Nucleation of austenite from pearlitic structure in an Fe–0.6C–1Cr alloy
The nucleation site of austenite from pearlitic structure during reverse transformation at 1073 K in Fe–0.6C–1Cr (mass%) alloy was examined by means of electron backscattering diffraction. It was found that austenite preferentially nucleates at high-angle boundaries (HABs) of pearlitic ferrite. Some...