Investigation of shrinkage behavior of Ni–Fe bimetallic anode tube support and the densification of electrolyte using co-sintering temperature

► The OCV of the cells is linearly related to the tube diameter shrinkage degree, it reaches 1.1 V which basically equals to the Nernst voltage prepared at 1400 °C. ► At each co-sintering temperature from 1250 °C to 1400 °C, the porosity of NiO–Fe 2O 3/GDC anode tubes is nearly 10% higher than that...