Hydrothermal upgrading of wood biomass: Influence of the addition of K2CO3 and cellulose/lignin ratio
The hydrothermal treatment of two different wood biomass samples such as cherry (hard wood) and cypress (soft wood), whose composition is different i.e. lignin, cellulose and hemicellulose were performed at 280°C for 15min with aq. K2CO3 with different concentrations (0–1M). The soft wood biomass co...
Gespeichert in:
Veröffentlicht in: | Fuel (Guildford) 2008-08, Vol.87 (10-11), p.2236-2242 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The hydrothermal treatment of two different wood biomass samples such as cherry (hard wood) and cypress (soft wood), whose composition is different i.e. lignin, cellulose and hemicellulose were performed at 280°C for 15min with aq. K2CO3 with different concentrations (0–1M). The soft wood biomass contains higher lignin content than hard wood biomass. The cellulose rich cherry wood biomass produced higher proportion of acetic acid than cypress. The lignin rich cypress produced the hydrocarbons with major portion of phenolic hydrocarbons and derivatives than cherry. The total oil yields from both cherry and cypress wood biomass produced 50wt% of liquid hydrocarbons at 280°C for 15min with 0.5M K2CO3 solution. The volatility distribution of liquid hydrocarbons showed the characteristic features of soft and hard wood biomasses. |
---|---|