Transparent mullite ceramic from single-phase gel by Spark Plasma Sintering

Monophasic mullite precursors with composition of 3Al 2O 3·2SiO 2 (3:2) were synthesized and then were sintered by Spark Plasma Sintering (SPS) to form transparent mullite ceramics. The precursor powders were calcined at 1100 °C for 2 h. The sintering was carried out by heating the sample to 1450 °C...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of the European Ceramic Society 2009-10, Vol.29 (13), p.2705-2711
Hauptverfasser: Zhang, Guimin, Wang, Yucheng, Fu, Zhengyi, Wang, Hao, Wang, Weiming, Zhang, Jinyong, Lee, Soo Wohn, Niihara, Kochi