Preparation and properties of toughened yellow zirconia ceramics
To obtain the high toughness yellow ceramic, using the Y2O3 (5%) stabilized ZrO2 as main starting material, Al2O3 as toughen reagent, NH4VO3, V2O5 as colorant, and mixed with ball mill, molded with dry press method and two times sintered. By testing the properties and structure of the ceramic, we ha...
Gespeichert in:
Veröffentlicht in: | Inorganic materials 2006-06, Vol.42 (6), p.681-683 |
---|---|
Hauptverfasser: | , , , , |
Format: | Artikel |
Sprache: | eng |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 683 |
---|---|
container_issue | 6 |
container_start_page | 681 |
container_title | Inorganic materials |
container_volume | 42 |
creator | Zhang, Peiping Wu, Guoxue Chi, Xioguo Wang, Yujie Liu, Shufeng |
description | To obtain the high toughness yellow ceramic, using the Y2O3 (5%) stabilized ZrO2 as main starting material, Al2O3 as toughen reagent, NH4VO3, V2O5 as colorant, and mixed with ball mill, molded with dry press method and two times sintered. By testing the properties and structure of the ceramic, we have optimized the best technical conditions, and the mechanism of toughness and color present has been studied. The result shows that the NH4VO3 as colorant is better than V2O5, and the color is between X = 0.396-0.412 and Y = 0.402-0.390. The highest bending strength of toughened ZrO2 ceramics is .1138 MPa, and the fracture toughness is 14.8 MPa m1/2. The toughen mechanism is that phase transformation of ZrO2 and the dispersion of toughen reagents, and the color causing is by the colorful ion (V4+) entered into the zirconia crystals lattice of the ceramic. |
doi_str_mv | 10.1134/S0020168506060185 |
format | Article |
fullrecord | <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_29308584</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>29182812</sourcerecordid><originalsourceid>FETCH-LOGICAL-c307t-a47131638d294f56b3f6e69edabe51374d49bfd4fcda24f190ad0e569ad332963</originalsourceid><addsrcrecordid>eNqNkE1LAzEYhIMoWKs_wFtO3lbz5muTm1K0CgUF9bykyRtdaTdrskXqr3dLvXmROcxhHoZhCDkHdgkg5NUzY5yBNorpUWDUAZmAZqYSUPNDMtnF1S4_JielfDDGpDJ2Qq6fMvYuu6FNHXVdoH1OPeahxUJTpEPavL1jh4FucbVKX_S7zT51raMes1u3vpySo-hWBc9-fUpe725fZvfV4nH-MLtZVF6weqicrEGAFiZwK6PSSxE1aovBLVGBqGWQdhmDjD44LiNY5gJDpa0LQnCrxZRc7HvHgZ8bLEOzbosfR7kO06Y03ApmlJH_AMFwA3wEYQ_6nErJGJs-t2uXtw2wZndq8-dU8QM-oGnG</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>29182812</pqid></control><display><type>article</type><title>Preparation and properties of toughened yellow zirconia ceramics</title><source>SpringerLink Journals</source><creator>Zhang, Peiping ; Wu, Guoxue ; Chi, Xioguo ; Wang, Yujie ; Liu, Shufeng</creator><creatorcontrib>Zhang, Peiping ; Wu, Guoxue ; Chi, Xioguo ; Wang, Yujie ; Liu, Shufeng</creatorcontrib><description>To obtain the high toughness yellow ceramic, using the Y2O3 (5%) stabilized ZrO2 as main starting material, Al2O3 as toughen reagent, NH4VO3, V2O5 as colorant, and mixed with ball mill, molded with dry press method and two times sintered. By testing the properties and structure of the ceramic, we have optimized the best technical conditions, and the mechanism of toughness and color present has been studied. The result shows that the NH4VO3 as colorant is better than V2O5, and the color is between X = 0.396-0.412 and Y = 0.402-0.390. The highest bending strength of toughened ZrO2 ceramics is .1138 MPa, and the fracture toughness is 14.8 MPa m1/2. The toughen mechanism is that phase transformation of ZrO2 and the dispersion of toughen reagents, and the color causing is by the colorful ion (V4+) entered into the zirconia crystals lattice of the ceramic.</description><identifier>ISSN: 0020-1685</identifier><identifier>EISSN: 1608-3172</identifier><identifier>DOI: 10.1134/S0020168506060185</identifier><language>eng</language><ispartof>Inorganic materials, 2006-06, Vol.42 (6), p.681-683</ispartof><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c307t-a47131638d294f56b3f6e69edabe51374d49bfd4fcda24f190ad0e569ad332963</citedby><cites>FETCH-LOGICAL-c307t-a47131638d294f56b3f6e69edabe51374d49bfd4fcda24f190ad0e569ad332963</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27924,27925</link.rule.ids></links><search><creatorcontrib>Zhang, Peiping</creatorcontrib><creatorcontrib>Wu, Guoxue</creatorcontrib><creatorcontrib>Chi, Xioguo</creatorcontrib><creatorcontrib>Wang, Yujie</creatorcontrib><creatorcontrib>Liu, Shufeng</creatorcontrib><title>Preparation and properties of toughened yellow zirconia ceramics</title><title>Inorganic materials</title><description>To obtain the high toughness yellow ceramic, using the Y2O3 (5%) stabilized ZrO2 as main starting material, Al2O3 as toughen reagent, NH4VO3, V2O5 as colorant, and mixed with ball mill, molded with dry press method and two times sintered. By testing the properties and structure of the ceramic, we have optimized the best technical conditions, and the mechanism of toughness and color present has been studied. The result shows that the NH4VO3 as colorant is better than V2O5, and the color is between X = 0.396-0.412 and Y = 0.402-0.390. The highest bending strength of toughened ZrO2 ceramics is .1138 MPa, and the fracture toughness is 14.8 MPa m1/2. The toughen mechanism is that phase transformation of ZrO2 and the dispersion of toughen reagents, and the color causing is by the colorful ion (V4+) entered into the zirconia crystals lattice of the ceramic.