Permanent Bubble Arrays from a Cross-Linked Poly(p ara-phenyleneethynylene): Picoliter Holes without Microfabrication
An azide-substituted poly(para-phenyleneethynylene) (PPE) 4 was prepared by the Heck−Cassar−Sonogashira−Hagihara method. Thin films of 4 form self-assembled bubble arrays from carbon disulfide solution utilizing the breath figure method. The as-formed porous films of 4 are soluble in common solvents...
Gespeichert in:
Veröffentlicht in: | Journal of the American Chemical Society 2004-03, Vol.126 (12), p.3678-3679 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 3679 |
---|---|
container_issue | 12 |
container_start_page | 3678 |
container_title | Journal of the American Chemical Society |
container_volume | 126 |
creator | Erdogan, Belma Song, Lulu Wilson, James N Park, Jung O Srinivasarao, Mohan Bunz, Uwe H. F |
description | An azide-substituted poly(para-phenyleneethynylene) (PPE) 4 was prepared by the Heck−Cassar−Sonogashira−Hagihara method. Thin films of 4 form self-assembled bubble arrays from carbon disulfide solution utilizing the breath figure method. The as-formed porous films of 4 are soluble in common solvents, and the air bubbles are interconnected. Upon heating to 300 °C, 4 cross-links and the thin film turn into insoluble matrix with isolated bubbles. The cross-linking process has transformed the bubble arrays of 4 into insoluble picoliter beakers or picoliter vials, whose diameters are approximately 3.0 and 1.5 μm at the top and bottom, respectively. |
doi_str_mv | 10.1021/ja0320020 |
format | Article |
fullrecord | <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_71754869</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>71754869</sourcerecordid><originalsourceid>FETCH-LOGICAL-a416t-29965cd75887f1e65b30d6ad9dc77d99501ba69c2d5090bff98bed61fe4a4b5c3</originalsourceid><addsrcrecordid>eNptkMGO0zAURS0EYsrAgh9A3oCYRcB2ajue3VBRBlFEJQaQ2FgvzovqThIXOxGTHVt-ky8hVasZFqxsPx9dvXsIecrZK84Ef70FlgvGBLtHZlwKlkku1H0yY9Ms04XKT8ijlLbTcy4K_pCccMnyQhk9IzdrjC102PX0zVCWDdKLGGFMtI6hpUAXMaSUrXx3jRVdh2Z8uaMQIdttsBsb7BD7zXi4nZ3_-fWbrr0Lje8x0svQYKI_fb8JQ08_ehdDDWX0DnofusfkQQ1NwifH85R8Wb69Wlxmq0_v3i8uVhnMueozYYySrtKyKHTNUckyZ5WCylRO68oYyXgJyjhRSWZYWdemKLFSvMY5zEvp8lPy4pC7i-HHgKm3rU8Om2YqHYZkNddyPrmYwLMD6PaVI9Z2F30LcbSc2b1me6t5Yp8dQ4eyxeqOPHqdgOdHAJKDpo7QOZ_-4RQzhdxz2YHzqceb23-I11bpXEt7tf5sxYevy-9iubDf7nLBJbsNQ-wmd_9Z8C_VCaHP</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>71754869</pqid></control><display><type>article</type><title>Permanent Bubble Arrays from a Cross-Linked Poly(p ara-phenyleneethynylene): Picoliter Holes without Microfabrication</title><source>American Chemical Society Journals</source><creator>Erdogan, Belma ; Song, Lulu ; Wilson, James N ; Park, Jung O ; Srinivasarao, Mohan ; Bunz, Uwe H. F</creator><creatorcontrib>Erdogan, Belma ; Song, Lulu ; Wilson, James N ; Park, Jung O ; Srinivasarao, Mohan ; Bunz, Uwe H. F</creatorcontrib><description>An azide-substituted poly(para-phenyleneethynylene) (PPE) 4 was prepared by the Heck−Cassar−Sonogashira−Hagihara method. Thin films of 4 form self-assembled bubble arrays from carbon disulfide solution utilizing the breath figure method. The as-formed porous films of 4 are soluble in common solvents, and the air bubbles are interconnected. Upon heating to 300 °C, 4 cross-links and the thin film turn into insoluble matrix with isolated bubbles. The cross-linking process has transformed the bubble arrays of 4 into insoluble picoliter beakers or picoliter vials, whose diameters are approximately 3.0 and 1.5 μm at the top and bottom, respectively.