High-temperature oxidation behavior and mechanism of Si3N4/Si3N4w/TiN nanocomposites ceramic cutting tool materials
High-temperature oxidation behaviors were observed through the SEM, TEM and XRD observation. Only a few intergranular TiN grains are oxidized into TiO2 oxidation layers at 850 deg C, owning to intragranular structure of nanocomposites, and the thickness of oxidation layer without porosity is very th...
Gespeichert in:
Veröffentlicht in: | Materials science & engineering. A, Structural materials : properties, microstructure and processing Structural materials : properties, microstructure and processing, 2007-06, Vol.459 (1-2), p.86-93 |
---|---|