Tuning Zn-ion de-solvation chemistry with trace amount of additive towards stable Aqueous Zn anodes

[Display omitted] •Trace additive effectively extends the cycle life of ZIBs.•The adsorbed NTA molecules reduce the de-solvation energy barrier.•NTA molecules provide a buffer layer to retard dendrite growth. Aqueous Zn-ion batteries (AZIBs) have attracted widespread attention due to their intrinsic...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of colloid and interface science 2025-01, Vol.677 (Pt B), p.462-471
Hauptverfasser: Qiao, Shizhe, Chang, Le, Cui, Ziyang, Wang, Dengke, Zhang, Wenming, Zhu, Qiancheng
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 471
container_issue Pt B
container_start_page 462
container_title Journal of colloid and interface science
container_volume 677
creator Qiao, Shizhe
Chang, Le
Cui, Ziyang
Wang, Dengke
Zhang, Wenming
Zhu, Qiancheng
description [Display omitted] •Trace additive effectively extends the cycle life of ZIBs.•The adsorbed NTA molecules reduce the de-solvation energy barrier.•NTA molecules provide a buffer layer to retard dendrite growth. Aqueous Zn-ion batteries (AZIBs) have attracted widespread attention due to their intrinsic safety, cost-effectiveness. However, active H2O in the solvated ions [Zn(H2O)6]2+ continuously migrate to the Zn surface to trigger hydrogen evolution reaction (HER) and accelerate Zn corrosion. Herein, Zn dendrites and the related by-products have been successfully inhibited by using trace amounts of Nitrilotriacetic acid (NTA). Theoretical research indicates that two carboxyl groups of NTA molecule strongly anchored on the Zn surface and exposed another carboxyl group outside. Due to the violent interaction of carboxyl groups of NTA with H2O, the de-solvation energy barrier of solvated Zn2+ ([Zn(H2O)6]2+) on the Zn surface was obviously decreased, inhibit the active water splitting. Meanwhile, the preferential adsorption of NTA on the Zn surface increases the thickness of electric double layer EDL and provides a buffer layer to hinder the dendrite growth. Using 0.04 M NTA as additives in 2.0 M ZnSO4 electrolyte, the cycling lifespan of both Zn||Zn symmetric and Zn||MnO2 full cells is markedly prolonged. This study provides certain perspectives for trace amounts of electrolyte additives to satisfy the demand of long-cycle life AZIBs.
doi_str_mv 10.1016/j.jcis.2024.08.088
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_3094468697</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0021979724018678</els_id><sourcerecordid>3094468697</sourcerecordid><originalsourceid>FETCH-LOGICAL-c237t-2435d3879b1b0886474fc3ba14196153ffec39e1597b126a460464aa527ef6873</originalsourceid><addsrcrecordid>eNp9UE1r3DAUFKWh2ST9Az0UHXPxRrJkyYJeliVfEMglueQiZOm50eK1tpK8If8-MrvJsTDweDAzzAxCvyhZUkLF1Wa5sT4ta1LzJWkL2m9oQYlqKkkJ-44WhNS0UlLJU3SW0oYQSptG_UCnTNGGc6YWyD5Nox__4pex8mHEDqoUhr3J82NfYetTju_4zedXnKOxgM02TGPGocfGOZ_9HnAObya6hFM23QB49W-CMKViic0YHKQLdNKbIcHP4z1HzzfXT-u76uHx9n69eqhszWSuas4ax1qpOtqVLoJL3lvWGcqpErRhfQ-WKaCNkh2theGCcMGNaWoJvWglO0eXB99dDCVDyrrEtzAMZpwDaUYU56IVaqbWB6qNIaUIvd5FvzXxXVOi53H1Rs_j6nlcTdqCtoh-H_2nbgvuS_K5ZiH8ORCgtNx7iDpZD6MF5yPYrF3w__P_ALA5iww</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>3094468697</pqid></control><display><type>article</type><title>Tuning Zn-ion de-solvation chemistry with trace amount of additive towards stable Aqueous Zn anodes</title><source>Elsevier ScienceDirect Journals Complete</source><creator>Qiao, Shizhe ; Chang, Le ; Cui, Ziyang ; Wang, Dengke ; Zhang, Wenming ; Zhu, Qiancheng</creator><creatorcontrib>Qiao, Shizhe ; Chang, Le ; Cui, Ziyang ; Wang, Dengke ; Zhang, Wenming ; Zhu, Qiancheng</creatorcontrib><description>[Display omitted] •Trace additive effectively extends the cycle life of ZIBs.