Dielectric Properties of Bi 2/3 Cu 3 Ti 4 O 12 Ceramics Prepared by Mechanical Ball Milling and Low Temperature Conventional Sintering

In the current study, Bi Cu Ti O (BCTO) ceramics were prepared by mechanical ball mill of the elemental oxides followed by conventional sintering of the powder without any pre-sintering heat treatments. The sintering temperature was in the range 950-990 °C, which is 100-150 °C lower than the previou...