Prediction of swelling of 18Cr10NiTi austenitic steel over a wide range of displacement rates

The internal components of pressurized water reactors of Russian types WWER-440 and WWER-1000 are constructed of annealed 18Cr10NiTi steel, a close analog to AISI 321. Void swelling of the internals is a concern for plant life extension and predictive equations are required to assess the potential o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of nuclear materials 2010-04, Vol.399 (1), p.114-121
Hauptverfasser: Kalchenko, A.S., Bryk, V.V., Lazarev, N.P., Neklyudov, I.M., Voyevodin, V.N., Garner, F.A.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 121
container_issue 1
container_start_page 114
container_title Journal of nuclear materials
container_volume 399
creator Kalchenko, A.S.
Bryk, V.V.
Lazarev, N.P.
Neklyudov, I.M.
Voyevodin, V.N.
Garner, F.A.
description The internal components of pressurized water reactors of Russian types WWER-440 and WWER-1000 are constructed of annealed 18Cr10NiTi steel, a close analog to AISI 321. Void swelling of the internals is a concern for plant life extension and predictive equations are required to assess the potential of swelling in critical components such as the baffle ring or reflection shield that surrounds the WWER core. The only previously available swelling data for this steel were derived at higher than PWR-relevant displacement rates in the BOR-60 fast reactor. The swelling equation previously developed from these data does not incorporate the effect of displacement rate on swelling. Using heavy-ion irradiation at very high dpa rates (10 −2 and 10 −3 dpa s −1) and doses (5–100 dpa) and coupling the results to available neutron data a swelling equation has been developed that specifically incorporates the effect of dpa rate on void swelling. Experimental results allow description of the swelling peak, the incubation period and the steady-state swelling rate over a wide range of irradiation temperature. For the first time it appears possible to describe both ion and neutron data on this steel within the framework of a single empirical model. Swelling maps constructed from this model permit forecasting of the behavior of the steel in WWERs under the required irradiation conditions, not only at already attained exposure doses, but more importantly to higher dose levels that will be reached following plant life extension.
doi_str_mv 10.1016/j.jnucmat.2010.01.010
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_787274518</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0022311510000115</els_id><sourcerecordid>787274518</sourcerecordid><originalsourceid>FETCH-LOGICAL-c371t-2ceea03f63e3bc0b28e43b344027a228f47c0de47e6a9306a251fb00fb00ba633</originalsourceid><addsrcrecordid>eNqFUE1LAzEQDaJgrf4EIRfxtHWS7FdPIsUvKOqhHiVks7Mly262JmmL_94sLV6FGeYxvDfDe4RcM5gxYPldO2vtVvcqzDjEHbBYcEImrCxEkpYcTskEgPNEMJadkwvvWwDI5pBNyNeHw9roYAZLh4b6PXadsesRs3LhGLyZlaFq6wNaE4ymEWBHhx06quje1EidsmscBbXxm05p7NGGuA3oL8lZozqPV8c5JZ9Pj6vFS7J8f35dPCwTLQoWEq4RFYgmFygqDRUvMRWVSFPgheK8bNJCQ41pgbmaC8gVz1hTAYxdqVyIKbk93N244XuLPsjeeB2tKIvD1suiLHiRZqyMzOzA1G7w3mEjN870yv1IBnJMU7bymKYc05TAYkHU3Rw_KK9V10TT2vg_Med5yXLOI-_-wMNod2fQSa8NWh1DdqiDrAfzz6dfFlGNMg</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>787274518</pqid></control><display><type>article</type><title>Prediction of swelling of 18Cr10NiTi austenitic steel over a wide range of displacement rates</title><source>Elsevier ScienceDirect Journals Complete</source><creator>Kalchenko, A.S. ; Bryk, V.V. ; Lazarev, N.P. ; Neklyudov, I.M. ; Voyevodin, V.N. ; Garner, F.A.</creator><creatorcontrib>Kalchenko, A.S. ; Bryk, V.V. ; Lazarev, N.P. ; Neklyudov, I.M. ; Voyevodin, V.N. ; Garner, F.A.