Strip Casting by a Single Roll Caster Equipped with a Scraper

A scraper was equipped to a single roll caster to improve the free solidified surface. The scraper contacted to the free solidified surface at the constant force. The some mount of semisolid layer at the surface was removed and the surface became flat. The scraper was made from the mild steel plate....

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Key engineering materials 2010-01, Vol.443, p.122-127
Hauptverfasser: Akitsu, Kazuya, Watari, Hisaki, Kumai, Shinji, Yamabayashi, Takanori, Nakamura, Ryoji
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 127
container_issue
container_start_page 122
container_title Key engineering materials
container_volume 443
creator Akitsu, Kazuya
Watari, Hisaki
Kumai, Shinji
Yamabayashi, Takanori
Nakamura, Ryoji
description A scraper was equipped to a single roll caster to improve the free solidified surface. The scraper contacted to the free solidified surface at the constant force. The some mount of semisolid layer at the surface was removed and the surface became flat. The scraper was made from the mild steel plate. The mild steel plate was covered by the insulator paper to prevent the cooling of the melt by the plate. The melt pool was made on the roll by the side dam plates, back dam plate and the scraper. Therefore, a tip or a nozzle was not needed. The AA5182 and AA6022 aluminum alloy were cast. The as-cast strips could be cold rolled. The microstructure of as-cast strip was not uniform at thickness direction. However, the microstructure became uniform after the cold rolling and the annealing.
doi_str_mv 10.4028/www.scientific.net/KEM.443.122
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_753684499</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>753684499</sourcerecordid><originalsourceid>FETCH-LOGICAL-c465t-99d52635f7603b83855b199607c3b495fc8855884229efa4df6c96c2521824173</originalsourceid><addsrcrecordid>eNqNkF1LwzAUhoMoOKf_oVd61S7fTS4UZcwPnAhOr0OWpS6ja2uSUvbvzZzgrVfn5ZyXB84DwCWCBYVYTIZhKIJxtomucqZobJw8z14KSkmBMD4CI8Q5zmUp2XHKEJFcCsxPwVkIGwgJEoiNwPUietdlUx2iaz6z5S7T2SKl2mZvbV3_HKzPZl-96zq7ygYX1_uK8bqz_hycVLoO9uJ3jsHH_ex9-pjPXx-epnfz3FDOYi7limFOWFVySJaCCMaWSEoOS0OWVLLKiLQSgmIsbaXpquJGcoMZRgJTVJIxuDpwO99-9TZEtXXB2LrWjW37oEpGuKBUytS8OTSNb0PwtlKdd1vtdwpBtdemkjb1p00lbSppU0mbStoS4PYAiF436XezVpu2901677-Ib596fHE</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>753684499</pqid></control><display><type>article</type><title>Strip Casting by a Single Roll Caster Equipped with a Scraper</title><source>Scientific.net Journals</source><creator>Akitsu, Kazuya ; Watari, Hisaki ; Kumai, Shinji ; Yamabayashi, Takanori ; Nakamura, Ryoji</creator><creatorcontrib>Akitsu, Kazuya ; Watari, Hisaki ; Kumai, Shinji ; Yamabayashi, Takanori ; Nakamura, Ryoji</creatorcontrib><description>A scraper was equipped to a single roll caster to improve the free solidified surface. The scraper contacted to the free solidified surface at the constant force. The some mount of semisolid layer at the surface was removed and the surface became flat. The scraper was made from the mild steel plate. The mild steel plate was covered by the insulator paper to prevent the cooling of the melt by the plate. The melt pool was made on the roll by the side dam plates, back dam plate and the scraper. Therefore, a tip or a nozzle was not needed. The AA5182 and AA6022 aluminum alloy were cast. The as-cast strips could be cold rolled. The microstructure of as-cast strip was not uniform at thickness direction. However, the microstructure became uniform after the cold rolling and the annealing.