Composition dependent ductility in the amorphous Zr–Ti–Ni–Cu–Be alloy system

This work maps the bending ductility versus composition of amorphous alloys in the Zr–Ti–Ni–Cu–Be system. Alloys with a Zr:Ti ratio of 5.67:1 show higher ductility and thermal stability over a wider composition range than those with a Zr:Ti ratio of 3:1. The loss of ductility occurs in alloys that h...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Scripta materialia 2006-10, Vol.55 (7), p.645-648
Hauptverfasser: Conner, R.D., Johnson, W.L.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:This work maps the bending ductility versus composition of amorphous alloys in the Zr–Ti–Ni–Cu–Be system. Alloys with a Zr:Ti ratio of 5.67:1 show higher ductility and thermal stability over a wider composition range than those with a Zr:Ti ratio of 3:1. The loss of ductility occurs in alloys that have compositions near those of quasicrystal or intermetallic phases, which form in the amorphous matrix upon cooling.
ISSN:1359-6462
0956-716X
1872-8456
DOI:10.1016/j.scriptamat.2006.06.003