Preparation of Thermo-Stable Bulk Metallic Glass of Nd60Cu20Ni10Al10 by Rapid Compression
Melt of Nd60Cu20Ni10Al10 alloy is solidified by rapid compression from 0.1 to 5.5 GPa at 793K and from 0.1 to 3.2 GPa at 873K within 20 ms, separately. A fully bulk metallic glass is obtained by the rapid compression method. By comparing with as-cast bulk metallic glass (BMG), it is found that Nd60C...