Low Temperature Sintering of Alumina by CuO-TiO2-Nb2O5 Additives
We examined sintering additives for alumina. When using CuO-TiO2-Nb2O5 additive, dense sintered alumina was obtained by firing at 1000°C or below, even though additive content was at most 10 mass%. It is considered that the formation of mixed oxide consists of CuO, TiO2 and Nb2O5 has an important ro...