State of Small Amount of Elements in Silicon Nitride Fabricated by Post-Sintering Process Using Low-Grade Silicon Powder as Raw Materials

The state of small amount of elements containing impurity in silicon nitride produced by the post sintering method from low-grade silicon powder was investigated. Iron reacted with other components in the raw materials in the sintering process to form iron silicide particles which were subsequently...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of the Ceramic Society of Japan 2004, Vol.112(1312), pp.665-668
Hauptverfasser: KITA, Hideki, OSUMI, Kazuo, UENO, Syunkichi, JAYASEELAN, D. Doni, IIZUKA, Tateoki
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 668
container_issue 1312
container_start_page 665
container_title Journal of the Ceramic Society of Japan
container_volume 112
creator KITA, Hideki
OSUMI, Kazuo
UENO, Syunkichi
JAYASEELAN, D. Doni
IIZUKA, Tateoki
description The state of small amount of elements containing impurity in silicon nitride produced by the post sintering method from low-grade silicon powder was investigated. Iron reacted with other components in the raw materials in the sintering process to form iron silicide particles which were subsequently distributed. Most particles were as large as 2 μm in diameter. Linear voids that were considered to originate in the difference of thermal expansion coefficients were observed in their perimeter. Ta2O5 also reacted with other elements and it was observed in the form of tantalum silicide particles. The size was few hundreds nanometer. Calcium was detected from multigrain pockets. However, not a particular particle segregation could be observed. For this reason, it is presumed that Calcium was solved into the grain-boundary phase.
doi_str_mv 10.2109/jcersj.112.665
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_29193344</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>29193344</sourcerecordid><originalsourceid>FETCH-LOGICAL-c436t-d723333b94d65673ef42430cb8c95069b63adb6e25e268613cec5591063aa3883</originalsourceid><addsrcrecordid>eNqFkU2LFDEQhoMoOKx79RwQvPWY70mOy7IfyqiD455DOl2zZuhO1iTDsD_Bf22acRfxYg6pqvA8BeFF6C0lS0aJ-bD3kMt-SSlbKiVfoAXVmnWUMPYSLYihopOCkNfovJTQE8KEForwBfq1ra4CTju8ndw44ospHWKd56sRJoi14BDxNozBp4i_hJrDAPja9Tn4Jg64f8SbVGq3DbFCDvEeb3LyUAq-K_O0TsfuJrsmPS3ZpOMAGbuCv7kj_uxmzY3lDXq1awXO_9QzdHd99f3ytlt_vfl4ebHuvOCqdsOK8XZ6IwYl1YrDTjDBie-1N5Io0yvuhl4Bk8CUVpR78FIaStq741rzM_T-tPchp58HKNVOoXgYRxchHYplhhrOhfg_qAVZKSEb-O4fcJ8OObZPWCqE1IYwThq1PFE-p1Iy7OxDDpPLj5YSO2doTxnalqFtGTbh00nYl-ru4Rl3uQY_wt845fP11DT5GfI_XLYQ-W-yBqle</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1445890230</pqid></control><display><type>article</type><title>State of Small Amount of Elements in Silicon Nitride Fabricated by Post-Sintering Process Using Low-Grade Silicon Powder as Raw Materials</title><source>J-STAGE (Japan Science &amp; Technology Information Aggregator, Electronic) Freely Available Titles - Japanese</source><source>EZB-FREE-00999 freely available EZB journals</source><source>Free Full-Text Journals in Chemistry</source><creator>KITA, Hideki ; OSUMI, Kazuo ; UENO, Syunkichi ; JAYASEELAN, D. Doni ; IIZUKA, Tateoki</creator><creatorcontrib>KITA, Hideki ; OSUMI, Kazuo ; UENO, Syunkichi ; JAYASEELAN, D. Doni ; IIZUKA, Tateoki</creatorcontrib><description>The state of small amount of elements containing impurity in silicon nitride produced by the post sintering method from low-grade silicon powder was investigated. Iron reacted with other components in the raw materials in the sintering process to form iron silicide particles which were subsequently distributed. Most particles were as large as 2 μm in diameter. Linear voids that were considered to originate in the difference of thermal expansion coefficients were observed in their perimeter. Ta2O5 also reacted with other elements and it was observed in the form of tantalum silicide particles. The size was few hundreds nanometer. Calcium was detected from multigrain pockets. However, not a particular particle segregation could be observed. For this reason, it is presumed that Calcium was solved into the grain-boundary phase.