Mechanical Properties of Cu-4.0wt%Ni-0.95wt%Si Alloys with and without P and Cr Addition

The effects of P and Cr addition and two-step aging on the microstructure and mechanical properties of a Cu-4wt%Ni-0.95wt%Si alloy have been examined. The addition of 0.02wt%P improves both strength and elongation because it suppresses discontinuous precipitation reaction. The Cr addition to the Cu-...