Analyzing indentation behavior of LaGaO3 single crystals using sharp indenters

The mechanical properties of (100) and (001) oriented LaGaO3 single crystals were studied using sharp indenters. Vickers hardness values for both the (100) and (001) samples were in the same range (about 8 GPa). The values for the indentation fracture toughness from Vickers indentation on the (100)...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of the European Ceramic Society 2008, Vol.28 (10), p.2039-2047
Hauptverfasser: PATHAK, Siddhartha, KALIDINDI, Surya R, MOSER, Benedikt, KLEMENZ, Christine, ORLOVSKAYA, Nina
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 2047
container_issue 10
container_start_page 2039
container_title Journal of the European Ceramic Society
container_volume 28
creator PATHAK, Siddhartha
KALIDINDI, Surya R
MOSER, Benedikt
KLEMENZ, Christine
ORLOVSKAYA, Nina
description The mechanical properties of (100) and (001) oriented LaGaO3 single crystals were studied using sharp indenters. Vickers hardness values for both the (100) and (001) samples were in the same range (about 8 GPa). The values for the indentation fracture toughness from Vickers indentation on the (100) samples were determined to be 0.8 plus or minus 0.2 MPa.m1/2. Different crack lengths, implying a strong anisotropy in the indentation fracture toughness values, were observed in the two mutually perpendicular directions in the indentations on the (001) samples. These measurements led to estimates of 0.5 plus or minus 0.1 and 1.3 plus or minus 0.3 MPa.m1/2 for the two different sets of cracks on the (001) samples. In-situ nanoindentation inside the SEM chamber using a cube-corner indenter was also used to study the indentation fracture response of these samples. 39 refs.
doi_str_mv 10.1016/j.jeurceramsoc.2008.02.010
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_34973864</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>34973864</sourcerecordid><originalsourceid>FETCH-LOGICAL-c324t-3c9dee24897973f8a7afdd888a288e54780c0eee773fdb0e3cc6727c33a075463</originalsourceid><addsrcrecordid>eNpNkF1LwzAUhoMoOKf_oQh613qStE3q3RCdwnA3Ct6Fs_TUtXTtTFph_nozNsSrA-_XgYexaw4JB57fNUlDo7PkcON7mwgAnYBIgMMJm3CtZJzz4uOUTaDIslgIXpyzC-8bAK6gKCbsddZhu_upu8-o7krqBhzqvotWtMbvundRX0ULnONSRj5kWoqs2_kBWx-NeyHya3TbY5Wcv2RnVTDp6nin7P3p8e3hOV4s5y8Ps0VspUiHWNqiJBKpLlShZKVRYVWWWmsUWlOWKg0WiEgFs1wBSWtzJZSVEkFlaS6n7Pawu3X910h-MJvaW2pb7KgfvZFp2NV5GoL3h6B1vfeOKrN19QbdznAwe4SmMf8Rmj1CA8IEhKF8c_yC3mJbOexs7f8WBMgMVID8C2aZd6Y</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>34973864</pqid></control><display><type>article</type><title>Analyzing indentation behavior of LaGaO3 single crystals using sharp indenters</title><source>Elsevier ScienceDirect Journals Complete</source><creator>PATHAK, Siddhartha ; KALIDINDI, Surya R ; MOSER, Benedikt ; KLEMENZ, Christine ; ORLOVSKAYA, Nina</creator><creatorcontrib>PATHAK, Siddhartha ; KALIDINDI, Surya R ; MOSER, Benedikt ; KLEMENZ, Christine ; ORLOVSKAYA, Nina</creatorcontrib><description>The mechanical properties of (100) and (001) oriented LaGaO3 single crystals were studied using sharp indenters. Vickers hardness values for both the (100) and (001) samples were in the same range (about 8 GPa). The values for the indentation fracture toughness from Vickers indentation on the (100) samples were determined to be 0.8 plus or minus 0.2 MPa.m1/2. Different crack lengths, implying a strong anisotropy in the indentation fracture toughness values, were observed in the two mutually perpendicular directions in the indentations on the (001) samples. These measurements led to estimates of 0.5 plus or minus 0.1 and 1.3 plus or minus 0.3 MPa.m1/2 for the two different sets of cracks on the (001) samples. In-situ nanoindentation inside the SEM chamber using a cube-corner indenter was also used to study the indentation fracture response of these samples. 