Integration of wood-based components – Cellulose nanofibrils and tannic acid - into a poly(vinyl alcohol) matrix to improve functional properties

Poly(vinyl alcohol) (PVA) biocomposite films reinforced with cellulose nanofibrils (CNF) and biologically active tannic acid (TA) were prepared. The influence of different concentrations of CNF and TA in the PVA polymer matrix was investigated in terms of mechanical properties, thermal properties an...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:International journal of biological macromolecules 2024-01, Vol.256 (Pt 2), p.128495-128495, Article 128495
Hauptverfasser: Osolnik, Urša, Vek, Viljem, Korošec, Romana Cerc, Oven, Primož, Poljanšek, Ida
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 128495
container_issue Pt 2
container_start_page 128495
container_title International journal of biological macromolecules
container_volume 256
creator Osolnik, Urša
Vek, Viljem
Korošec, Romana Cerc
Oven, Primož
Poljanšek, Ida
description Poly(vinyl alcohol) (PVA) biocomposite films reinforced with cellulose nanofibrils (CNF) and biologically active tannic acid (TA) were prepared. The influence of different concentrations of CNF and TA in the PVA polymer matrix was investigated in terms of mechanical properties, thermal properties and hydrophobicity improvement of the prepared films. The results showed that in all cases the addition of CNF and TA improved the values of tensile strength and elastic modulus. The PVA film with 10 % CNF exhibited a 30 % higher tensile strength, and the three-component PVA film with 2 % CNF and 10 % TA (P2C10T) exhibited a 40 % higher tensile strength compared to the neat PVA film. The thermal properties (Tg, Tonset) of the PVA biocomposite films were greatly improved, with a significant effect observed for the three-component PVA films. The Tg of the PVA film with 10 % CNF and 10 % TA was 87 °C, 12 °C higher than that of the neat PVA film. For three-component PVA biocomposites with 4 % and 6 % CNF and with all weight percentages of TA, the Tonset shifted to a higher temperature range by about 30 °C compared to the neat PVA film. The PVA film with 2 % CNF and 10 % TA exhibited about a 20° higher contact angle than the neat PVA film. Moreover, the addition of both fillers to the PVA matrix resulted in PVA biocomposites with lower water absorption. PVA film with 10 % TA absorbed about 90 % less water and PVA film with 10 % CNF and 10 % TA absorbed about 80 % less water than the neat PVA film after the films were soaked in water for one hour. The better properties of the composite films produced are due to hydrogen and ester bonds between the components of the composite, which was confirmed by FT-IR spectroscopy. Antioxidant effective films were also obtained due to the biologically active TA to the PVA and PVA/CNF systems. [Display omitted]
doi_str_mv 10.1016/j.ijbiomac.2023.128495
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_2896810239</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0141813023053941</els_id><sourcerecordid>2896810239</sourcerecordid><originalsourceid>FETCH-LOGICAL-c416t-2b52acbcec24f311c42fa0121df2b4d9f43b6bbfbbc20285850184cd59eb6c73</originalsourceid><addsrcrecordid>eNqFkctuFDEQRS0EIkPgFyIvw6IHP7o77h1oxCNSJDbZW36UwSO33djugdnxD_lDvgSPJmHLqqSqW3V16yB0RcmWEjq-22_9Xvs0K7NlhPEtZaKfhmdoQ8XN1BFC-HO0IbSnnaCcXKBXpexbdxyoeIkuuCB8mAa-QQ-3scK3rKpPESeHf6ZkO60KWGzSvKQIsRb85_cD3kEIa0gFcFQxOa-zDwWraHFVMXqDlfEWd9jHmrDCSwrH64OPx4BVMOl7Cm_xrGr2v3Cb-3nJ6QDYrdGcrFXArbFArh7Ka_TCqVDgzWO9RPefPt7vvnR3Xz_f7j7cdaanY-2YHpgy2oBhveOUmp45RSij1jHd28n1XI9aO61Ne5EYxECo6I0dJtCjueGX6Pp8tjn_WKFUOftiWkoVIa1FMjGNgrbnTk06nqUmp1IyOLlkP6t8lJTIEw-5l0885ImHPPNoi1ePHquewf5bewLQBO_PAmhBDx6yLMZDNGB9BlOlTf5_Hn8BlCCjuA</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>2896810239</pqid></control><display><type>article</type><title>Integration of wood-based components – Cellulose nanofibrils and tannic acid - into a poly(vinyl alcohol) matrix to improve functional properties</title><source>ScienceDirect Journals (5 years ago - present)</source><creator>Osolnik, Urša ; Vek, Viljem ; Korošec, Romana Cerc ; Oven, Primož ; Poljanšek, Ida</creator><creatorcontrib>Osolnik, Urša ; Vek, Viljem ; Korošec, Romana Cerc ; Oven, Primož ; Poljanšek, Ida</creatorcontrib><description>Poly(vinyl alcohol) (PVA) biocomposite films reinforced with cellulose nanofibrils (CNF) and biologically active tannic acid (TA) were prepared. The influence of different concentrations of CNF and TA in the PVA polymer matrix was investigated in terms of mechanical properties, thermal properties