</creatorcontrib><description>The internal components of pressurized water reactors of Russian types WWER-440 and WWER-1000 are constructed of annealed 18Cr10NiTi steel, a close analog to AISI 321. Void swelling of the internals is a concern for plant life extension and predictive equations are required to assess the potential of swelling in critical components such as the baffle ring or reflection shield that surrounds the WWER core. The only previously available swelling data for this steel were derived at higher than PWR-relevant displacement rates in the BOR-60 fast reactor. The swelling equation previously developed from these data does not incorporate the effect of displacement rate on swelling. Using heavy-ion irradiation at very high dpa rates (10 −2 and 10 −3 dpa s −1) and doses (5–100 dpa) and coupling the results to available neutron data a swelling equation has been developed that specifically incorporates the effect of dpa rate on void swelling. Experimental results allow description of the swelling peak, the incubation period and the steady-state swelling rate over a wide range of irradiation temperature. For the first time it appears possible to describe both ion and neutron data on this steel within the framework of a single empirical model. Swelling maps constructed from this model permit forecasting of the behavior of the steel in WWERs under the required irradiation conditions, not only at already attained exposure doses, but more importantly to higher dose levels that will be reached following plant life extension.</description><identifier>ISSN: 0022-3115</identifier><identifier>EISSN: 1873-4820</identifier><identifier>DOI: 10.1016/j.jnucmat.2010.01.010</identifier><identifier>CODEN: JNUMAM</identifier><language>eng</language><publisher>Amsterdam: Elsevier B.V</publisher><subject>Applied sciences ; Austenitic stainless steels ; Controled nuclear fusion plants ; Displacement ; Energy ; Energy. Thermal use of fuels ; Exact sciences and technology ; Fission nuclear power plants ; Fuels ; Installations for energy generation and conversion: thermal and electrical energy ; Iron and steel plants ; Irradiation ; Mathematical analysis ; Mathematical models ; Nuclear fuels ; Structural steels ; Swelling ; Voids</subject><ispartof>Journal of nuclear materials, 2010-04, Vol.399 (1), p.114-121</ispartof><rights>2010 Elsevier B.V.</rights><rights>2015 INIST-CNRS</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c371t-2ceea03f63e3bc0b28e43b344027a228f47c0de47e6a9306a251fb00fb00ba633</citedby><cites>FETCH-LOGICAL-c371t-2ceea03f63e3bc0b28e43b344027a228f47c0de47e6a9306a251fb00fb00ba633</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://dx.doi.org/10.1016/j.jnucmat.2010.01.010$$EHTML$$P50$$Gelsevier$$H</linktohtml><link.rule.ids>314,780,784,3550,27924,27925,45995</link.rule.ids><backlink>$$Uhttp://pascal-francis.inist.fr/vibad/index.php?action=getRecordDetail&amp;idt=22681622$$DView record in Pascal Francis$$Hfree_for_read</backlink></links><search><creatorcontrib>Kalchenko, A.S.</creatorcontrib><creatorcontrib>Bryk, V.V.</creatorcontrib><creatorcontrib>Lazarev, N.P.</creatorcontrib><creatorcontrib>Neklyudov, I.M.</creatorcontrib><creatorcontrib>Voyevodin, V.N.</creatorcontrib><creatorcontrib>Garner, F.A.</creatorcontrib><title>Prediction of swelling of 18Cr10NiTi austenitic steel over a wide range of displacement rates</title><title>Journal of nuclear materials</title><description>The internal components of pressurized water reactors of Russian types WWER-440 and WWER-1000 are constructed of annealed 18Cr10NiTi steel, a close analog to AISI 321. Void swelling of the internals is a concern for plant life extension and predictive equations are required to assess the potential of swelling in critical components such as the baffle ring or reflection shield that surrounds the WWER core. The only previously available swelling data for this steel were derived at higher than PWR-relevant displacement rates in the BOR-60 fast reactor. The swelling equation previously developed from these data does not incorporate the effect of displacement rate on swelling. Using heavy-ion irradiation at very high dpa rates (10 −2 and 10 −3 dpa s −1) and doses (5–100 dpa) and coupling the results to available neutron data a swelling equation has been developed that specifically incorporates