</description><identifier>ISSN: 0002-7863</identifier><identifier>EISSN: 1520-5126</identifier><identifier>DOI: 10.1021/ja0320020</identifier><identifier>PMID: 15038697</identifier><identifier>CODEN: JACSAT</identifier><language>eng</language><publisher>Washington, DC: American Chemical Society</publisher><subject>Analytical chemistry ; Chemistry ; Exact sciences and technology ; General, instrumentation</subject><ispartof>Journal of the American Chemical Society, 2004-03, Vol.126 (12), p.3678-3679</ispartof><rights>Copyright © 2004 American Chemical Society</rights><rights>2004 INIST-CNRS</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-a416t-29965cd75887f1e65b30d6ad9dc77d99501ba69c2d5090bff98bed61fe4a4b5c3</citedby><cites>FETCH-LOGICAL-a416t-29965cd75887f1e65b30d6ad9dc77d99501ba69c2d5090bff98bed61fe4a4b5c3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://pubs.acs.org/doi/pdf/10.1021/ja0320020$$EPDF$$P50$$Gacs$$H</linktopdf><linktohtml>$$Uhttps://pubs.acs.org/doi/10.1021/ja0320020$$EHTML$$P50$$Gacs$$H</linktohtml><link.rule.ids>314,780,784,2765,27076,27924,27925,56738,56788</link.rule.ids><backlink>$$Uhttp://pascal-francis.inist.fr/vibad/index.php?action=getRecordDetail&idt=15609857$$DView record in Pascal Francis$$Hfree_for_read</backlink><backlink>$$Uhttps://www.ncbi.nlm.nih.gov/pubmed/15038697$$D View this record in MEDLINE/PubMed$$Hfree_for_read</backlink></links><search><creatorcontrib>Erdogan, Belma</creatorcontrib><creatorcontrib>Song, Lulu</creatorcontrib><creatorcontrib>Wilson, James N</creatorcontrib><creatorcontrib>Park, Jung O</creatorcontrib><creatorcontrib>Srinivasarao, Mohan</creatorcontrib><creatorcontrib>Bunz, Uwe H. F</creatorcontrib><title>Permanent Bubble Arrays from a Cross-Linked Poly(p ara-phenyleneethynylene): Picoliter Holes without Microfabrication</title><title>Journal of the American Chemical Society</title><addtitle>J. Am. Chem. Soc</addtitle><description>An azide-substituted poly(para-phenyleneethynylene) (PPE) 4 was prepared by the Heck−Cassar−Sonogashira−Hagihara method. Thin films of 4 form self-assembled bubble arrays from carbon disulfide solution utilizing the breath figure method. The as-formed porous films of 4 are soluble in common solvents, and the air bubbles are interconnected. Upon heating to 300 °C, 4 cross-links and the thin film turn into insoluble matrix with isolated bubbles. The cross-linking process has transformed the bubble arrays of 4 into insoluble picoliter beakers or picoliter vials, whose diameters are approximately 3.0 and 1.5 μm at the top and bottom, respectively.</description><subject>Analytical chemistry</subject><subject>Chemistry</subject><subject>Exact sciences and technology</subject><subject>General, instrumentation</subject><issn>0002-7863</issn><issn>1520-5126</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2004</creationdate><recordtype>article</recordtype><recordid>eNptkMGO0zAURS0EYsrAgh9A3oCYRcB2ajue3VBRBlFEJQaQ2FgvzovqThIXOxGTHVt-ky8hVasZFqxsPx9dvXsIecrZK84Ef70FlgvGBLtHZlwKlkku1H0yY9Ms04XKT8ijlLbTcy4K_pCccMnyQhk9IzdrjC102PX0zVCWDdKLGGFMtI6hpUAXMaSUrXx3jRVdh2Z8uaMQIdttsBsb7BD7zXi4nZ3_-fWbrr0Lje8x0svQYKI_fb8JQ08_ehdDDWX0DnofusfkQQ1NwifH85R8Wb69Wlxmq0_v3i8uVhnMueozYYySrtKyKHTNUckyZ5WCylRO68oYyXgJyjhRSWZYWdemKLFSvMY5zEvp8lPy4pC7i-HHgKm3rU8Om2YqHYZkNddyPrmYwLMD6PaVI9Z2F30LcbSc2b1me6t5Yp8dQ4eyxeqOPHqdgOdHAJKDpo7QOZ_-4RQzhdxz2YHzqceb23-I11bpXEt7tf5sxYevy-9iubDf7nLBJbsNQ-wmd_9Z8C_VCaHP</recordid><startdate>20040331</startdate><enddate>20040331</enddate><creator>Erdogan, Belma</creator><creator>Song, Lulu</creator><creator>Wilson, James N</creator><creator>Park, Jung O</creator><creator>Srinivasarao, Mohan</creator><creator>Bunz, Uwe H. F</creator><general>American Chemical Society</general><scope>BSCLL</scope><scope>IQODW</scope><scope>NPM</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7X8</scope></search><sort><creationdate>20040331</creationdate><title>Permanent Bubble Arrays