Novel method to produce β-TCP scaffolds

The production of ceramic scaffolds by a novel method was reported in this work. The method comprised the mixture of colloidal silica and β-tricalcium phosphate (β-TCP) powder, where paraffin microspheres were further added to provide the porosity in the scaffold after firing. Thermo-gravimetric ana...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials letters 2011-01, Vol.65 (2), p.275-277
Hauptverfasser: Ribeiro, Gabriela B.M., Trommer, Rafael M., dos Santos, Luis A., Bergmann, Carlos P.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 277
container_issue 2
container_start_page 275
container_title Materials letters
container_volume 65
creator Ribeiro, Gabriela B.M.
Trommer, Rafael M.
dos Santos, Luis A.
Bergmann, Carlos P.
description The production of ceramic scaffolds by a novel method was reported in this work. The method comprised the mixture of colloidal silica and β-tricalcium phosphate (β-TCP) powder, where paraffin microspheres were further added to provide the porosity in the scaffold after firing. Thermo-gravimetric analysis showed that the paraffin was completely degraded before 550 °C, where the heat treatment at 1100 °C was enough to remove the paraffin and provide porosity and mechanical strength. The scaffold had an open porosity, but with poor pore interconnection. The density of the scaffold was 1.11 ± 0.03 g/cm 3 with a porosity of 64.98 ± 1.1%, and the compression strength was 5.02 ± 1.2 MPa.
doi_str_mv 10.1016/j.matlet.2010.09.066
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_861535464</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0167577X10008268</els_id><sourcerecordid>861535464</sourcerecordid><originalsourceid>FETCH-LOGICAL-c362t-9779b1bc9d34bc3acea0491d761d54cd813f4099266fe8d8bbafbaaa5f385aea3</originalsourceid><addsrcrecordid>eNp9kMtKxDAUhoMoOI6-gWB3umlNmjRpNoIM3kBUcAbchTQ50Q7tZEw6A76WD-IzmaGuXR04fP-5fAidElwQTPjlsuj10MFQlDi1sCww53toQmpBcyaF3EeThIm8EuLtEB3FuMQYM4nZBF08-S10WQ_Dh7fZ4LN18HZjIPv5zuezlywa7ZzvbDxGB053EU7-6hQtbm_ms_v88fnuYXb9mBvKyyGXQsiGNEZayhpDtQGdNhErOLEVM7Ym1DEsZcm5g9rWTaNdo7WuHK0rDZpO0fk4Nx3yuYE4qL6NBrpOr8Bvoqo5qWjFOEskG0kTfIwBnFqHttfhSxGsdl7UUo1e1M6LwlIlLyl2Nsac9kq_hzaqxWsCquSEYirLRFyNBKQ_ty0EFU0LKwO2DWAGZX37_4pfBCx3HQ</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>861535464</pqid></control><display><type>article</type><title>Novel method to produce β-TCP scaffolds</title><source>Elsevier ScienceDirect Journals Complete</source><creator>Ribeiro, Gabriela B.M. ; Trommer, Rafael M. ; dos Santos, Luis A. ; Bergmann, Carlos P.</creator><creatorcontrib>Ribeiro, Gabriela B.M. ; Trommer, Rafael M. ; dos Santos, Luis A. ; Bergmann, Carlos P.</creatorcontrib><description>The production of ceramic scaffolds by a novel method was reported in this work. The method comprised the mixture of colloidal silica and β-tricalcium phosphate (β-TCP) powder, where paraffin microspheres were further added to provide the porosity in the scaffold after firing. Thermo-gravimetric analysis showed that the paraffin was completely degraded before 550 °C, where the heat treatment at 1100 °C was enough to remove the paraffin and provide porosity and mechanical strength. The scaffold had an open porosity, but with poor pore interconnection. The density of the scaffold was 1.11 ± 0.03 g/cm 3 with a porosity of 64.98 ± 1.1%, and the compression strength was 5.02 ± 1.2 MPa.