Design of Glass-Ceramic Matrix by Modification of Microstructure for High Strength LTCC Application

For low temperature co-fired ceramics (LTCC) materials, BaO-B2O3-MgO-Al2O3 glass system was tested. The starting temperature for densification of a sintered body was at 700°C and the onset temperature for crystallization of a sintered body was 820°C. With the sintering temperature, the sintered body...