ADHESION OF THE BIOACTIVE LAYER ON TITANIUM ALLOY SUBSTRATE BY TAPE-TEST

An attempt was made to assess whether the ASTM D 3359 test is a suitable method for adhesion measurement of layers formed on Ti6Al4V surfaces by: alkali treatment in 10 mol/l NaOH; precalcification in SCS (supersaturated calcification solution); and in-vitro tests in SBF (simulated body fluid). The...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Ceramics (Praha) 2008-01, Vol.52 (3), p.130-138
Hauptverfasser: Horkavcova, D, Plesingerova, B, Helebrant, A, Vojtko, M, Prochazka, V
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 138
container_issue 3
container_start_page 130
container_title Ceramics (Praha)
container_volume 52
creator Horkavcova, D
Plesingerova, B
Helebrant, A
Vojtko, M
Prochazka, V
description An attempt was made to assess whether the ASTM D 3359 test is a suitable method for adhesion measurement of layers formed on Ti6Al4V surfaces by: alkali treatment in 10 mol/l NaOH; precalcification in SCS (supersaturated calcification solution); and in-vitro tests in SBF (simulated body fluid). The tape-test is suitable for the evaluation of adhesion of coatings after chemical treatment and after short-time precalcification. Adhesion of the coatings was excellent, classified as category 5. The test is not suitable for coatings precalcified for a long time when large spherical crystals are formed. The cracking of the coatings during drying prevented reliable results of adhesion of HA-coatings to substrate after in-vitro tests to be obtained. 12 refs.
format Article
fullrecord <record><control><sourceid>proquest</sourceid><recordid>TN_cdi_proquest_miscellaneous_35326324</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>35326324</sourcerecordid><originalsourceid>FETCH-LOGICAL-p186t-bbbcab799f0e0102a8524071051e433e40cafad0cdcfe1afacc286a6f676339e3</originalsourceid><addsrcrecordid>eNotjEFLwzAYhnNQ2Jz-h5y8FdIkTdNjVjMbiIusXwc9jTRLQalumu3_W3Cn94Hn4b1DSyIFzQou5AI9pPRJCBNFKZeoUS-Nbo3bYrfB0Gi8Nk7VYPYaW9XrHZ4NGFBb071hZa3rcdutW9gpmNseg3rXGegWHtH96KcUn267Qt1GQ91k1r2aWtnsnEtxyYZhCH4oq2okkeSEellQTsqcFHnkjEVOgh_9kYRjGGM-YwhUCi9GUQrGqshW6Pn_9_x7-rnGdDl8faQQp8l_x9M1HVjBqGCUsz-xTEJp</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>35326324</pqid></control><display><type>article</type><title>ADHESION OF THE BIOACTIVE LAYER ON TITANIUM ALLOY SUBSTRATE BY TAPE-TEST</title><source>DOAJ Directory of Open Access Journals</source><source>EZB-FREE-00999 freely available EZB journals</source><source>Free Full-Text Journals in Chemistry</source><creator>Horkavcova, D ; Plesingerova, B ; Helebrant, A ; Vojtko, M ; Prochazka, V</creator><creatorcontrib>Horkavcova, D ; Plesingerova, B ; Helebrant, A ; Vojtko, M ; Prochazka, V</creatorcontrib><description>An attempt was made to assess whether the ASTM D 3359 test is a suitable method for adhesion measurement of layers formed on Ti6Al4V surfaces by: alkali treatment in 10 mol/l NaOH; precalcification in SCS (supersaturated calcification solution); and in-vitro tests in SBF (simulated body fluid). The tape-test is suitable for the evaluation of adhesion of coatings after chemical treatment and after short-time precalcification. Adhesion of the coatings was excellent, classified as category 5. The test is not suitable for coatings precalcified for a long time when large spherical crystals are formed. The cracking of the coatings during drying prevented reliable results of adhesion of HA-coatings to substrate after in-vitro tests to be obtained. 12 refs.</description><identifier>ISSN: 0862-5468</identifier><language>eng</language><ispartof>Ceramics (Praha), 2008-01, Vol.52 (3), p.130-138</ispartof><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784</link.rule.ids></links><search><creatorcontrib>Horkavcova, D</creatorcontrib><creatorcontrib>Plesingerova, B</creatorcontrib><creatorcontrib>Helebrant, A</creatorcontrib><creatorcontrib>Vojtko, M</creatorcontrib><creatorcontrib>Prochazka, V</creatorcontrib><title>ADHESION OF THE BIOACTIVE LAYER ON TITANIUM ALLOY SUBSTRATE BY TAPE-TEST</title><title>Ceramics (Praha)</title><description>An attempt was made to assess whether the ASTM D 3359 test is a suitable method for adhesion measurement of layers formed on Ti6Al4V surfaces by: alkali treatment in 10 mol/l NaOH; precalcification in SCS (supersaturated calcification solution); and in-vitro tests in SBF (simulated body fluid). The tape-test is suitable for the evaluation of adhesion of coatings after chemical treatment and after short-time precalcification. Adhesion of the coatings was excellent, classified as category 5. The test is not suitable for coatings precalcified for a long time when large spherical crystals are formed. The cracking of the coatings during drying prevented reliable results of adhesion of HA-coatings to substrate after in-vitro tests to be obtained. 