</description><identifier>ISSN: 0167-577X</identifier><identifier>EISSN: 1873-4979</identifier><identifier>DOI: 10.1016/j.matlet.2010.09.066</identifier><language>eng</language><publisher>Elsevier B.V</publisher><subject>Ceramics ; Colloidal silica ; Density ; Firing ; heat treatment ; Interconnection ; Microspheres ; new methods ; Paraffin microspheres ; Paraffins ; Phosphates ; Porosity ; Scaffold ; Scaffolds ; silica ; thermogravimetry ; Tricalcium phosphate</subject><ispartof>Materials letters, 2011-01, Vol.65 (2), p.275-277</ispartof><rights>2010 Elsevier B.V.</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c362t-9779b1bc9d34bc3acea0491d761d54cd813f4099266fe8d8bbafbaaa5f385aea3</citedby><cites>FETCH-LOGICAL-c362t-9779b1bc9d34bc3acea0491d761d54cd813f4099266fe8d8bbafbaaa5f385aea3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://www.sciencedirect.com/science/article/pii/S0167577X10008268$$EHTML$$P50$$Gelsevier$$H</linktohtml><link.rule.ids>314,776,780,3537,27901,27902,65306</link.rule.ids></links><search><creatorcontrib>Ribeiro, Gabriela B.M.</creatorcontrib><creatorcontrib>Trommer, Rafael M.</creatorcontrib><creatorcontrib>dos Santos, Luis A.</creatorcontrib><creatorcontrib>Bergmann, Carlos P.</creatorcontrib><title>Novel method to produce β-TCP scaffolds</title><title>Materials letters</title><description>The production of ceramic scaffolds by a novel method was reported in this work. The method comprised the mixture of colloidal silica and β-tricalcium phosphate (β-TCP) powder, where paraffin microspheres were further added to provide the porosity in the scaffold after firing. Thermo-gravimetric analysis showed that the paraffin was completely degraded before 550 °C, where the heat treatment at 1100 °C was enough to remove the paraffin and provide porosity and mechanical strength. The scaffold had an open porosity, but with poor pore interconnection. The density of the scaffold was 1.11 ± 0.03 g/cm 3 with a porosity of 64.98 ± 1.1%, and the compression strength was 5.02 ± 1.2 MPa.</description><subject>Ceramics</subject><subject>Colloidal silica</subject><subject>Density</subject><subject>Firing</subject><subject>heat treatment</subject><subject>Interconnection</subject><subject>Microspheres</subject><subject>new methods</subject><subject>Paraffin microspheres</subject><subject>Paraffins</subject><subject>Phosphates</subject><subject>Porosity</subject><subject>Scaffold</subject><subject>Scaffolds</subject><subject>silica</subject><subject>thermogravimetry</subject><subject>Tricalcium phosphate</subject><issn>0167-577X</issn><issn>1873-4979</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2011</creationdate><recordtype>article</recordtype><recordid>eNp9kMtKxDAUhoMoOI6-gWB3umlNmjRpNoIM3kBUcAbchTQ50Q7tZEw6A76WD-IzmaGuXR04fP-5fAidElwQTPjlsuj10MFQlDi1sCww53toQmpBcyaF3EeThIm8EuLtEB3FuMQYM4nZBF08-S10WQ_Dh7fZ4LN18HZjIPv5zuezlywa7ZzvbDxGB053EU7-6hQtbm_ms_v88fnuYXb9mBvKyyGXQsiGNEZayhpDtQGdNhErOLEVM7Ym1DEsZcm5g9rWTaNdo7WuHK0rDZpO0fk4Nx3yuYE4qL6NBrpOr8Bvoqo5qWjFOEskG0kTfIwBnFqHttfhSxGsdl7UUo1e1M6LwlIlLyl2Nsac9kq_hzaqxWsCquSEYirLRFyNBKQ_ty0EFU0LKwO2DWAGZX37_4pfBCx3HQ</recordid><startdate>20110131</startdate><enddate>20110131</enddate><creator>Ribeiro, Gabriela B.M.</creator><creator>Trommer, Rafael M.</creator><creator>dos Santos, Luis A.</creator><creator>Bergmann, Carlos P.</creator><general>Elsevier B.V</general><scope>FBQ</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7QQ</scope><scope>7SR</scope><scope>8BQ</scope><scope>8FD</scope><scope>JG9</scope></search><sort><creationdate>20110131</creationdate><title>Novel method to produce β-TCP scaffolds</title><author>Ribeiro, Gabriela B.M. ; Trommer, Rafael M. ; dos Santos, Luis A. ; Bergmann, Carlos P.