</description><identifier>ISSN: 1013-9826</identifier><identifier>ISSN: 1662-9795</identifier><identifier>EISSN: 1662-9795</identifier><identifier>DOI: 10.4028/www.scientific.net/KEM.443.122</identifier><language>eng</language><publisher>Trans Tech Publications Ltd</publisher><subject>Aluminum base alloys ; Annealing ; Carbon steels ; Cold rolling ; Cooling ; Covering ; Insulators ; Melt pools ; Melts ; Microstructure ; Nozzles ; Rolls ; Scrapers ; Semisolids ; Strip ; Strip casting</subject><ispartof>Key engineering materials, 2010-01, Vol.443, p.122-127</ispartof><rights>2010 Trans Tech Publications Ltd</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c465t-99d52635f7603b83855b199607c3b495fc8855884229efa4df6c96c2521824173</citedby></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Uhttps://www.scientific.net/Image/TitleCover/934?width=600</thumbnail><link.rule.ids>314,776,780,27901,27902</link.rule.ids></links><search><creatorcontrib>Akitsu, Kazuya</creatorcontrib><creatorcontrib>Watari, Hisaki</creatorcontrib><creatorcontrib>Kumai, Shinji</creatorcontrib><creatorcontrib>Yamabayashi, Takanori</creatorcontrib><creatorcontrib>Nakamura, Ryoji</creatorcontrib><title>Strip Casting by a Single Roll Caster Equipped with a Scraper</title><title>Key engineering materials</title><description>A scraper was equipped to a single roll caster to improve the free solidified surface. The scraper contacted to the free solidified surface at the constant force. The some mount of semisolid layer at the surface was removed and the surface became flat. The scraper was made from the mild steel plate. The mild steel plate was covered by the insulator paper to prevent the cooling of the melt by the plate. The melt pool was made on the roll by the side dam plates, back dam plate and the scraper. Therefore, a tip or a nozzle was not needed. The AA5182 and AA6022 aluminum alloy were cast. The as-cast strips could be cold rolled. The microstructure of as-cast strip was not uniform at thickness direction. However, the microstructure became uniform after the cold rolling and the annealing.</description><subject>Aluminum base alloys</subject><subject>Annealing</subject><subject>Carbon steels</subject><subject>Cold rolling</subject><subject>Cooling</subject><subject>Covering</subject><subject>Insulators</subject><subject>Melt pools</subject><subject>Melts</subject><subject>Microstructure</subject><subject>Nozzles</subject><subject>Rolls</subject><subject>Scrapers</subject><subject>Semisolids</subject><subject>Strip</subject><subject>Strip casting</subject><issn>1013-9826</issn><issn>1662-9795</issn><issn>1662-9795</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2010</creationdate><recordtype>article</recordtype><recordid>eNqNkF1LwzAUhoMoOKf_oVd61S7fTS4UZcwPnAhOr0OWpS6ja2uSUvbvzZzgrVfn5ZyXB84DwCWCBYVYTIZhKIJxtomucqZobJw8z14KSkmBMD4CI8Q5zmUp2XHKEJFcCsxPwVkIGwgJEoiNwPUietdlUx2iaz6z5S7T2SKl2mZvbV3_HKzPZl-96zq7ygYX1_uK8bqz_hycVLoO9uJ3jsHH_ex9-pjPXx-epnfz3FDOYi7limFOWFVySJaCCMaWSEoOS0OWVLLKiLQSgmIsbaXpquJGcoMZRgJTVJIxuDpwO99-9TZEtXXB2LrWjW37oEpGuKBUytS8OTSNb0PwtlKdd1vtdwpBtdemkjb1p00lbSppU0mbStoS4PYAiF436XezVpu2901677-Ib596fHE</recordid><startdate>20100101</startdate><enddate>20100101</enddate><creator>Akitsu, Kazuya</creator><creator>Watari, Hisaki</creator><creator>Kumai, Shinji</creator><creator>Yamabayashi, Takanori</creator><creator>Nakamura, Ryoji</creator><general>Trans Tech Publications Ltd</general><scope>AAYXX</scope><scope>CITATION</scope><scope>7QF</scope><scope>7SR</scope><scope>8BQ</scope><scope>8FD</scope><scope>JG9</scope></search><sort><creationdate>20100101</creationdate><title>Strip Casting by a Single Roll Caster Equipped with a Scraper</title><author>Akitsu, Kazuya ; Watari, Hisaki ; Kumai, Shinji ; Yamabayashi, Takanori ; Nakamura, Ryoji</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c465t-99d52635f7603b83855b199607c3b495fc8855884229efa4df6c96c2521824173</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2010</creationdate><topic>Aluminum base alloys</topic><topic>Annealing</topic><topic>Carbon steels</topic><topic>Cold rolling</topic><topic>Cooling</topic><topic>Covering</topic><topic>Insulators</topic><topic>Melt pools</topic><topic>Melts</topic><topic>Microstructure</topic><topic>Nozzles</topic><topic>Rolls</topic><topic>Scrapers</topic><topic>Semisolids</topic><topic>Strip</topic><topic>Strip casting</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Akitsu, Kazuya</creatorcontrib><creatorcontrib>Watari, Hisaki</creatorcontrib><creatorcontrib>Kumai, Shinji</creatorcontrib><creatorcontrib>Yamabayashi, Takanori</creatorcontrib><creatorcontrib>Nakamura, Ryoji</creatorcontrib><collection>CrossRef</collection><collection>Aluminium Industry Abstracts</collection><collection>Engineered Materials Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><jtitle>Key engineering materials</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Akitsu, Kazuya</au><au>Watari, Hisaki</au><au>Kumai, Shinji</au><au>Yamabayashi, Takanori</au><au>Nakamura, Ryoji</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Strip Casting by a Single Roll Caster Equipped with a Scraper</atitle><jtitle>Key engineering materials</jtitle><date>2010-01-01</date><risdate>2010</risdate><volume>443</volume><spage>122</spage><epage>127</epage><pages>122-127</pages><issn>1013-9826</issn><issn>1662-9795</issn><eissn>1662-9795</eissn><abstract>A scraper was equipped to a single roll caster to improve the free solidified surface. The scraper contacted to the free solidified surface at the constant force. The some mount of semisolid layer at the surface was removed and the surface became flat. The scraper was made from the mild steel plate. The mild steel plate was covered by the insulator paper to prevent the cooling of the melt by the plate. The melt pool was made on the roll by the side dam plates, back dam plate and the scraper. Therefore, a tip or a nozzle was not needed. The AA5182 and AA6022 aluminum alloy were cast. The as-cast strips could be cold rolled. The microstructure of as-cast strip was not uniform at thickness direction. However, the microstructure became uniform after the cold rolling and the annealing.</abstract><pub>Trans Tech Publications Ltd</pub><doi>10.4028/www.scientific.net/KEM.443.122</doi><tpages>6</tpages></addata></record>
fulltext fulltext
identifier ISSN: 1013-9826
ispartof Key engineering materials, 2010-01, Vol.443, p.122-127
issn 1013-9826
1662-9795
1662-9795
language eng
recordid cdi_proquest_miscellaneous_753684499
source Scientific.net Journals
subjects Aluminum base alloys
Annealing
Carbon steels
Cold rolling
Cooling
Covering
Insulators
Melt pools
Melts
Microstructure
Nozzles
Rolls
Scrapers
Semisolids
Strip
Strip casting
title Strip Casting by a Single Roll Caster Equipped with a Scraper
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-09T08%3A50%3A23IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Strip%20Casting%20by%20a%20Single%20Roll%20Caster%20Equipped%20with%20a%20Scraper&rft.jtitle=Key%20engineering%20materials&rft.au=Akitsu,%20Kazuya&rft.date=2010-01-01&rft.volume=443&rft.spage=122&rft.epage=127&rft.pages=122-127&rft.issn=1013-9826&rft.eissn=1662-9795&rft_id=info:doi/10.4028/www.scientific.net/KEM.443.122&rft_dat=%3Cproquest_cross%3E753684499%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=753684499&rft_id=info:pmid/&rfr_iscdi=true