The Influence of Stirring Time on Mechanical Properties of Sn–58Bi Alloy Treated in the Semi-Solid State by Mechanical Stirring Process

In this paper, the technology of semi-solid casting was to used are produced Sn-Bi alloy. The influence of agitating time at 125 °C on the microstructure and mechanical properties of of Sn-58Bi casting alloy were discussed. The eutectic Sn-Bi alloy was mechanically agitated during the casting solidi...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Key engineering materials 2011-06, Vol.480-481, p.1521-1524
Hauptverfasser: Li, Yong, He, Jian Nan, Wu, Yu Chi, Xiao, Xiao Ting, Zheng, Yu Chuan, Cheng, Xiao Ling, Zheng, Chun Chun, Hu, Yong Jun, Zhong, Bin Qiang, He, Yuan Chuan, Li, Feng
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:In this paper, the technology of semi-solid casting was to used are produced Sn-Bi alloy. The influence of agitating time at 125 °C on the microstructure and mechanical properties of of Sn-58Bi casting alloy were discussed. The eutectic Sn-Bi alloy was mechanically agitated during the casting solidification process. The results indicated that non-lamellar Sn-Bi structure with long plate shape, short strip, small size block and suborbicular block shape Sn phase was obtained for different stirring time. The elongation of Sn-Bi alloy with non-lamellar eutectic structure is improved prominently. Compared with the elongation of lamellar eutectic Sn-Bi alloy prepared by conventional die casting, the elongation of semi-solid Sn-Bi alloy with suborbicular block shape Sn phase is enhanced up to 45%.
ISSN:1013-9826
1662-9795
1662-9795
DOI:10.4028/www.scientific.net/KEM.480-481.1521