•The adsorbed NTA molecules reduce the de-solvation energy barrier.•NTA molecules provide a buffer layer to retard dendrite growth. Aqueous Zn-ion batteries (AZIBs) have attracted widespread attention due to their intrinsic safety, cost-effectiveness. However, active H2O in the solvated ions [Zn(H2O)6]2+ continuously migrate to the Zn surface to trigger hydrogen evolution reaction (HER) and accelerate Zn corrosion. Herein, Zn dendrites and the related by-products have been successfully inhibited by using trace amounts of Nitrilotriacetic acid (NTA). Theoretical research indicates that two carboxyl groups of NTA molecule strongly anchored on the Zn surface and exposed another carboxyl group outside. Due to the violent interaction of carboxyl groups of NTA with H2O, the de-solvation energy barrier of solvated Zn2+ ([Zn(H2O)6]2+) on the Zn surface was obviously decreased, inhibit the active water splitting. Meanwhile, the preferential adsorption of NTA on the Zn surface increases the thickness of electric double layer EDL and provides a buffer layer to hinder the dendrite growth. Using 0.04 M NTA as additives in 2.0 M ZnSO4 electrolyte, the cycling lifespan of both Zn||Zn symmetric and Zn||MnO2 full cells is markedly prolonged. This study provides certain perspectives for trace amounts of electrolyte additives to satisfy the demand of long-cycle life AZIBs.</description><identifier>ISSN: 0021-9797</identifier><identifier>ISSN: 1095-7103</identifier><identifier>EISSN: 1095-7103</identifier><identifier>DOI: 10.1016/j.jcis.2024.08.088</identifier><identifier>PMID: 39154439</identifier><language>eng</language><publisher>United States: Elsevier Inc</publisher><subject>Aqueous Zn-ion batteries ; De-solvation ; Electric double layer ; Nitrilotriacetic acid</subject><ispartof>Journal of colloid and interface science, 2025-01, Vol.677 (Pt B), p.462-471</ispartof><rights>2024 Elsevier Inc.</rights><rights>Copyright © 2024 Elsevier Inc. All rights reserved.</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><cites>FETCH-LOGICAL-c237t-2435d3879b1b0886474fc3ba14196153ffec39e1597b126a460464aa527ef6873</cites><orcidid>0000-0001-5480-1434</orcidid></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://dx.doi.org/10.1016/j.jcis.2024.08.088$$EHTML$$P50$$Gelsevier$$H</linktohtml><link.rule.ids>315,781,785,3551,27929,27930,46000</link.rule.ids><backlink>$$Uhttps://www.ncbi.nlm.nih.gov/pubmed/39154439$$D View this record in MEDLINE/PubMed$$Hfree_for_read</backlink></links><search><creatorcontrib>Qiao, Shizhe</creatorcontrib><creatorcontrib>Chang, Le</creatorcontrib><creatorcontrib>Cui, Ziyang</creatorcontrib><creatorcontrib>Wang, Dengke</creatorcontrib><creatorcontrib>Zhang, Wenming</creatorcontrib><creatorcontrib>Zhu, Qiancheng</creatorcontrib><title>Tuning Zn-ion de-solvation chemistry with trace amount of additive towards stable Aqueous Zn anodes</title><title>Journal of colloid and interface science</title><addtitle>J Colloid Interface Sci</addtitle><description>[Display omitted] •Trace additive effectively extends the cycle life of ZIBs.•The adsorbed NTA molecules reduce the de-solvation energy barrier.