A study on martensitic phase transformation in 9Cr–1W–0.23V–0.063Ta–0.56Mn–0.09C–0.02N (wt.%) reduced activation steel using differential scanning calorimetry

The salient characteristics of martensite formation kinetics in 9Cr–1W–0.23V–0.063Ta–0.09C–0.02N (wt.%) reduced activation steel have been investigated using differential scanning calorimetry and supplemented by microscopy characterisation. Accurate determination of the martensite start ( M S) and f...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of nuclear materials 2010-10, Vol.405 (1), p.59-69
Hauptverfasser: Raju, S., Jeya Ganesh, B., Rai, Arun Kumar, Mythili, R., Saroja, S., Raj, Baldev
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 69
container_issue 1
container_start_page 59
container_title Journal of nuclear materials
container_volume 405
creator Raju, S.
Jeya Ganesh, B.
Rai, Arun Kumar
Mythili, R.
Saroja, S.
Raj, Baldev
description The salient characteristics of martensite formation kinetics in 9Cr–1W–0.23V–0.063Ta–0.09C–0.02N (wt.%) reduced activation steel have been investigated using differential scanning calorimetry and supplemented by microscopy characterisation. Accurate determination of the martensite start ( M S) and finish ( M f) temperatures as a function of cooling rate (1–99 K min −1) and holding time (1–120 min) in the γ-austenite phase field have been made. The critical cooling rate to form nearly 100% martensite is found to be of the order of 5–6 K min −1. The measured latent heat for the martensite transformation is found to be in the range 62–75 J g −1. In the case of austenitisation at 1323 K, it is found that the grain size of the parent austenite exhibited significant growth and the observed M S temperature too exhibited a systematic increase with austenite grain size. However, for those samples that are solution treated at a slightly lower temperature of 1253 K, the M S is found to be initially insensitive to the increase in holding time for up to about 30 min. This trend is followed later on by the usual increasing character of M S for further rise in the holding periods, up to about 120 min. This unusual initial behaviour is also reflected by the corresponding variation in the hardness values of the quenched in martensite. Moreover, the growth of parent austenite grains has also been restricted during the initial phase of solution annealing at 1253 K. This is attributed to the presence of undissolved carbide particles, which exert a pinning influence on the movement of austenite grain boundaries. The observed athermal martensite formation kinetics is described well by the Koistinen–Marburger relation.
doi_str_mv 10.1016/j.jnucmat.2010.07.036
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_849440460</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0022311510003466</els_id><sourcerecordid>849440460</sourcerecordid><originalsourceid>FETCH-LOGICAL-c371t-5cb509dcbe8e1a74be2647b8dbdf3121d0f350ef3cd1ba6ccf680be72b1bde2a3</originalsourceid><addsrcrecordid>eNqFUUtuFDEUbCGQGBKOgORNBCy682z3d4WiUUiQAmwCLC1_nsGjHvdgu4NmlzvkFhyLk-BJj9iycVmlevU-VRSvKFQUaHu-qTZ-1luZKgaZg64C3j4pVrTveFn3DJ4WKwDGSk5p87x4EeMGAJoBmlXx-4LENJs9mTzZypDQR5ecJrsfMiJJQfpop5C9XRY4T4Z1-HP_QL_lByrGvz4itPxWPv6a9qNfqGG9IPtE3vxK1dlbEtDMGg2ROrm7xTAmxJHM0fnvxDhrMaBPTo4kaun9gdVynILbYgr70-KZlWPEl0c8Kb68v7xdX5c3n68-rC9uSs07mspGqwYGoxX2SGVXK2Rt3aneKGM5ZdSA5Q2g5dpQJVutbduDwo4pqgwyyU-K14vvLkw_Z4xJbF3UOI7S4zRH0ddDXUPdQlY2i1KHKcaAVuzyrDLsBQVxiEZsxDEacYhGQCdyNLnu7NhB5kVHm6-sXfxXzDirB8qarHu36DCve-cwiKgd-nxEF1AnYSb3n05_ASidrX4</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>849440460</pqid></control><display><type>article</type><title>A study on martensitic phase transformation in 9Cr–1W–0.23V–0.063Ta–0.56Mn–0.09C–0.02N (wt.%) reduced activation steel using differential scanning calorimetry</title><source>Elsevier ScienceDirect Journals</source><creator>Raju, S. ; Jeya Ganesh, B. ; Rai, Arun Kumar ; Mythili, R. ; Saroja, S. ; Raj, Baldev</creator><creatorcontrib>Raju, S. ; Jeya Ganesh, B. ; Rai, Arun Kumar ; Mythili, R. ; Saroja, S. ; Raj, Baldev</creatorcontrib><description>The salient characteristics of martensite formation kinetics in 9Cr–1W–0.23V–0.063Ta–0.09C–0.02N (wt.