Interfacial microstructure and strength of lead-free Sn-Zn-RE BGA solder bumps

Rare earth (RE) elements, primarily La and Ce, were doped in Sn-Zn solder to improve its properties such as wettability. The interfacial microstructure evolution and shear strength of the Sn-9Zn and Sn-9Zn-0.5RE (in wt%) solder bumps on Au/Ni/Cu under bump metallization (UBM) in a ball grid array (B...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:IEEE transactions on advanced packaging 2005-05, Vol.28 (2), p.252-258
Hauptverfasser: Law, C.M.T., Wu, C.M.L., Yu, D.Q., Li, M., Chi, D.Z.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Rare earth (RE) elements, primarily La and Ce, were doped in Sn-Zn solder to improve its properties such as wettability. The interfacial microstructure evolution and shear strength of the Sn-9Zn and Sn-9Zn-0.5RE (in wt%) solder bumps on Au/Ni/Cu under bump metallization (UBM) in a ball grid array (BGA) were investigated after thermal aging at 150 /spl deg/C for up to 1000 h. In the as-reflowed Sn-9Zn solder bump, AuSn/sub 4/ intermetallic compounds (IMCs) and Au-Zn circular IMCs formed close to the solder/UBM interface, together with the formation of a Ni-Zn-Sn ternary IMC layer of about 1 /spl mu/m in thickness. In contrast, in the as-reflowed Sn-9Zn-0.5RE solder bump, a spalled layer of Au-Zn was formed above the Ni layer. Sn-Ce-La and Sn-Zn-Ce-La phases were found near the interface at positions near the surface of the solder ball. Upon thermal aging at 150 /spl deg/C, the concentration of Zn in the Ni-Zn-Sn ternary layer of Sn-9Zn increased with aging time. For Sn-9Zn-0.5RE, the Au-Zn layer began to dissolve after 500 h of thermal aging. The shear strength of the Sn-9Zn ball was decreased after the addition of RE elements, although it was still higher than that of the Sn-37Pb and Sn-36Pb-2Ag Pb-bearing solders. The fracture mode of the Sn-9Zn system was changed from ductile to partly brittle after adding the RE elements. This is mainly due to the presence of the brittle Au-Zn layer.
ISSN:1521-3323
1557-9980
DOI:10.1109/TADVP.2005.846939