Early hydration of C4AF with silica fume and its role on katoite composition

C4AF is considered the least reactive main clinker phase, but its reactivity may be affected by adding supplementary cementitious materials (SCMs). Pure C4AF was synthesised in a laboratory furnace, and the role of silica fume without gypsum on its early hydration properties was monitored. Burning w...