the effect of dpa rate on void swelling. Experimental results allow description of the swelling peak, the incubation period and the steady-state swelling rate over a wide range of irradiation temperature. For the first time it appears possible to describe both ion and neutron data on this steel within the framework of a single empirical model. Swelling maps constructed from this model permit forecasting of the behavior of the steel in WWERs under the required irradiation conditions, not only at already attained exposure doses, but more importantly to higher dose levels that will be reached following plant life extension.</description><subject>Applied sciences</subject><subject>Austenitic stainless steels</subject><subject>Controled nuclear fusion plants</subject><subject>Displacement</subject><subject>Energy</subject><subject>Energy. Thermal use of fuels</subject><subject>Exact sciences and technology</subject><subject>Fission nuclear power plants</subject><subject>Fuels</subject><subject>Installations for energy generation and conversion: thermal and electrical energy</subject><subject>Iron and steel plants</subject><subject>Irradiation</subject><subject>Mathematical analysis</subject><subject>Mathematical models</subject><subject>Nuclear fuels</subject><subject>Structural steels</subject><subject>Swelling</subject><subject>Voids</subject><issn>0022-3115</issn><issn>1873-4820</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2010</creationdate><recordtype>article</recordtype><recordid>eNqFUE1LAzEQDaJgrf4EIRfxtHWS7FdPIsUvKOqhHiVks7Mly262JmmL_94sLV6FGeYxvDfDe4RcM5gxYPldO2vtVvcqzDjEHbBYcEImrCxEkpYcTskEgPNEMJadkwvvWwDI5pBNyNeHw9roYAZLh4b6PXadsesRs3LhGLyZlaFq6wNaE4ymEWBHhx06quje1EidsmscBbXxm05p7NGGuA3oL8lZozqPV8c5JZ9Pj6vFS7J8f35dPCwTLQoWEq4RFYgmFygqDRUvMRWVSFPgheK8bNJCQ41pgbmaC8gVz1hTAYxdqVyIKbk93N244XuLPsjeeB2tKIvD1suiLHiRZqyMzOzA1G7w3mEjN870yv1IBnJMU7bymKYc05TAYkHU3Rw_KK9V10TT2vg_Med5yXLOI-_-wMNod2fQSa8NWh1DdqiDrAfzz6dfFlGNMg</recordid><startdate>20100401</startdate><enddate>20100401</enddate><creator>Kalchenko, A.S.</creator><creator>Bryk, V.V.</creator><creator>Lazarev, N.P.</creator><creator>Neklyudov, I.M.</creator><creator>Voyevodin, V.N.</creator><creator>Garner, F.A.</creator><general>Elsevier B.V</general><general>Elsevier</general><scope>IQODW</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7SR</scope><scope>7TB</scope><scope>7U5</scope><scope>8BQ</scope><scope>8FD</scope><scope>FR3</scope><scope>JG9</scope><scope>L7M</scope></search><sort><creationdate>20100401</creationdate><title>Prediction of swelling of 18Cr10NiTi austenitic steel over a wide range of displacement rates</title><author>Kalchenko, A.S. ; Bryk, V.V. ; Lazarev, N.P. ; Neklyudov, I.M. ; Voyevodin, V.N. ; Garner, F.A.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c371t-2ceea03f63e3bc0b28e43b344027a228f47c0de47e6a9306a251fb00fb00ba633</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2010</creationdate><topic>Applied sciences</topic><topic>Austenitic stainless steels</topic><topic>Controled nuclear fusion plants</topic><topic>Displacement</topic><topic>Energy</topic><topic>Energy. Thermal use of fuels</topic><topic>Exact sciences and technology</topic><topic>Fission nuclear power plants</topic><topic>Fuels</topic><topic>Installations for energy generation and conversion: thermal and electrical energy</topic><topic>Iron and steel plants</topic><topic>Irradiation</topic><topic>Mathematical analysis</topic><topic>Mathematical models</topic><topic>Nuclear fuels</topic><topic>Structural steels</topic><topic>Swelling</topic><topic>Voids</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Kalchenko, A.S.</creatorcontrib><creatorcontrib>Bryk, V.V.</creatorcontrib><creatorcontrib>Lazarev, N.P.</creatorcontrib><creatorcontrib>Neklyudov, I.M.</creatorcontrib><creatorcontrib>Voyevodin, V.N.</creatorcontrib><creatorcontrib>Garner, F.A.