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c362t-9779b1bc9d34bc3acea0491d761d54cd813f4099266fe8d8bbafbaaa5f385aea3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2011</creationdate><topic>Ceramics</topic><topic>Colloidal silica</topic><topic>Density</topic><topic>Firing</topic><topic>heat treatment</topic><topic>Interconnection</topic><topic>Microspheres</topic><topic>new methods</topic><topic>Paraffin microspheres</topic><topic>Paraffins</topic><topic>Phosphates</topic><topic>Porosity</topic><topic>Scaffold</topic><topic>Scaffolds</topic><topic>silica</topic><topic>thermogravimetry</topic><topic>Tricalcium phosphate</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Ribeiro, Gabriela B.M.</creatorcontrib><creatorcontrib>Trommer, Rafael M.</creatorcontrib><creatorcontrib>dos Santos, Luis A.</creatorcontrib><creatorcontrib>Bergmann, Carlos P.</creatorcontrib><collection>AGRIS</collection><collection>CrossRef</collection><collection>Ceramic Abstracts</collection><collection>Engineered Materials Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><jtitle>Materials letters</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Ribeiro, Gabriela B.M.</au><au>Trommer, Rafael M.</au><au>dos Santos, Luis A.</au><au>Bergmann, Carlos P.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Novel method to produce β-TCP scaffolds</atitle><jtitle>Materials letters</jtitle><date>2011-01-31</date><risdate>2011</risdate><volume>65</volume><issue>2</issue><spage>275</spage><epage>277</epage><pages>275-277</pages><issn>0167-577X</issn><eissn>1873-4979</eissn><abstract>The production of ceramic scaffolds by a novel method was reported in this work. The method comprised the mixture of colloidal silica and β-tricalcium phosphate (β-TCP) powder, where paraffin microspheres were further added to provide the porosity in the scaffold after firing. Thermo-gravimetric analysis showed that the paraffin was completely degraded before 550 °C, where the heat treatment at 1100 °C was enough to remove the paraffin and provide porosity and mechanical strength. The scaffold had an open porosity, but with poor pore interconnection. The density of the scaffold was 1.11 ± 0.03 g/cm 3 with a porosity of 64.98 ± 1.1%, and the compression strength was 5.02 ± 1.2 MPa.</abstract><pub>Elsevier B.V</pub><doi>10.1016/j.matlet.2010.09.066</doi><tpages>3</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0167-577X
ispartof Materials letters, 2011-01, Vol.65 (2), p.275-277
issn 0167-577X
1873-4979
language eng
recordid cdi_proquest_miscellaneous_861535464
source Elsevier ScienceDirect Journals Complete
subjects Ceramics
Colloidal silica
Density
Firing
heat treatment
Interconnection
Microspheres
new methods
Paraffin microspheres
Paraffins
Phosphates
Porosity
Scaffold
Scaffolds
silica
thermogravimetry
Tricalcium phosphate
title Novel method to produce β-TCP scaffolds
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-04T18%3A04%3A18IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Novel%20method%20to%20produce%20%CE%B2-TCP%20scaffolds&rft.jtitle=Materials%20letters&rft.au=Ribeiro,%20Gabriela%20B.M.&rft.date=2011-01-31&rft.volume=65&rft.issue=2&rft.spage=275&rft.epage=277&rft.pages=275-277&rft.issn=0167-577X&rft.eissn=1873-4979&rft_id=info:doi/10.1016/j.matlet.2010.09.066&rft_dat=%3Cproquest_cross%3E861535464%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=861535464&rft_id=info:pmid/&rft_els_id=S0167577X10008268&rfr_iscdi=true