%) reduced activation steel have been investigated using differential scanning calorimetry and supplemented by microscopy characterisation. Accurate determination of the martensite start ( M S) and finish ( M f) temperatures as a function of cooling rate (1–99 K min −1) and holding time (1–120 min) in the γ-austenite phase field have been made. The critical cooling rate to form nearly 100% martensite is found to be of the order of 5–6 K min −1. The measured latent heat for the martensite transformation is found to be in the range 62–75 J g −1. In the case of austenitisation at 1323 K, it is found that the grain size of the parent austenite exhibited significant growth and the observed M S temperature too exhibited a systematic increase with austenite grain size. However, for those samples that are solution treated at a slightly lower temperature of 1253 K, the M S is found to be initially insensitive to the increase in holding time for up to about 30 min. This trend is followed later on by the usual increasing character of M S for further rise in the holding periods, up to about 120 min. This unusual initial behaviour is also reflected by the corresponding variation in the hardness values of the quenched in martensite. Moreover, the growth of parent austenite grains has also been restricted during the initial phase of solution annealing at 1253 K. This is attributed to the presence of undissolved carbide particles, which exert a pinning influence on the movement of austenite grain boundaries. The observed athermal martensite formation kinetics is described well by the Koistinen–Marburger relation.</description><identifier>ISSN: 0022-3115</identifier><identifier>EISSN: 1873-4820</identifier><identifier>DOI: 10.1016/j.jnucmat.2010.07.036</identifier><identifier>CODEN: JNUMAM</identifier><language>eng</language><publisher>Amsterdam: Elsevier B.V</publisher><subject>Applied sciences ; Controled nuclear fusion plants ; Energy ; Energy. Thermal use of fuels ; Exact sciences and technology ; Fission nuclear power plants ; Fuels ; Installations for energy generation and conversion: thermal and electrical energy ; Nuclear fuels</subject><ispartof>Journal of nuclear materials, 2010-10, Vol.405 (1), p.59-69</ispartof><rights>2010 Elsevier B.V.</rights><rights>2015 INIST-CNRS</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c371t-5cb509dcbe8e1a74be2647b8dbdf3121d0f350ef3cd1ba6ccf680be72b1bde2a3</citedby><cites>FETCH-LOGICAL-c371t-5cb509dcbe8e1a74be2647b8dbdf3121d0f350ef3cd1ba6ccf680be72b1bde2a3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://www.sciencedirect.com/science/article/pii/S0022311510003466$$EHTML$$P50$$Gelsevier$$H</linktohtml><link.rule.ids>314,776,780,3537,27901,27902,65306</link.rule.ids><backlink>$$Uhttp://pascal-francis.inist.fr/vibad/index.php?action=getRecordDetail&amp;idt=23249125$$DView record in Pascal Francis$$Hfree_for_read</backlink></links><search><creatorcontrib>Raju, S.</creatorcontrib><creatorcontrib>Jeya Ganesh, B.</creatorcontrib><creatorcontrib>Rai, Arun Kumar</creatorcontrib><creatorcontrib>Mythili, R.</creatorcontrib><creatorcontrib>Saroja, S.</creatorcontrib><creatorcontrib>Raj, Baldev</creatorcontrib><title>A study on martensitic phase transformation in 9Cr–1W–0.23V–0.063Ta–0.56Mn–0.09C–0.02N (wt.%) reduced activation steel using differential scanning calorimetry</title><title>Journal of nuclear materials</title><description>The salient characteristics of martensite formation kinetics in 9Cr–1W–0.23V–0.063Ta–0.09C–0.02N (wt.