The Effect of Coating Thickness on Corrosion Resistance of Hydroxyapatite Coated Ti6Al4V and 316L SS Implants

Hydroxyapatite (HAP) has been coated onto Ti6Al4V and 316L SS substrates by sol-gel method. The coating thicknesses for the analysis were about 40 and 72 μm. Adhesion and corrosion tests have been conducted on uncoated and HAP-coated substrates. The coatings were characterized by XRD, SEM, and adhes...