High Strength AA7050 Al alloy processed by ECAP: Microstructure and mechanical properties

► ECAP improves the strength of the AA7050 Al alloy with no loss on ductility. ► Room temperature ECAP strengthens the alloy by grain refinement and work hardening. ► ECAP at 150 °C strengthens the alloy by grain refinement and precipitation. ► Second phase precipitation is accelerated by ECAP. ► Pr...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials science & engineering. A, Structural materials : properties, microstructure and processing Structural materials : properties, microstructure and processing, 2011-07, Vol.528 (18), p.5804-5811
Hauptverfasser: Cardoso, K.R., Travessa, D.N., Botta, W.J., Jorge, A.M.