Effects of Alumina-blasting and Adhesive Primers on Bonding between Resin Luting Agent and Zirconia Ceramics

This study evaluated the effect of alumina-blasting and three commercial adhesive primers on the shear bond strength of a dual-cured resin luting agent to zirconia ceramics. Two different-sized zirconia ceramic specimens were treated with or without alumina-blasting and then treated with one of thre...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Dental Materials Journal 2006, Vol.25(4), pp.669-674
Hauptverfasser: TSUO, Yukiko, YOSHIDA, Keiichi, ATSUTA, Mitsuru
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 674
container_issue 4
container_start_page 669
container_title Dental Materials Journal
container_volume 25
creator TSUO, Yukiko
YOSHIDA, Keiichi
ATSUTA, Mitsuru
description This study evaluated the effect of alumina-blasting and three commercial adhesive primers on the shear bond strength of a dual-cured resin luting agent to zirconia ceramics. Two different-sized zirconia ceramic specimens were treated with or without alumina-blasting and then treated with one of three adhesive primers. Subsequently, specimens were cemented together with Linkmax HV (GC). Half of the specimens were stored in water at 37°C for 24 hours and the other half thermocycled 10,000 times before shear bond strength testing. For groups treated with either alumina-blasting or primer, shear bond strength significantly decreased after thermal cycling. For groups treated with both alumina-blasting and one of the three primers, there were no significant differences in shear bond strength before and after thermal cycling (p
doi_str_mv 10.4012/dmj.25.669
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_68322135</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>68322135</sourcerecordid><originalsourceid>FETCH-LOGICAL-c568t-52eb6ad10608428045b6ecd2e64c1dcea3176b4b0892c518a9a55d468be9906d3</originalsourceid><addsrcrecordid>eNpF0EFP2zAUB3ALMa2F7cIHQD5xQEpnO7brnFCpyoZUadO0XXaxHPuldZU4YCegffsZUtjF7_B-7y_5j9AFJQtOKPviusOCiYWU1QmaU6VoQUtJT9GcMLUsuODLGTpL6UAIr6RSH9GMLstSsaqao3bTNGCHhPsGr9qx88EUdWvS4MMOm-Dwyu0h-SfAP6LvIGYY8G0f3Mu-huEZIOCfWQS8HV-PVjsIw-vpHx9tH7zBa4im8zZ9Qh8a0yb4fJzn6Pfd5tf6W7H9_vV-vdoWVkg1FIJBLY2jRBLFmSJc1BKsYyC5pc6CKelS1rwmqmJWUGUqI4TjUtVQVUS68hxdTbkPsX8cIQ2688lC25oA_Zi0VCVjtBQZXk_Qxj6lCI1-yL808a-mRL90q3O3mgmdu8348pg61h24__RYZgY3EzikwezgHZg4eNvCWxafnhz5vrF7EzWE8h-NjIwK</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>68322135</pqid></control><display><type>article</type><title>Effects of Alumina-blasting and Adhesive Primers on Bonding between Resin Luting Agent and Zirconia Ceramics</title><source>J-STAGE Free</source><source>MEDLINE</source><source>Freely Accessible Japanese Titles</source><source>Elektronische Zeitschriftenbibliothek - Frei zugängliche E-Journals</source><creator>TSUO, Yukiko ; YOSHIDA, Keiichi ; ATSUTA, Mitsuru</creator><creatorcontrib>TSUO, Yukiko ; YOSHIDA, Keiichi ; ATSUTA, Mitsuru</creatorcontrib><description>This study evaluated the effect of alumina-blasting and three commercial adhesive primers on the shear bond strength of a dual-cured resin luting agent to zirconia ceramics. Two different-sized zirconia ceramic specimens were treated with or without alumina-blasting and then treated with one of three adhesive primers. Subsequently, specimens were cemented together with Linkmax HV (GC). Half of the specimens were stored in water at 37°C for 24 hours and the other half thermocycled 10,000 times before shear bond strength testing. For groups treated with either alumina-blasting or primer, shear bond strength significantly decreased after thermal cycling. For groups treated with both alumina-blasting and one of the three primers, there were no significant differences in shear bond strength before and after thermal cycling (p&lt;0.05). It was thus concluded that the application of each of the three adhesive primers following alumina-blasting was effective for strong bonding of resin luting agent to zirconia ceramics.