Evaluation of S–N curves with more than one failure mode

In very high cycle fatigue, researchers and engineers are often confronted with S–N curves which exhibit more than one type of failure. Generally, it is assumed that every specific crack-initiation type has its own S–N curve, so that in this case two or more S–N curves can be drawn in the S–N diagra...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:International journal of fatigue 2011, Vol.33 (1), p.19-22
Hauptverfasser: Bomas, Hubert, Burkart, Klaus, Zoch, Hans-Werner
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 22
container_issue 1
container_start_page 19
container_title International journal of fatigue
container_volume 33
creator Bomas, Hubert
Burkart, Klaus
Zoch, Hans-Werner
description In very high cycle fatigue, researchers and engineers are often confronted with S–N curves which exhibit more than one type of failure. Generally, it is assumed that every specific crack-initiation type has its own S–N curve, so that in this case two or more S–N curves can be drawn in the S–N diagrams. This paper will show an S–N diagram with two failure types and will provide a generalised method of drawing correct S–N curves for every single type of failure.
doi_str_mv 10.1016/j.ijfatigue.2010.04.010
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_849473583</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0142112310001027</els_id><sourcerecordid>849473583</sourcerecordid><originalsourceid>FETCH-LOGICAL-c347t-a2c4316d2d71ab0a04f3897bf96f5e26e41fcb6488a16e29d9f3f47055f369b23</originalsourceid><addsrcrecordid>eNqFkMtOwzAURC0EEqXwDWTHKsGvxDG7qioPqYIFsLYc55o6yqPYSRE7_oE_5EswKmLL6khzZ0a6g9A5wRnBpLhsMtdYPbqXCTKKo4p5FnGAZqQUMmU8p4dohgmnKSGUHaOTEBqMscQin6Gr1U63U4wPfTLY5PHr4_M-MZPfQUje3LhJusFDMm50PPeQWO3aKQrdUMMpOrK6DXD2yzl6vl49LW_T9cPN3XKxTg3jYkw1NZyRoqa1ILrCGnPLSikqKwubAy2AE2uqgpelJgVQWUvLLBc4zy0rZEXZHF3se7d-eJ0gjKpzwUDb6h6GKaiSSy5YXrLoFHun8UMIHqzaetdp_64IVj9jqUb9jaV-xlKYq4iYXOyTEB_ZOfAqGAe9gdp5MKOqB_dvxzdQAncC</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>849473583</pqid></control><display><type>article</type><title>Evaluation of S–N curves with more than one failure mode</title><source>Elsevier ScienceDirect Journals</source><creator>Bomas, Hubert ; Burkart, Klaus ; Zoch, Hans-Werner</creator><creatorcontrib>Bomas, Hubert ; Burkart, Klaus ; Zoch, Hans-Werner</creatorcontrib><description>In very high cycle fatigue, researchers and engineers are often confronted with S–N curves which exhibit more than one type of failure. Generally, it is assumed that every specific crack-initiation type has its own S–N curve, so that in this case two or more S–N curves can be drawn in the S–N diagrams. This paper will show an S–N diagram with two failure types and will provide a generalised method of drawing correct S–N curves for every single type of failure.</description><identifier>ISSN: 0142-1123</identifier><identifier>EISSN: 1879-3452</identifier><identifier>DOI: 10.1016/j.ijfatigue.2010.04.010</identifier><language>eng</language><publisher>Elsevier Ltd</publisher><subject>Crack initiation ; Failure modes ; Fatigue (materials) ; Fatigue failure ; Fatigue life ; High cycle fatigue ; Inclusions ; S N diagrams ; S–N curve ; Very high cycle fatigue (VHCF)</subject><ispartof>International journal of fatigue, 2011, Vol.33 (1), p.19-22</ispartof><rights>2010 Elsevier Ltd</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c347t-a2c4316d2d71ab0a04f3897bf96f5e26e41fcb6488a16e29d9f3f47055f369b23</citedby></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://dx.doi.org/10.1016/j.ijfatigue.2010.04.010$$EHTML$$P50$$Gelsevier$$H</linktohtml><link.rule.ids>314,777,781,3537,4010,27904,27905,27906,45976</link.rule.ids></links><search><creatorcontrib>Bomas, Hubert</creatorcontrib><creatorcontrib>Burkart, Klaus</creatorcontrib><creatorcontrib>Zoch, Hans-Werner</creatorcontrib><title>Evaluation of S–N curves with more than one failure mode</title><title>International journal of fatigue</title><description>In very high cycle fatigue, researchers and engineers are often confronted with S–N curves which exhibit more than one type of failure. Generally, it is assumed that every specific crack-initiation type has its own S–N curve, so that in this case two or more S–N curves can be drawn in the S–N diagrams. This paper will show an S–N diagram with two failure types and will provide a generalised method of drawing correct S–N curves for every single type of failure.