from a Cross-Linked Poly(p ara-phenyleneethynylene): Picoliter Holes without Microfabrication</title><author>Erdogan, Belma ; Song, Lulu ; Wilson, James N ; Park, Jung O ; Srinivasarao, Mohan ; Bunz, Uwe H. F</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-a416t-29965cd75887f1e65b30d6ad9dc77d99501ba69c2d5090bff98bed61fe4a4b5c3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2004</creationdate><topic>Analytical chemistry</topic><topic>Chemistry</topic><topic>Exact sciences and technology</topic><topic>General, instrumentation</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Erdogan, Belma</creatorcontrib><creatorcontrib>Song, Lulu</creatorcontrib><creatorcontrib>Wilson, James N</creatorcontrib><creatorcontrib>Park, Jung O</creatorcontrib><creatorcontrib>Srinivasarao, Mohan</creatorcontrib><creatorcontrib>Bunz, Uwe H. F</creatorcontrib><collection>Istex</collection><collection>Pascal-Francis</collection><collection>PubMed</collection><collection>CrossRef</collection><collection>MEDLINE - Academic</collection><jtitle>Journal of the American Chemical Society</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Erdogan, Belma</au><au>Song, Lulu</au><au>Wilson, James N</au><au>Park, Jung O</au><au>Srinivasarao, Mohan</au><au>Bunz, Uwe H. F</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Permanent Bubble Arrays from a Cross-Linked Poly(p ara-phenyleneethynylene): Picoliter Holes without Microfabrication</atitle><jtitle>Journal of the American Chemical Society</jtitle><addtitle>J. Am. Chem. Soc</addtitle><date>2004-03-31</date><risdate>2004</risdate><volume>126</volume><issue>12</issue><spage>3678</spage><epage>3679</epage><pages>3678-3679</pages><issn>0002-7863</issn><eissn>1520-5126</eissn><coden>JACSAT</coden><abstract>An azide-substituted poly(para-phenyleneethynylene) (PPE) 4 was prepared by the Heck−Cassar−Sonogashira−Hagihara method. Thin films of 4 form self-assembled bubble arrays from carbon disulfide solution utilizing the breath figure method. The as-formed porous films of 4 are soluble in common solvents, and the air bubbles are interconnected. Upon heating to 300 °C, 4 cross-links and the thin film turn into insoluble matrix with isolated bubbles. The cross-linking process has transformed the bubble arrays of 4 into insoluble picoliter beakers or picoliter vials, whose diameters are approximately 3.0 and 1.5 μm at the top and bottom, respectively.</abstract><cop>Washington, DC</cop><pub>American Chemical Society</pub><pmid>15038697</pmid><doi>10.1021/ja0320020</doi><tpages>2</tpages></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0002-7863 |
ispartof | Journal of the American Chemical Society, 2004-03, Vol.126 (12), p.3678-3679 |
issn | 0002-7863 1520-5126 |
language | eng |
recordid | cdi_proquest_miscellaneous_71754869 |
source | American Chemical Society Journals |
subjects | Analytical chemistry Chemistry Exact sciences and technology General, instrumentation |
title | Permanent Bubble Arrays from a Cross-Linked Poly(p ara-phenyleneethynylene): Picoliter Holes without Microfabrication |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T04%3A13%3A54IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Permanent%20Bubble%20Arrays%20from%20a%20Cross-Linked%20Poly(p%20ara-phenyleneethynylene):%E2%80%89%20Picoliter%20Holes%20without%20Microfabrication&rft.jtitle=Journal%20of%20the%20American%20Chemical%20Society&rft.au=Erdogan,%20Belma&rft.date=2004-03-31&rft.volume=126&rft.issue=12&rft.spage=3678&rft.epage=3679&rft.pages=3678-3679&rft.issn=0002-7863&rft.eissn=1520-5126&rft.coden=JACSAT&rft_id=info:doi/10.1021/ja0320020&rft_dat=%3Cproquest_cross%3E71754869%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=71754869&rft_id=info:pmid/15038697&rfr_iscdi=true |