</description><identifier>ISSN: 0914-5400</identifier><identifier>ISSN: 1882-0743</identifier><identifier>EISSN: 1882-1022</identifier><identifier>EISSN: 1348-6535</identifier><identifier>DOI: 10.2109/jcersj.112.665</identifier><language>eng</language><publisher>Tokyo: The Ceramic Society of Japan</publisher><subject>Calcium ; Cost ; Impurity ; Iron ; Post-sintering ; Reaction-bonding ; Silicon nitride</subject><ispartof>Journal of the Ceramic Society of Japan, 2004, Vol.112(1312), pp.665-668</ispartof><rights>2004 The Ceramic Society of Japan</rights><rights>Copyright Japan Science and Technology Agency 2004</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c436t-d723333b94d65673ef42430cb8c95069b63adb6e25e268613cec5591063aa3883</citedby><cites>FETCH-LOGICAL-c436t-d723333b94d65673ef42430cb8c95069b63adb6e25e268613cec5591063aa3883</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,1883,4024,27923,27924,27925</link.rule.ids></links><search><creatorcontrib>KITA, Hideki</creatorcontrib><creatorcontrib>OSUMI, Kazuo</creatorcontrib><creatorcontrib>UENO, Syunkichi</creatorcontrib><creatorcontrib>JAYASEELAN, D. Doni</creatorcontrib><creatorcontrib>IIZUKA, Tateoki</creatorcontrib><title>State of Small Amount of Elements in Silicon Nitride Fabricated by Post-Sintering Process Using Low-Grade Silicon Powder as Raw Materials</title><title>Journal of the Ceramic Society of Japan</title><addtitle>J. Ceram. Soc. Japan</addtitle><description>The state of small amount of elements containing impurity in silicon nitride produced by the post sintering method from low-grade silicon powder was investigated. Iron reacted with other components in the raw materials in the sintering process to form iron silicide particles which were subsequently distributed. Most particles were as large as 2 μm in diameter. Linear voids that were considered to originate in the difference of thermal expansion coefficients were observed in their perimeter. Ta2O5 also reacted with other elements and it was observed in the form of tantalum silicide particles. The size was few hundreds nanometer. Calcium was detected from multigrain pockets. However, not a particular particle segregation could be observed. For this reason, it is presumed that Calcium was solved into the grain-boundary phase.</description><subject>Calcium</subject><subject>Cost</subject><subject>Impurity</subject><subject>Iron</subject><subject>Post-sintering</subject><subject>Reaction-bonding</subject><subject>Silicon nitride</subject><issn>0914-5400</issn><issn>1882-0743</issn><issn>1882-1022</issn><issn>1348-6535</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2004</creationdate><recordtype>article</recordtype><recordid>eNqFkU2LFDEQhoMoOKx79RwQvPWY70mOy7IfyqiD455DOl2zZuhO1iTDsD_Bf22acRfxYg6pqvA8BeFF6C0lS0aJ-bD3kMt-SSlbKiVfoAXVmnWUMPYSLYihopOCkNfovJTQE8KEForwBfq1ra4CTju8ndw44ospHWKd56sRJoi14BDxNozBp4i_hJrDAPja9Tn4Jg64f8SbVGq3DbFCDvEeb3LyUAq-K_O0TsfuJrsmPS3ZpOMAGbuCv7kj_uxmzY3lDXq1awXO_9QzdHd99f3ytlt_vfl4ebHuvOCqdsOK8XZ6IwYl1YrDTjDBie-1N5Io0yvuhl4Bk8CUVpR78FIaStq741rzM_T-tPchp58HKNVOoXgYRxchHYplhhrOhfg_qAVZKSEb-O4fcJ8OObZPWCqE1IYwThq1PFE-p1Iy7OxDDpPLj5YSO2doTxnalqFtGTbh00nYl-ru4Rl3uQY_wt845fP11DT5GfI_XLYQ-W-yBqle</recordid><startdate>2004</startdate><enddate>2004</enddate><creator>KITA, Hideki</creator><creator>OSUMI, Kazuo</creator><creator>UENO, Syunkichi</creator><creator>JAYASEELAN, D. Doni</creator><creator>IIZUKA, Tateoki</creator><general>The Ceramic Society of Japan</general><general>Japan Science and Technology Agency</general><scope>AAYXX</scope><scope>CITATION</scope><scope>7QQ</scope><scope>7SR</scope><scope>8FD</scope><scope>JG9</scope></search><sort><creationdate>2004</creationdate><title>State of Small Amount of Elements in Silicon Nitride Fabricated by Post-Sintering Process Using Low-Grade Silicon Powder as