Wear resistance of isosit and polymethyl methacrylate occlusal splint material

Simulated occlusal wear utilizing the artifical mouth included natural enamel against isosit and polymethyl methacrylate splint materials. The results reported in volume loss (mm 3) demonstrated the isosit material to be 55–67% more resistant to wear than polymethyl methacrylate. No wear occurred on...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Dental materials 1987-04, Vol.3 (2), p.82-84
Hauptverfasser: Schulte, J.K., Anderson, G.C., Sakaguchi, R.L., DeLong, R.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Simulated occlusal wear utilizing the artifical mouth included natural enamel against isosit and polymethyl methacrylate splint materials. The results reported in volume loss (mm 3) demonstrated the isosit material to be 55–67% more resistant to wear than polymethyl methacrylate. No wear occurred on the enamel surface opposing either splint material.
ISSN:0109-5641