</description><identifier>ISSN: 0287-4547</identifier><identifier>EISSN: 1881-1361</identifier><identifier>DOI: 10.4012/dmj.25.669</identifier><identifier>PMID: 17338299</identifier><language>eng</language><publisher>Japan: The Japanese Society for Dental Materials and Devices</publisher><subject>Aluminum Oxide ; Analysis of Variance ; Bond strength ; Dental Bonding ; Dental Porcelain ; Dental Stress Analysis ; Dentistry ; Materials Testing ; Methacrylates ; Organophosphorus Compounds ; Resin Cements ; Resin luting agent ; Shear Strength ; Surface Properties ; Tricarboxylic Acids ; Yttrium ; Zirconia ceramic ; Zirconium</subject><ispartof>Dental Materials Journal, 2006, Vol.25(4), pp.669-674</ispartof><rights>2006 The Japanese Society for Dental Materials and Devices</rights><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c568t-52eb6ad10608428045b6ecd2e64c1dcea3176b4b0892c518a9a55d468be9906d3</citedby><cites>FETCH-LOGICAL-c568t-52eb6ad10608428045b6ecd2e64c1dcea3176b4b0892c518a9a55d468be9906d3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,776,780,1877,4010,27900,27901,27902</link.rule.ids><backlink>$$Uhttps://www.ncbi.nlm.nih.gov/pubmed/17338299$$D View this record in MEDLINE/PubMed$$Hfree_for_read</backlink></links><search><creatorcontrib>TSUO, Yukiko</creatorcontrib><creatorcontrib>YOSHIDA, Keiichi</creatorcontrib><creatorcontrib>ATSUTA, Mitsuru</creatorcontrib><title>Effects of Alumina-blasting and Adhesive Primers on Bonding between Resin Luting Agent and Zirconia Ceramics</title><title>Dental Materials Journal</title><addtitle>Dent. Mater. J.</addtitle><description>This study evaluated the effect of alumina-blasting and three commercial adhesive primers on the shear bond strength of a dual-cured resin luting agent to zirconia ceramics. Two different-sized zirconia ceramic specimens were treated with or without alumina-blasting and then treated with one of three adhesive primers. Subsequently, specimens were cemented together with Linkmax HV (GC). Half of the specimens were stored in water at 37°C for 24 hours and the other half thermocycled 10,000 times before shear bond strength testing. For groups treated with either alumina-blasting or primer, shear bond strength significantly decreased after thermal cycling. For groups treated with both alumina-blasting and one of the three primers, there were no significant differences in shear bond strength before and after thermal cycling (p&lt;0.05). It was thus concluded that the application of each of the three adhesive primers following alumina-blasting was effective for strong bonding of resin luting agent to zirconia ceramics.</description><subject>Aluminum Oxide</subject><subject>Analysis of Variance</subject><subject>Bond strength</subject><subject>Dental Bonding</subject><subject>Dental Porcelain</subject><subject>Dental Stress Analysis</subject><subject>Dentistry</subject><subject>Materials Testing</subject><subject>Methacrylates</subject><subject>Organophosphorus Compounds</subject><subject>Resin Cements</subject><subject>Resin luting agent</subject><subject>Shear Strength</subject><subject>Surface Properties</subject><subject>Tricarboxylic Acids</subject><subject>Yttrium</subject><subject>Zirconia ceramic</subject><subject>Zirconium</subject><issn>0287-4547</issn><issn>1881-1361</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2006</creationdate><recordtype>article</recordtype><sourceid>EIF</sourceid><recordid>eNpF0EFP2zAUB3ALMa2F7cIHQD5xQEpnO7brnFCpyoZUadO0XXaxHPuldZU4YCegffsZUtjF7_B-7y_5j9AFJQtOKPviusOCiYWU1QmaU6VoQUtJT9GcMLUsuODLGTpL6UAIr6RSH9GMLstSsaqao3bTNGCHhPsGr9qx88EUdWvS4MMOm-Dwyu0h-SfAP6LvIGYY8G0f3Mu-huEZIOCfWQS8HV-PVjsIw-vpHx9tH7zBa4im8zZ9Qh8a0yb4fJzn6Pfd5tf6W7H9_vV-vdoWVkg1FIJBLY2jRBLFmSJc1BKsYyC5pc6CKelS1rwmqmJWUGUqI4TjUtVQVUS68hxdTbkPsX8cIQ2688lC25oA_Zi0VCVjtBQZXk_Qxj6lCI1-yL808a-mRL90q3O3mgmdu8348pg61h24__RYZgY3EzikwezgHZg4eNvCWxafnhz5vrF7EzWE8h-NjIwK</recordid><startdate>2006</startdate><enddate>2006</enddate><creator>TSUO, Yukiko</creator><creator>YOSHIDA, Keiichi</creator><creator>ATSUTA, Mitsuru</creator><general>The Japanese Society for Dental Materials and Devices</general><scope>CGR</scope><scope>CUY</scope><scope>CVF</scope><scope>ECM</scope><scope>EIF</scope><scope>NPM</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7X8</scope></search><sort><creationdate>2006</creationdate><title>Effects of Alumina-blasting and Adhesive Primers on Bonding between Resin Luting Agent and Zirconia Ceramics</title><author>TSUO, Yukiko ; YOSHIDA, Keiichi ; ATSUTA, Mitsuru</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c568t-52eb6ad10608428045b6ecd2e64c1dcea3176b4b0892c518a9a55d468be9906d3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2006</creationdate><topic>Aluminum Oxide</topic><topic>Analysis of Variance</topic><topic>Bond strength</topic><topic>Dental Bonding</topic><topic>Dental Porcelain</topic><topic>Dental Stress Analysis</topic><topic>Dentistry</topic><topic>Materials Testing</topic><topic>Methacrylates</topic><topic>Organophosphorus Compounds</topic><topic>Resin Cements</topic><topic>Resin luting agent</topic><topic>Shear Strength</topic><topic>Surface Properties</topic><topic>Tricarboxylic Acids</topic><topic>Yttrium</topic><topic>Zirconia ceramic</topic><topic>Zirconium</topic><toplevel>online_resources</toplevel><creatorcontrib>TSUO, Yukiko</creatorcontrib><creatorcontrib>YOSHIDA, Keiichi</creatorcontrib><creatorcontrib>ATSUTA, Mitsuru</creatorcontrib><collection>Medline</collection><collection>MEDLINE</collection><collection>MEDLINE (Ovid)</collection><collection>MEDLINE</collection><collection>MEDLINE</collection><collection>PubMed</collection><collection>CrossRef</collection><collection>MEDLINE - Academic</collection><jtitle>Dental Materials Journal</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>TSUO, Yukiko</au><au>YOSHIDA, Keiichi</au><au>ATSUTA, Mitsuru</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Effects of Alumina-blasting and Adhesive Primers on Bonding between Resin Luting Agent and Zirconia Ceramics</atitle><jtitle>Dental Materials Journal</jtitle><addtitle>Dent. Mater. J.</addtitle><date>2006</date><risdate>2006</risdate><volume>25</volume><issue>4</issue><spage>669</spage><epage>674</epage><pages>669-674</pages><issn>0287-4547</issn><eissn>1881-1361</eissn><abstract>This study evaluated the effect of alumina-blasting and three commercial adhesive primers on the shear bond strength of a dual-cured resin luting agent to zirconia ceramics. Two different-sized zirconia ceramic specimens were treated with or without alumina-blasting and then treated with one of three adhesive primers. Subsequently, specimens were cemented together with Linkmax HV (GC). Half of the specimens were stored in water at 37°C for 24 hours and the other half thermocycled 10,000 times before shear bond strength testing. For groups treated with either alumina-blasting or primer, shear bond strength significantly decreased after thermal cycling. For groups treated with both alumina-blasting and one of the three primers, there were no significant differences in shear bond strength before and after thermal cycling (p&lt;0.05). It was thus concluded that the application of each of the three adhesive primers following alumina-blasting was effective for strong bonding of resin luting agent to zirconia ceramics.</abstract><cop>Japan</cop><pub>The Japanese Society for Dental Materials and Devices</pub><pmid>17338299</pmid><doi>10.4012/dmj.25.669</doi><tpages>6</tpages><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 0287-4547
ispartof Dental Materials Journal, 2006, Vol.25(4), pp.669-674
issn 0287-4547
1881-1361
language eng
recordid cdi_proquest_miscellaneous_68322135
source J-STAGE Free; MEDLINE; Freely Accessible Japanese Titles; Elektronische Zeitschriftenbibliothek - Frei zugängliche E-Journals
subjects Aluminum Oxide
Analysis of Variance
Bond strength
Dental Bonding
Dental Porcelain
Dental Stress Analysis
Dentistry
Materials Testing
Methacrylates
Organophosphorus Compounds
Resin Cements
Resin luting agent
Shear Strength
Surface Properties
Tricarboxylic Acids
Yttrium
Zirconia ceramic
Zirconium
title Effects of Alumina-blasting and Adhesive Primers on Bonding between Resin Luting Agent and Zirconia Ceramics
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-06T14%3A38%3A17IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Effects%20of%20Alumina-blasting%20and%20Adhesive%20Primers%20on%20Bonding%20between%20Resin%20Luting%20Agent%20and%20Zirconia%20Ceramics&rft.jtitle=Dental%20Materials%20Journal&rft.au=TSUO,%20Yukiko&rft.date=2006&rft.volume=25&rft.issue=4&rft.spage=669&rft.epage=674&rft.pages=669-674&rft.issn=0287-4547&rft.eissn=1881-1361&rft_id=info:doi/10.4012/dmj.25.669&rft_dat=%3Cproquest_cross%3E68322135%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=68322135&rft_id=info:pmid/17338299&rfr_iscdi=true