Coalescence and breakup of contact areas: Effects on surface temperatures
In a study of the mechanisms by which thin polymeric films can prevent or delay the onset of fretting corrosion, experimental observations were made of the apparent real area of contact and temperatures generated by friction in a dry-sliding system consisting of stationary polymer-coated steel balls...