</creatorcontrib><collection>Pascal-Francis</collection><collection>CrossRef</collection><collection>Engineered Materials Abstracts</collection><collection>Mechanical &amp; Transportation Engineering Abstracts</collection><collection>Solid State and Superconductivity Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Engineering Research Database</collection><collection>Materials Research Database</collection><collection>Advanced Technologies Database with Aerospace</collection><jtitle>Journal of nuclear materials</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Kalchenko, A.S.</au><au>Bryk, V.V.</au><au>Lazarev, N.P.</au><au>Neklyudov, I.M.</au><au>Voyevodin, V.N.</au><au>Garner, F.A.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Prediction of swelling of 18Cr10NiTi austenitic steel over a wide range of displacement rates</atitle><jtitle>Journal of nuclear materials</jtitle><date>2010-04-01</date><risdate>2010</risdate><volume>399</volume><issue>1</issue><spage>114</spage><epage>121</epage><pages>114-121</pages><issn>0022-3115</issn><eissn>1873-4820</eissn><coden>JNUMAM</coden><abstract>The internal components of pressurized water reactors of Russian types WWER-440 and WWER-1000 are constructed of annealed 18Cr10NiTi steel, a close analog to AISI 321. Void swelling of the internals is a concern for plant life extension and predictive equations are required to assess the potential of swelling in critical components such as the baffle ring or reflection shield that surrounds the WWER core. The only previously available swelling data for this steel were derived at higher than PWR-relevant displacement rates in the BOR-60 fast reactor. The swelling equation previously developed from these data does not incorporate the effect of displacement rate on swelling. Using heavy-ion irradiation at very high dpa rates (10 −2 and 10 −3 dpa s −1) and doses (5–100 dpa) and coupling the results to available neutron data a swelling equation has been developed that specifically incorporates the effect of dpa rate on void swelling. Experimental results allow description of the swelling peak, the incubation period and the steady-state swelling rate over a wide range of irradiation temperature. For the first time it appears possible to describe both ion and neutron data on this steel within the framework of a single empirical model. Swelling maps constructed from this model permit forecasting of the behavior of the steel in WWERs under the required irradiation conditions, not only at already attained exposure doses, but more importantly to higher dose levels that will be reached following plant life extension.</abstract><cop>Amsterdam</cop><pub>Elsevier B.V</pub><doi>10.1016/j.jnucmat.2010.01.010</doi><tpages>8</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0022-3115
ispartof Journal of nuclear materials, 2010-04, Vol.399 (1), p.114-121
issn 0022-3115
1873-4820
language eng
recordid cdi_proquest_miscellaneous_787274518
source Elsevier ScienceDirect Journals Complete
subjects Applied sciences
Austenitic stainless steels
Controled nuclear fusion plants
Displacement
Energy
Energy. Thermal use of fuels
Exact sciences and technology
Fission nuclear power plants
Fuels
Installations for energy generation and conversion: thermal and electrical energy
Iron and steel plants
Irradiation
Mathematical analysis
Mathematical models
Nuclear fuels
Structural steels
Swelling
Voids
title Prediction of swelling of 18Cr10NiTi austenitic steel over a wide range of displacement rates
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T13%3A43%3A59IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Prediction%20of%20swelling%20of%2018Cr10NiTi%20austenitic%20steel%20over%20a%20wide%20range%20of%20displacement%20rates&rft.jtitle=Journal%20of%20nuclear%20materials&rft.au=Kalchenko,%20A.S.&rft.date=2010-04-01&rft.volume=399&rft.issue=1&rft.spage=114&rft.epage=121&rft.pages=114-121&rft.issn=0022-3115&rft.eissn=1873-4820&rft.coden=JNUMAM&rft_id=info:doi/10.1016/j.jnucmat.2010.01.010&rft_dat=%3Cproquest_cross%3E787274518%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=787274518&rft_id=info:pmid/&rft_els_id=S0022311510000115&rfr_iscdi=true