</description><subject>Crack initiation</subject><subject>Failure modes</subject><subject>Fatigue (materials)</subject><subject>Fatigue failure</subject><subject>Fatigue life</subject><subject>High cycle fatigue</subject><subject>Inclusions</subject><subject>S N diagrams</subject><subject>S–N curve</subject><subject>Very high cycle fatigue (VHCF)</subject><issn>0142-1123</issn><issn>1879-3452</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2011</creationdate><recordtype>article</recordtype><recordid>eNqFkMtOwzAURC0EEqXwDWTHKsGvxDG7qioPqYIFsLYc55o6yqPYSRE7_oE_5EswKmLL6khzZ0a6g9A5wRnBpLhsMtdYPbqXCTKKo4p5FnGAZqQUMmU8p4dohgmnKSGUHaOTEBqMscQin6Gr1U63U4wPfTLY5PHr4_M-MZPfQUje3LhJusFDMm50PPeQWO3aKQrdUMMpOrK6DXD2yzl6vl49LW_T9cPN3XKxTg3jYkw1NZyRoqa1ILrCGnPLSikqKwubAy2AE2uqgpelJgVQWUvLLBc4zy0rZEXZHF3se7d-eJ0gjKpzwUDb6h6GKaiSSy5YXrLoFHun8UMIHqzaetdp_64IVj9jqUb9jaV-xlKYq4iYXOyTEB_ZOfAqGAe9gdp5MKOqB_dvxzdQAncC</recordid><startdate>2011</startdate><enddate>2011</enddate><creator>Bomas, Hubert</creator><creator>Burkart, Klaus</creator><creator>Zoch, Hans-Werner</creator><general>Elsevier Ltd</general><scope>AAYXX</scope><scope>CITATION</scope><scope>7SR</scope><scope>8BQ</scope><scope>8FD</scope><scope>FR3</scope><scope>JG9</scope><scope>KR7</scope></search><sort><creationdate>2011</creationdate><title>Evaluation of S–N curves with more than one failure mode</title><author>Bomas, Hubert ; Burkart, Klaus ; Zoch, Hans-Werner</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c347t-a2c4316d2d71ab0a04f3897bf96f5e26e41fcb6488a16e29d9f3f47055f369b23</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2011</creationdate><topic>Crack initiation</topic><topic>Failure modes</topic><topic>Fatigue (materials)</topic><topic>Fatigue failure</topic><topic>Fatigue life</topic><topic>High cycle fatigue</topic><topic>Inclusions</topic><topic>S N diagrams</topic><topic>S–N curve</topic><topic>Very high cycle fatigue (VHCF)</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Bomas, Hubert</creatorcontrib><creatorcontrib>Burkart, Klaus</creatorcontrib><creatorcontrib>Zoch, Hans-Werner</creatorcontrib><collection>CrossRef</collection><collection>Engineered Materials Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Engineering Research Database</collection><collection>Materials Research Database</collection><collection>Civil Engineering Abstracts</collection><jtitle>International journal of fatigue</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Bomas, Hubert</au><au>Burkart, Klaus</au><au>Zoch, Hans-Werner</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Evaluation of S–N curves with more than one failure mode</atitle><jtitle>International journal of fatigue</jtitle><date>2011</date><risdate>2011</risdate><volume>33</volume><issue>1</issue><spage>19</spage><epage>22</epage><pages>19-22</pages><issn>0142-1123</issn><eissn>1879-3452</eissn><abstract>In very high cycle fatigue, researchers and engineers are often confronted with S–N curves which exhibit more than one type of failure. Generally, it is assumed that every specific crack-initiation type has its own S–N curve, so that in this case two or more S–N curves can be drawn in the S–N diagrams. This paper will show an S–N diagram with two failure types and will provide a generalised method of drawing correct S–N curves for every single type of failure.</abstract><pub>Elsevier Ltd</pub><doi>10.1016/j.ijfatigue.2010.04.010</doi><tpages>4</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0142-1123
ispartof International journal of fatigue, 2011, Vol.33 (1), p.19-22
issn 0142-1123
1879-3452
language eng
recordid cdi_proquest_miscellaneous_849473583
source Elsevier ScienceDirect Journals
subjects Crack initiation
Failure modes
Fatigue (materials)
Fatigue failure
Fatigue life
High cycle fatigue
Inclusions
S N diagrams
S–N curve
Very high cycle fatigue (VHCF)
title Evaluation of S–N curves with more than one failure mode
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-19T21%3A23%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Evaluation%20of%20S%E2%80%93N%20curves%20with%20more%20than%20one%20failure%20mode&rft.jtitle=International%20journal%20of%20fatigue&rft.au=Bomas,%20Hubert&rft.date=2011&rft.volume=33&rft.issue=1&rft.spage=19&rft.epage=22&rft.pages=19-22&rft.issn=0142-1123&rft.eissn=1879-3452&rft_id=info:doi/10.1016/j.ijfatigue.2010.04.010&rft_dat=%3Cproquest_cross%3E849473583%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=849473583&rft_id=info:pmid/&rft_els_id=S0142112310001027&rfr_iscdi=true