39 refs.</description><identifier>ISSN: 0955-2219</identifier><identifier>EISSN: 1873-619X</identifier><identifier>DOI: 10.1016/j.jeurceramsoc.2008.02.010</identifier><language>eng</language><publisher>Oxford: Elsevier</publisher><subject>Condensed matter: structure, mechanical and thermal properties ; Exact sciences and technology ; Mechanical and acoustical properties of condensed matter ; Mechanical properties of solids ; Physics ; Tribology and hardness</subject><ispartof>Journal of the European Ceramic Society, 2008, Vol.28 (10), p.2039-2047</ispartof><rights>2008 INIST-CNRS</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c324t-3c9dee24897973f8a7afdd888a288e54780c0eee773fdb0e3cc6727c33a075463</citedby><cites>FETCH-LOGICAL-c324t-3c9dee24897973f8a7afdd888a288e54780c0eee773fdb0e3cc6727c33a075463</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,4024,27923,27924,27925</link.rule.ids><backlink>$$Uhttp://pascal-francis.inist.fr/vibad/index.php?action=getRecordDetail&amp;idt=20350787$$DView record in Pascal Francis$$Hfree_for_read</backlink></links><search><creatorcontrib>PATHAK, Siddhartha</creatorcontrib><creatorcontrib>KALIDINDI, Surya R</creatorcontrib><creatorcontrib>MOSER, Benedikt</creatorcontrib><creatorcontrib>KLEMENZ, Christine</creatorcontrib><creatorcontrib>ORLOVSKAYA, Nina</creatorcontrib><title>Analyzing indentation behavior of LaGaO3 single crystals using sharp indenters</title><title>Journal of the European Ceramic Society</title><description>The mechanical properties of (100) and (001) oriented LaGaO3 single crystals were studied using sharp indenters. Vickers hardness values for both the (100) and (001) samples were in the same range (about 8 GPa). The values for the indentation fracture toughness from Vickers indentation on the (100) samples were determined to be 0.8 plus or minus 0.2 MPa.m1/2. Different crack lengths, implying a strong anisotropy in the indentation fracture toughness values, were observed in the two mutually perpendicular directions in the indentations on the (001) samples. These measurements led to estimates of 0.5 plus or minus 0.1 and 1.3 plus or minus 0.3 MPa.m1/2 for the two different sets of cracks on the (001) samples. In-situ nanoindentation inside the SEM chamber using a cube-corner indenter was also used to study the indentation fracture response of these samples. 39 refs.</description><subject>Condensed matter: structure, mechanical and thermal properties</subject><subject>Exact sciences and technology</subject><subject>Mechanical and acoustical properties of condensed matter</subject><subject>Mechanical properties of solids</subject><subject>Physics</subject><subject>Tribology and hardness</subject><issn>0955-2219</issn><issn>1873-619X</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2008</creationdate><recordtype>article</recordtype><recordid>eNpNkF1LwzAUhoMoOKf_oQh613qStE3q3RCdwnA3Ct6Fs_TUtXTtTFph_nozNsSrA-_XgYexaw4JB57fNUlDo7PkcON7mwgAnYBIgMMJm3CtZJzz4uOUTaDIslgIXpyzC-8bAK6gKCbsddZhu_upu8-o7krqBhzqvotWtMbvundRX0ULnONSRj5kWoqs2_kBWx-NeyHya3TbY5Wcv2RnVTDp6nin7P3p8e3hOV4s5y8Ps0VspUiHWNqiJBKpLlShZKVRYVWWWmsUWlOWKg0WiEgFs1wBSWtzJZSVEkFlaS6n7Pawu3X910h-MJvaW2pb7KgfvZFp2NV5GoL3h6B1vfeOKrN19QbdznAwe4SmMf8Rmj1CA8IEhKF8c_yC3mJbOexs7f8WBMgMVID8C2aZd6Y</recordid><startdate>2008</startdate><enddate>2008</enddate><creator>PATHAK, Siddhartha</creator><creator>KALIDINDI, Surya R</creator><creator>MOSER, Benedikt</creator><creator>KLEMENZ, Christine</creator><creator>ORLOVSKAYA, Nina</creator><general>Elsevier</general><scope>IQODW</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7QQ</scope><scope>7SR</scope><scope>8FD</scope><scope>JG9</scope></search><sort><creationdate>2008</creationdate><title>Analyzing indentation behavior of LaGaO3 single crystals using sharp indenters</title><author>PATHAK, Siddhartha ; KALIDINDI, Surya R ; MOSER, Benedikt ; KLEMENZ, Christine ; ORLOVSKAYA, Nina</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c324t-3c9dee24897973f8a7afdd888a288e54780c0eee773fdb0e3cc6727c33a075463</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2008</creationdate><topic>Condensed matter: structure, mechanical and thermal properties</topic><topic>Exact sciences and technology</topic><topic>Mechanical and acoustical properties of condensed matter</topic><topic>Mechanical properties of solids</topic><topic>Physics</topic><topic>Tribology and hardness</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>PATHAK, Siddhartha</creatorcontrib><creatorcontrib>KALIDINDI, Surya R</creatorcontrib><creatorcontrib>MOSER, Benedikt</creatorcontrib><creatorcontrib>KLEMENZ, Christine</creatorcontrib><creatorcontrib>ORLOVSKAYA, Nina</creatorcontrib><collection>Pascal-Francis</collection><collection>CrossRef</collection><collection>Ceramic Abstracts</collection><collection>Engineered Materials Abstracts</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><jtitle>Journal of the European Ceramic Society</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>PATHAK, Siddhartha</au><au>KALIDINDI, Surya R</au><au>MOSER, Benedikt</au><au>KLEMENZ, Christine</au><au>ORLOVSKAYA, Nina</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Analyzing indentation behavior of LaGaO3 single crystals using sharp indenters</atitle><jtitle>Journal of the European Ceramic Society</jtitle><date>2008</date><risdate>2008</risdate><volume>28</volume><issue>10</issue><spage>2039</spage><epage>2047</epage><pages>2039-2047</pages><issn>0955-2219</issn><eissn>1873-619X</eissn><abstract>The mechanical properties of (100) and (001) oriented LaGaO3 single crystals were studied using sharp indenters. Vickers hardness values for both the (100) and (001) samples were in the same range (about 8 GPa). The values for the indentation fracture toughness from Vickers indentation on the (100) samples were determined to be 0.8 plus or minus 0.2 MPa.m1/2. Different crack lengths, implying a strong anisotropy in the indentation fracture toughness values, were observed in the two mutually perpendicular directions in the indentations on the (001) samples. These measurements led to estimates of 0.5 plus or minus 0.1 and 1.3 plus or minus 0.3 MPa.m1/2 for the two different sets of cracks on the (001) samples. In-situ nanoindentation inside the SEM chamber using a cube-corner indenter was also used to study the indentation fracture response of these samples. 39 refs.</abstract><cop>Oxford</cop><pub>Elsevier</pub><doi>10.1016/j.jeurceramsoc.2008.02.010</doi><tpages>9</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0955-2219
ispartof Journal of the European Ceramic Society, 2008, Vol.28 (10), p.2039-2047
issn 0955-2219
1873-619X
language eng
recordid cdi_proquest_miscellaneous_34973864
source Elsevier ScienceDirect Journals Complete
subjects Condensed matter: structure, mechanical and thermal properties
Exact sciences and technology
Mechanical and acoustical properties of condensed matter
Mechanical properties of solids
Physics
Tribology and hardness
title Analyzing indentation behavior of LaGaO3 single crystals using sharp indenters
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-01T14%3A37%3A03IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Analyzing%20indentation%20behavior%20of%20LaGaO3%20single%20crystals%20using%20sharp%20indenters&rft.jtitle=Journal%20of%20the%20European%20Ceramic%20Society&rft.au=PATHAK,%20Siddhartha&rft.date=2008&rft.volume=28&rft.issue=10&rft.spage=2039&rft.epage=2047&rft.pages=2039-2047&rft.issn=0955-2219&rft.eissn=1873-619X&rft_id=info:doi/10.1016/j.jeurceramsoc.2008.02.010&rft_dat=%3Cproquest_cross%3E34973864%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=34973864&rft_id=info:pmid/&rfr_iscdi=true