</description><issn>0020-1685</issn><issn>1608-3172</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2006</creationdate><recordtype>article</recordtype><recordid>eNqNkE1LAzEYhIMoWKs_wFtO3lbz5muTm1K0CgUF9bykyRtdaTdrskXqr3dLvXmROcxhHoZhCDkHdgkg5NUzY5yBNorpUWDUAZmAZqYSUPNDMtnF1S4_JielfDDGpDJ2Qq6fMvYuu6FNHXVdoH1OPeahxUJTpEPavL1jh4FucbVKX_S7zT51raMes1u3vpySo-hWBc9-fUpe725fZvfV4nH-MLtZVF6weqicrEGAFiZwK6PSSxE1aovBLVGBqGWQdhmDjD44LiNY5gJDpa0LQnCrxZRc7HvHgZ8bLEOzbosfR7kO06Y03ApmlJH_AMFwA3wEYQ_6nErJGJs-t2uXtw2wZndq8-dU8QM-oGnG</recordid><startdate>20060601</startdate><enddate>20060601</enddate><creator>Zhang, Peiping</creator><creator>Wu, Guoxue</creator><creator>Chi, Xioguo</creator><creator>Wang, Yujie</creator><creator>Liu, Shufeng</creator><scope>AAYXX</scope><scope>CITATION</scope><scope>7QQ</scope><scope>7SR</scope><scope>8BQ</scope><scope>8FD</scope><scope>JG9</scope><scope>7QF</scope></search><sort><creationdate>20060601</creationdate><title>Preparation and properties of toughened yellow zirconia ceramics</title><author>Zhang, Peiping ; Wu, Guoxue ; Chi, Xioguo ; Wang, Yujie ; Liu, Shufeng</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c307t-a47131638d294f56b3f6e69edabe51374d49bfd4fcda24f190ad0e569ad332963</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2006</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Zhang, Peiping</creatorcontrib><creatorcontrib>Wu, Guoxue</creatorcontrib><creatorcontrib>Chi, Xioguo</creatorcontrib><creatorcontrib>Wang, Yujie</creatorcontrib><creatorcontrib>Liu, Shufeng</creatorcontrib><collection>CrossRef</collection><collection>Ceramic Abstracts</collection><collection>Engineered Materials Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><collection>Aluminium Industry Abstracts</collection><jtitle>Inorganic materials</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Zhang, Peiping</au><au>Wu, Guoxue</au><au>Chi, Xioguo</au><au>Wang, Yujie</au><au>Liu, Shufeng</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Preparation and properties of toughened yellow zirconia ceramics</atitle><jtitle>Inorganic materials</jtitle><date>2006-06-01</date><risdate>2006</risdate><volume>42</volume><issue>6</issue><spage>681</spage><epage>683</epage><pages>681-683</pages><issn>0020-1685</issn><eissn>1608-3172</eissn><abstract>To obtain the high toughness yellow ceramic, using the Y2O3 (5%) stabilized ZrO2 as main starting material, Al2O3 as toughen reagent, NH4VO3, V2O5 as colorant, and mixed with ball mill, molded with dry press method and two times sintered. By testing the properties and structure of the ceramic, we have optimized the best technical conditions, and the mechanism of toughness and color present has been studied. The result shows that the NH4VO3 as colorant is better than V2O5, and the color is between X = 0.396-0.412 and Y = 0.402-0.390. The highest bending strength of toughened ZrO2 ceramics is .1138 MPa, and the fracture toughness is 14.8 MPa m1/2. The toughen mechanism is that phase transformation of ZrO2 and the dispersion of toughen reagents, and the color causing is by the colorful ion (V4+) entered into the zirconia crystals lattice of the ceramic.</abstract><doi>10.1134/S0020168506060185</doi><tpages>3</tpages></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0020-1685 |
ispartof | Inorganic materials, 2006-06, Vol.42 (6), p.681-683 |
issn | 0020-1685 1608-3172 |
language | eng |
recordid | cdi_proquest_miscellaneous_29308584 |
source | SpringerLink Journals |
title | Preparation and properties of toughened yellow zirconia ceramics |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T09%3A24%3A50IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Preparation%20and%20properties%20of%20toughened%20yellow%20zirconia%20ceramics&rft.jtitle=Inorganic%20materials&rft.au=Zhang,%20Peiping&rft.date=2006-06-01&rft.volume=42&rft.issue=6&rft.spage=681&rft.epage=683&rft.pages=681-683&rft.issn=0020-1685&rft.eissn=1608-3172&rft_id=info:doi/10.1134/S0020168506060185&rft_dat=%3Cproquest_cross%3E29182812%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=29182812&rft_id=info:pmid/&rfr_iscdi=true |