Effects of temperature and strain rate on tensile properties and activation energy for dynamic strain aging in alloy 625

Alloy 625 ammonia cracker tubes were service exposed for 60,000 hours at 873K. These were then subjected to a solution-annealing treatment at 1473 K for 0.5 hours. The effects of temperature and strain rate on the tensile properties of the solution-annealed alloy were examined in the temperature ran...