%) reduced activation steel have been investigated using differential scanning calorimetry and supplemented by microscopy characterisation. Accurate determination of the martensite start ( M S) and finish ( M f) temperatures as a function of cooling rate (1–99 K min −1) and holding time (1–120 min) in the γ-austenite phase field have been made. The critical cooling rate to form nearly 100% martensite is found to be of the order of 5–6 K min −1. The measured latent heat for the martensite transformation is found to be in the range 62–75 J g −1. In the case of austenitisation at 1323 K, it is found that the grain size of the parent austenite exhibited significant growth and the observed M S temperature too exhibited a systematic increase with austenite grain size. However, for those samples that are solution treated at a slightly lower temperature of 1253 K, the M S is found to be initially insensitive to the increase in holding time for up to about 30 min. This trend is followed later on by the usual increasing character of M S for further rise in the holding periods, up to about 120 min. This unusual initial behaviour is also reflected by the corresponding variation in the hardness values of the quenched in martensite. Moreover, the growth of parent austenite grains has also been restricted during the initial phase of solution annealing at 1253 K. This is attributed to the presence of undissolved carbide particles, which exert a pinning influence on the movement of austenite grain boundaries. The observed athermal martensite formation kinetics is described well by the Koistinen–Marburger relation.</description><subject>Applied sciences</subject><subject>Controled nuclear fusion plants</subject><subject>Energy</subject><subject>Energy. Thermal use of fuels</subject><subject>Exact sciences and technology</subject><subject>Fission nuclear power plants</subject><subject>Fuels</subject><subject>Installations for energy generation and conversion: thermal and electrical energy</subject><subject>Nuclear fuels</subject><issn>0022-3115</issn><issn>1873-4820</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2010</creationdate><recordtype>article</recordtype><recordid>eNqFUUtuFDEUbCGQGBKOgORNBCy682z3d4WiUUiQAmwCLC1_nsGjHvdgu4NmlzvkFhyLk-BJj9iycVmlevU-VRSvKFQUaHu-qTZ-1luZKgaZg64C3j4pVrTveFn3DJ4WKwDGSk5p87x4EeMGAJoBmlXx-4LENJs9mTzZypDQR5ecJrsfMiJJQfpop5C9XRY4T4Z1-HP_QL_lByrGvz4itPxWPv6a9qNfqGG9IPtE3vxK1dlbEtDMGg2ROrm7xTAmxJHM0fnvxDhrMaBPTo4kaun9gdVynILbYgr70-KZlWPEl0c8Kb68v7xdX5c3n68-rC9uSs07mspGqwYGoxX2SGVXK2Rt3aneKGM5ZdSA5Q2g5dpQJVutbduDwo4pqgwyyU-K14vvLkw_Z4xJbF3UOI7S4zRH0ddDXUPdQlY2i1KHKcaAVuzyrDLsBQVxiEZsxDEacYhGQCdyNLnu7NhB5kVHm6-sXfxXzDirB8qarHu36DCve-cwiKgd-nxEF1AnYSb3n05_ASidrX4</recordid><startdate>20101001</startdate><enddate>20101001</enddate><creator>Raju, S.</creator><creator>Jeya Ganesh, B.</creator><creator>Rai, Arun Kumar</creator><creator>Mythili, R.</creator><creator>Saroja, S.</creator><creator>Raj, Baldev</creator><general>Elsevier B.V</general><general>Elsevier</general><scope>IQODW</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7ST</scope><scope>C1K</scope><scope>SOI</scope></search><sort><creationdate>20101001</creationdate><title>A study on martensitic phase transformation in 9Cr–1W–0.23V–0.063Ta–0.56Mn–0.09C–0.02N (wt.%) reduced activation steel using differential scanning calorimetry</title><author>Raju, S. ; Jeya Ganesh, B. ; Rai, Arun Kumar ; Mythili, R. ; Saroja, S. ; Raj, Baldev</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c371t-5cb509dcbe8e1a74be2647b8dbdf3121d0f350ef3cd1ba6ccf680be72b1bde2a3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2010</creationdate><topic>Applied sciences</topic><topic>Controled nuclear fusion plants</topic><topic>Energy</topic><topic>Energy. Thermal use of fuels</topic><topic>Exact sciences and technology</topic><topic>Fission nuclear power plants</topic><topic>Fuels</topic><topic>Installations for energy generation and conversion: thermal and electrical energy</topic><topic>Nuclear fuels</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Raju, S.</creatorcontrib><creatorcontrib>Jeya Ganesh, B.</creatorcontrib><creatorcontrib>Rai, Arun Kumar</creatorcontrib><creatorcontrib>Mythili, R.</creatorcontrib><creatorcontrib>Saroja, S.</creatorcontrib><creatorcontrib>Raj, Baldev</creatorcontrib><collection>Pascal-Francis</collection><collection>CrossRef</collection><collection>Environment Abstracts</collection><collection>Environmental Sciences and Pollution Management</collection><collection>Environment Abstracts</collection><jtitle>Journal of nuclear materials</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Raju, S.