Raw Materials</title><author>KITA, Hideki ; OSUMI, Kazuo ; UENO, Syunkichi ; JAYASEELAN, D. Doni ; IIZUKA, Tateoki</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c436t-d723333b94d65673ef42430cb8c95069b63adb6e25e268613cec5591063aa3883</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2004</creationdate><topic>Calcium</topic><topic>Cost</topic><topic>Impurity</topic><topic>Iron</topic><topic>Post-sintering</topic><topic>Reaction-bonding</topic><topic>Silicon nitride</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>KITA, Hideki</creatorcontrib><creatorcontrib>OSUMI, Kazuo</creatorcontrib><creatorcontrib>UENO, Syunkichi</creatorcontrib><creatorcontrib>JAYASEELAN, D. Doni</creatorcontrib><creatorcontrib>IIZUKA, Tateoki</creatorcontrib><collection>CrossRef</collection><collection>Ceramic Abstracts</collection><collection>Engineered Materials Abstracts</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><jtitle>Journal of the Ceramic Society of Japan</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>KITA, Hideki</au><au>OSUMI, Kazuo</au><au>UENO, Syunkichi</au><au>JAYASEELAN, D. Doni</au><au>IIZUKA, Tateoki</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>State of Small Amount of Elements in Silicon Nitride Fabricated by Post-Sintering Process Using Low-Grade Silicon Powder as Raw Materials</atitle><jtitle>Journal of the Ceramic Society of Japan</jtitle><addtitle>J. Ceram. Soc. Japan</addtitle><date>2004</date><risdate>2004</risdate><volume>112</volume><issue>1312</issue><spage>665</spage><epage>668</epage><pages>665-668</pages><issn>0914-5400</issn><issn>1882-0743</issn><eissn>1882-1022</eissn><eissn>1348-6535</eissn><abstract>The state of small amount of elements containing impurity in silicon nitride produced by the post sintering method from low-grade silicon powder was investigated. Iron reacted with other components in the raw materials in the sintering process to form iron silicide particles which were subsequently distributed. Most particles were as large as 2 μm in diameter. Linear voids that were considered to originate in the difference of thermal expansion coefficients were observed in their perimeter. Ta2O5 also reacted with other elements and it was observed in the form of tantalum silicide particles. The size was few hundreds nanometer. Calcium was detected from multigrain pockets. However, not a particular particle segregation could be observed. For this reason, it is presumed that Calcium was solved into the grain-boundary phase.</abstract><cop>Tokyo</cop><pub>The Ceramic Society of Japan</pub><doi>10.2109/jcersj.112.665</doi><tpages>4</tpages><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 0914-5400
ispartof Journal of the Ceramic Society of Japan, 2004, Vol.112(1312), pp.665-668
issn 0914-5400
1882-0743
1882-1022
1348-6535
language eng
recordid cdi_proquest_miscellaneous_29193344
source J-STAGE (Japan Science & Technology Information Aggregator, Electronic) Freely Available Titles - Japanese; EZB-FREE-00999 freely available EZB journals; Free Full-Text Journals in Chemistry
subjects Calcium
Cost
Impurity
Iron
Post-sintering
Reaction-bonding
Silicon nitride
title State of Small Amount of Elements in Silicon Nitride Fabricated by Post-Sintering Process Using Low-Grade Silicon Powder as Raw Materials
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-29T05%3A10%3A46IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=State%20of%20Small%20Amount%20of%20Elements%20in%20Silicon%20Nitride%20Fabricated%20by%20Post-Sintering%20Process%20Using%20Low-Grade%20Silicon%20Powder%20as%20Raw%20Materials&rft.jtitle=Journal%20of%20the%20Ceramic%20Society%20of%20Japan&rft.au=KITA,%20Hideki&rft.date=2004&rft.volume=112&rft.issue=1312&rft.spage=665&rft.epage=668&rft.pages=665-668&rft.issn=0914-5400&rft.eissn=1882-1022&rft_id=info:doi/10.2109/jcersj.112.665&rft_dat=%3Cproquest_cross%3E29193344%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1445890230&rft_id=info:pmid/&rfr_iscdi=true