Evolution of secondary phases in Cr-V low-alloy steels during aging

The influence of both bulk vanadium content and aging conditions on the evolution of secondary phases in Cr-V low-alloy steels was studied. Three 0.1C-0.9Cr-V steels with different vanadium contents (0, 0.258, and 0.512 wt pct) were aged for 100 to 5,000 hours at 773, 853, 953, and 993 K. In the inv...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Metallurgical and materials transactions. A, Physical metallurgy and materials science Physical metallurgy and materials science, 2004-03, Vol.35 (3), p.751-759
Hauptverfasser: JANOVEC, J, VYROSTKOVA, A, SVOBODA, M, KROUPA, A, GRABKE, H. J