•NTA molecules provide a buffer layer to retard dendrite growth. Aqueous Zn-ion batteries (AZIBs) have attracted widespread attention due to their intrinsic safety, cost-effectiveness. However, active H2O in the solvated ions [Zn(H2O)6]2+ continuously migrate to the Zn surface to trigger hydrogen evolution reaction (HER) and accelerate Zn corrosion. Herein, Zn dendrites and the related by-products have been successfully inhibited by using trace amounts of Nitrilotriacetic acid (NTA). Theoretical research indicates that two carboxyl groups of NTA molecule strongly anchored on the Zn surface and exposed another carboxyl group outside. Due to the violent interaction of carboxyl groups of NTA with H2O, the de-solvation energy barrier of solvated Zn2+ ([Zn(H2O)6]2+) on the Zn surface was obviously decreased, inhibit the active water splitting. Meanwhile, the preferential adsorption of NTA on the Zn surface increases the thickness of electric double layer EDL and provides a buffer layer to hinder the dendrite growth. Using 0.04 M NTA as additives in 2.0 M ZnSO4 electrolyte, the cycling lifespan of both Zn||Zn symmetric and Zn||MnO2 full cells is markedly prolonged. This study provides certain perspectives for trace amounts of electrolyte additives to satisfy the demand of long-cycle life AZIBs.</description><subject>Aqueous Zn-ion batteries</subject><subject>De-solvation</subject><subject>Electric double layer</subject><subject>Nitrilotriacetic acid</subject><issn>0021-9797</issn><issn>1095-7103</issn><issn>1095-7103</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2025</creationdate><recordtype>article</recordtype><recordid>eNp9UE1r3DAUFKWh2ST9Az0UHXPxRrJkyYJeliVfEMglueQiZOm50eK1tpK8If8-MrvJsTDweDAzzAxCvyhZUkLF1Wa5sT4ta1LzJWkL2m9oQYlqKkkJ-44WhNS0UlLJU3SW0oYQSptG_UCnTNGGc6YWyD5Nox__4pex8mHEDqoUhr3J82NfYetTju_4zedXnKOxgM02TGPGocfGOZ_9HnAObya6hFM23QB49W-CMKViic0YHKQLdNKbIcHP4z1HzzfXT-u76uHx9n69eqhszWSuas4ax1qpOtqVLoJL3lvWGcqpErRhfQ-WKaCNkh2theGCcMGNaWoJvWglO0eXB99dDCVDyrrEtzAMZpwDaUYU56IVaqbWB6qNIaUIvd5FvzXxXVOi53H1Rs_j6nlcTdqCtoh-H_2nbgvuS_K5ZiH8ORCgtNx7iDpZD6MF5yPYrF3w__P_ALA5iww</recordid><startdate>20250101</startdate><enddate>20250101</enddate><creator>Qiao, Shizhe</creator><creator>Chang, Le</creator><creator>Cui, Ziyang</creator><creator>Wang, Dengke</creator><creator>Zhang, Wenming</creator><creator>Zhu, Qiancheng</creator><general>Elsevier Inc</general><scope>NPM</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7X8</scope><orcidid>https://orcid.org/0000-0001-5480-1434</orcidid></search><sort><creationdate>20250101</creationdate><title>Tuning Zn-ion de-solvation chemistry with trace amount of additive towards stable Aqueous Zn anodes</title><author>Qiao, Shizhe ; Chang, Le ; Cui, Ziyang ; Wang, Dengke ; Zhang, Wenming ; Zhu, Qiancheng</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c237t-2435d3879b1b0886474fc3ba14196153ffec39e1597b126a460464aa527ef6873</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2025</creationdate><topic>Aqueous Zn-ion batteries</topic><topic>De-solvation</topic><topic>Electric double layer</topic><topic>Nitrilotriacetic acid</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Qiao, Shizhe</creatorcontrib><creatorcontrib>Chang, Le</creatorcontrib><creatorcontrib>Cui, Ziyang</creatorcontrib><creatorcontrib>Wang, Dengke</creatorcontrib><creatorcontrib>Zhang, Wenming</creatorcontrib><creatorcontrib>Zhu, Qiancheng</creatorcontrib><collection>PubMed</collection><collection>CrossRef</collection><collection>MEDLINE - Academic</collection><jtitle>Journal of colloid