AC anodization of aluminum, electrodeposition of nickel and optical property examination

Commercial grade aluminum was anodized to form porous anodic films using alternating current at a voltage of 15 V and a temperature of 25°C. The AC anodization was implemented in phosphoric acid and in an electrolyte modified by dissolving 1.1 g/l iron powder. The presence of iron species in the mod...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Solar energy materials and solar cells 2000-10, Vol.64 (3), p.279-289