12 refs.</description><issn>0862-5468</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2008</creationdate><recordtype>article</recordtype><recordid>eNotjEFLwzAYhnNQ2Jz-h5y8FdIkTdNjVjMbiIusXwc9jTRLQalumu3_W3Cn94Hn4b1DSyIFzQou5AI9pPRJCBNFKZeoUS-Nbo3bYrfB0Gi8Nk7VYPYaW9XrHZ4NGFBb071hZa3rcdutW9gpmNseg3rXGegWHtH96KcUn267Qt1GQ91k1r2aWtnsnEtxyYZhCH4oq2okkeSEellQTsqcFHnkjEVOgh_9kYRjGGM-YwhUCi9GUQrGqshW6Pn_9_x7-rnGdDl8faQQp8l_x9M1HVjBqGCUsz-xTEJp</recordid><startdate>20080101</startdate><enddate>20080101</enddate><creator>Horkavcova, D</creator><creator>Plesingerova, B</creator><creator>Helebrant, A</creator><creator>Vojtko, M</creator><creator>Prochazka, V</creator><scope>7QQ</scope><scope>7SR</scope><scope>8BQ</scope><scope>8FD</scope><scope>JG9</scope></search><sort><creationdate>20080101</creationdate><title>ADHESION OF THE BIOACTIVE LAYER ON TITANIUM ALLOY SUBSTRATE BY TAPE-TEST</title><author>Horkavcova, D ; Plesingerova, B ; Helebrant, A ; Vojtko, M ; Prochazka, V</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-p186t-bbbcab799f0e0102a8524071051e433e40cafad0cdcfe1afacc286a6f676339e3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2008</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Horkavcova, D</creatorcontrib><creatorcontrib>Plesingerova, B</creatorcontrib><creatorcontrib>Helebrant, A</creatorcontrib><creatorcontrib>Vojtko, M</creatorcontrib><creatorcontrib>Prochazka, V</creatorcontrib><collection>Ceramic Abstracts</collection><collection>Engineered Materials Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><jtitle>Ceramics (Praha)</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Horkavcova, D</au><au>Plesingerova, B</au><au>Helebrant, A</au><au>Vojtko, M</au><au>Prochazka, V</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>ADHESION OF THE BIOACTIVE LAYER ON TITANIUM ALLOY SUBSTRATE BY TAPE-TEST</atitle><jtitle>Ceramics (Praha)</jtitle><date>2008-01-01</date><risdate>2008</risdate><volume>52</volume><issue>3</issue><spage>130</spage><epage>138</epage><pages>130-138</pages><issn>0862-5468</issn><abstract>An attempt was made to assess whether the ASTM D 3359 test is a suitable method for adhesion measurement of layers formed on Ti6Al4V surfaces by: alkali treatment in 10 mol/l NaOH; precalcification in SCS (supersaturated calcification solution); and in-vitro tests in SBF (simulated body fluid). The tape-test is suitable for the evaluation of adhesion of coatings after chemical treatment and after short-time precalcification. Adhesion of the coatings was excellent, classified as category 5. The test is not suitable for coatings precalcified for a long time when large spherical crystals are formed. The cracking of the coatings during drying prevented reliable results of adhesion of HA-coatings to substrate after in-vitro tests to be obtained. 12 refs.</abstract><tpages>9</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0862-5468
ispartof Ceramics (Praha), 2008-01, Vol.52 (3), p.130-138
issn 0862-5468
language eng
recordid cdi_proquest_miscellaneous_35326324
source DOAJ Directory of Open Access Journals; EZB-FREE-00999 freely available EZB journals; Free Full-Text Journals in Chemistry
title ADHESION OF THE BIOACTIVE LAYER ON TITANIUM ALLOY SUBSTRATE BY TAPE-TEST
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-25T15%3A28%3A46IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=ADHESION%20OF%20THE%20BIOACTIVE%20LAYER%20ON%20TITANIUM%20ALLOY%20SUBSTRATE%20BY%20TAPE-TEST&rft.jtitle=Ceramics%20(Praha)&rft.au=Horkavcova,%20D&rft.date=2008-01-01&rft.volume=52&rft.issue=3&rft.spage=130&rft.epage=138&rft.pages=130-138&rft.issn=0862-5468&rft_id=info:doi/&rft_dat=%3Cproquest%3E35326324%3C/proquest%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=35326324&rft_id=info:pmid/&rfr_iscdi=true