and interface science</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Qiao, Shizhe</au><au>Chang, Le</au><au>Cui, Ziyang</au><au>Wang, Dengke</au><au>Zhang, Wenming</au><au>Zhu, Qiancheng</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Tuning Zn-ion de-solvation chemistry with trace amount of additive towards stable Aqueous Zn anodes</atitle><jtitle>Journal of colloid and interface science</jtitle><addtitle>J Colloid Interface Sci</addtitle><date>2025-01-01</date><risdate>2025</risdate><volume>677</volume><issue>Pt B</issue><spage>462</spage><epage>471</epage><pages>462-471</pages><issn>0021-9797</issn><issn>1095-7103</issn><eissn>1095-7103</eissn><abstract>[Display omitted] •Trace additive effectively extends the cycle life of ZIBs.•The adsorbed NTA molecules reduce the de-solvation energy barrier.•NTA molecules provide a buffer layer to retard dendrite growth. Aqueous Zn-ion batteries (AZIBs) have attracted widespread attention due to their intrinsic safety, cost-effectiveness. However, active H2O in the solvated ions [Zn(H2O)6]2+ continuously migrate to the Zn surface to trigger hydrogen evolution reaction (HER) and accelerate Zn corrosion. Herein, Zn dendrites and the related by-products have been successfully inhibited by using trace amounts of Nitrilotriacetic acid (NTA). Theoretical research indicates that two carboxyl groups of NTA molecule strongly anchored on the Zn surface and exposed another carboxyl group outside. Due to the violent interaction of carboxyl groups of NTA with H2O, the de-solvation energy barrier of solvated Zn2+ ([Zn(H2O)6]2+) on the Zn surface was obviously decreased, inhibit the active water splitting. Meanwhile, the preferential adsorption of NTA on the Zn surface increases the thickness of electric double layer EDL and provides a buffer layer to hinder the dendrite growth. Using 0.04 M NTA as additives in 2.0 M ZnSO4 electrolyte, the cycling lifespan of both Zn||Zn symmetric and Zn||MnO2 full cells is markedly prolonged. This study provides certain perspectives for trace amounts of electrolyte additives to satisfy the demand of long-cycle life AZIBs.</abstract><cop>United States</cop><pub>Elsevier Inc</pub><pmid>39154439</pmid><doi>10.1016/j.jcis.2024.08.088</doi><tpages>10</tpages><orcidid>https://orcid.org/0000-0001-5480-1434</orcidid></addata></record>
fulltext fulltext
identifier ISSN: 0021-9797
ispartof Journal of colloid and interface science, 2025-01, Vol.677 (Pt B), p.462-471
issn 0021-9797
1095-7103
1095-7103
language eng
recordid cdi_proquest_miscellaneous_3094468697
source Elsevier ScienceDirect Journals Complete
subjects Aqueous Zn-ion batteries
De-solvation
Electric double layer
Nitrilotriacetic acid
title Tuning Zn-ion de-solvation chemistry with trace amount of additive towards stable Aqueous Zn anodes
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-13T03%3A52%3A35IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Tuning%20Zn-ion%20de-solvation%20chemistry%20with%20trace%20amount%20of%20additive%20towards%20stable%20Aqueous%20Zn%20anodes&rft.jtitle=Journal%20of%20colloid%20and%20interface%20science&rft.au=Qiao,%20Shizhe&rft.date=2025-01-01&rft.volume=677&rft.issue=Pt%20B&rft.spage=462&rft.epage=471&rft.pages=462-471&rft.issn=0021-9797&rft.eissn=1095-7103&rft_id=info:doi/10.1016/j.jcis.2024.08.088&rft_dat=%3Cproquest_cross%3E3094468697%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=3094468697&rft_id=info:pmid/39154439&rft_els_id=S0021979724018678&rfr_iscdi=true