Lee, Chia-Hua, Yu, Wan-Chin, Lin, Chun-Min
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Photoelectrodes for dye-sensitized solar cells were fabricated using commercially available zinc oxide (ZnO) nanoparticles and sensitized with the dye N719. This study systematically investigates the effects of two fabrication factors: the ZnO film thickness and the dye adsorption time. Results show that these two fabrication factors must be optimized simultaneously to obtain efficient ZnO/N719-based cells. Different film thicknesses require different dye adsorption times for optimal cell performance. This is because a prolonged dye adsorption time leads to a significant deterioration in cell performance. This is contrary to what is normally observed for titanium dioxide-based cells. The highest overall power conversion efficiency obtained in this study was 5.61%, which was achieved by 26-μm-thick photoelectrodes sensitized in a dye solution for 2 h. In addition, the best-performing cell demonstrated remarkable at-rest stability despite the use of a liquid electrolyte. Approximately 70% of the initial efficiency remained after more than 1 year of room-temperature storage in the dark. To better understand how dye adsorption time affects electron transport properties, this study also investigated cells based on 26-μm-thick films using electrochemical impedance spectroscopy (EIS). The EIS results show good agreement with the measured device performance parameters.
ISSN:1556-276X
1931-7573
1556-276X
DOI:10.1186/1556-276X-7-688