</au><au>Jeya Ganesh, B.</au><au>Rai, Arun Kumar</au><au>Mythili, R.</au><au>Saroja, S.</au><au>Raj, Baldev</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>A study on martensitic phase transformation in 9Cr–1W–0.23V–0.063Ta–0.56Mn–0.09C–0.02N (wt.%) reduced activation steel using differential scanning calorimetry</atitle><jtitle>Journal of nuclear materials</jtitle><date>2010-10-01</date><risdate>2010</risdate><volume>405</volume><issue>1</issue><spage>59</spage><epage>69</epage><pages>59-69</pages><issn>0022-3115</issn><eissn>1873-4820</eissn><coden>JNUMAM</coden><abstract>The salient characteristics of martensite formation kinetics in 9Cr–1W–0.23V–0.063Ta–0.09C–0.02N (wt.%) reduced activation steel have been investigated using differential scanning calorimetry and supplemented by microscopy characterisation. Accurate determination of the martensite start ( M S) and finish ( M f) temperatures as a function of cooling rate (1–99 K min −1) and holding time (1–120 min) in the γ-austenite phase field have been made. The critical cooling rate to form nearly 100% martensite is found to be of the order of 5–6 K min −1. The measured latent heat for the martensite transformation is found to be in the range 62–75 J g −1. In the case of austenitisation at 1323 K, it is found that the grain size of the parent austenite exhibited significant growth and the observed M S temperature too exhibited a systematic increase with austenite grain size. However, for those samples that are solution treated at a slightly lower temperature of 1253 K, the M S is found to be initially insensitive to the increase in holding time for up to about 30 min. This trend is followed later on by the usual increasing character of M S for further rise in the holding periods, up to about 120 min. This unusual initial behaviour is also reflected by the corresponding variation in the hardness values of the quenched in martensite. Moreover, the growth of parent austenite grains has also been restricted during the initial phase of solution annealing at 1253 K. This is attributed to the presence of undissolved carbide particles, which exert a pinning influence on the movement of austenite grain boundaries. The observed athermal martensite formation kinetics is described well by the Koistinen–Marburger relation.</abstract><cop>Amsterdam</cop><pub>Elsevier B.V</pub><doi>10.1016/j.jnucmat.2010.07.036</doi><tpages>11</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0022-3115
ispartof Journal of nuclear materials, 2010-10, Vol.405 (1), p.59-69
issn 0022-3115
1873-4820
language eng
recordid cdi_proquest_miscellaneous_849440460
source Elsevier ScienceDirect Journals
subjects Applied sciences
Controled nuclear fusion plants
Energy
Energy. Thermal use of fuels
Exact sciences and technology
Fission nuclear power plants
Fuels
Installations for energy generation and conversion: thermal and electrical energy
Nuclear fuels
title A study on martensitic phase transformation in 9Cr–1W–0.23V–0.063Ta–0.56Mn–0.09C–0.02N (wt.%) reduced activation steel using differential scanning calorimetry
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-28T20%3A15%3A18IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=A%20study%20on%20martensitic%20phase%20transformation%20in%209Cr%E2%80%931W%E2%80%930.23V%E2%80%930.063Ta%E2%80%930.56Mn%E2%80%930.09C%E2%80%930.02N%20(wt.%25)%20reduced%20activation%20steel%20using%20differential%20scanning%20calorimetry&rft.jtitle=Journal%20of%20nuclear%20materials&rft.au=Raju,%20S.&rft.date=2010-10-01&rft.volume=405&rft.issue=1&rft.spage=59&rft.epage=69&rft.pages=59-69&rft.issn=0022-3115&rft.eissn=1873-4820&rft.coden=JNUMAM&rft_id=info:doi/10.1016/j.jnucmat.2010.07.036&rft_dat=%3Cproquest_cross%3E849440460%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=849440460&rft_id=info:pmid/&rft_els_id=S0022311510003466&rfr_iscdi=true