and hydrophobicity improvement of the prepared films. The results showed that in all cases the addition of CNF and TA improved the values of tensile strength and elastic modulus. The PVA film with 10 % CNF exhibited a 30 % higher tensile strength, and the three-component PVA film with 2 % CNF and 10 % TA (P2C10T) exhibited a 40 % higher tensile strength compared to the neat PVA film. The thermal properties (Tg, Tonset) of the PVA biocomposite films were greatly improved, with a significant effect observed for the three-component PVA films. The Tg of the PVA film with 10 % CNF and 10 % TA was 87 °C, 12 °C higher than that of the neat PVA film. For three-component PVA biocomposites with 4 % and 6 % CNF and with all weight percentages of TA, the Tonset shifted to a higher temperature range by about 30 °C compared to the neat PVA film. The PVA film with 2 % CNF and 10 % TA exhibited about a 20° higher contact angle than the neat PVA film. Moreover, the addition of both fillers to the PVA matrix resulted in PVA biocomposites with lower water absorption. PVA film with 10 % TA absorbed about 90 % less water and PVA film with 10 % CNF and 10 % TA absorbed about 80 % less water than the neat PVA film after the films were soaked in water for one hour. The better properties of the composite films produced are due to hydrogen and ester bonds between the components of the composite, which was confirmed by FT-IR spectroscopy. Antioxidant effective films were also obtained due to the biologically active TA to the PVA and PVA/CNF systems. [Display omitted]</description><identifier>ISSN: 0141-8130</identifier><identifier>EISSN: 1879-0003</identifier><identifier>DOI: 10.1016/j.ijbiomac.2023.128495</identifier><identifier>PMID: 38035953</identifier><language>eng</language><publisher>Netherlands: Elsevier B.V</publisher><subject>Biocomposite ; Cellulose nanofibrils ; PVA ; Tannic acid</subject><ispartof>International journal of biological macromolecules, 2024-01, Vol.256 (Pt 2), p.128495-128495, Article 128495</ispartof><rights>2023 The Authors</rights><rights>Copyright © 2023 The Authors. Published by Elsevier B.V. All rights reserved.</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c416t-2b52acbcec24f311c42fa0121df2b4d9f43b6bbfbbc20285850184cd59eb6c73</citedby><cites>FETCH-LOGICAL-c416t-2b52acbcec24f311c42fa0121df2b4d9f43b6bbfbbc20285850184cd59eb6c73</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://dx.doi.org/10.1016/j.ijbiomac.2023.128495$$EHTML$$P50$$Gelsevier$$Hfree_for_read</linktohtml><link.rule.ids>314,780,784,3549,27923,27924,45994</link.rule.ids><backlink>$$Uhttps://www.ncbi.nlm.nih.gov/pubmed/38035953$$D View this record in MEDLINE/PubMed$$Hfree_for_read</backlink></links><search><creatorcontrib>Osolnik, Urša</creatorcontrib><creatorcontrib>Vek, Viljem</creatorcontrib><creatorcontrib>Korošec, Romana Cerc</creatorcontrib><creatorcontrib>Oven, Primož</creatorcontrib><creatorcontrib>Poljanšek, Ida</creatorcontrib><title>Integration of wood-based components – Cellulose nanofibrils and tannic acid - into a poly(vinyl alcohol) matrix to improve functional properties</title><title>International journal of biological macromolecules</title><addtitle>Int J Biol Macromol</addtitle><description>Poly(vinyl alcohol) (PVA) biocomposite films reinforced with cellulose nanofibrils (CNF) and biologically active tannic acid (TA) were prepared. The influence of different concentrations of CNF and TA in the PVA polymer matrix was investigated in terms of mechanical properties, thermal properties and hydrophobicity improvement of the prepared films. The results showed that in all cases the addition of CNF and TA improved the values of tensile strength and elastic modulus. The PVA film with 10 % CNF exhibited a 30 % higher tensile strength, and the three-component PVA film with 2 % CNF and 10 % TA (P2C10T) exhibited a 40 % higher tensile strength compared to the neat PVA film. The thermal properties (Tg, Tonset) of the PVA biocomposite films were greatly improved, with a significant effect observed for the three-component PVA films. The Tg of the PVA film with 10 % CNF and 10 % TA was 87 °C, 12 °C higher than that of the neat PVA film. For three-component PVA biocomposites with 4 % and 6 % CNF and with all weight percentages of TA, the Tonset shifted to a higher temperature range by about 30 °C compared to the neat PVA film. The PVA film with 2 % CNF and 10 % TA exhibited about a 20° higher contact angle than the neat PVA film. Moreover, the addition of both fillers to the PVA matrix resulted in PVA biocomposites with lower water absorption. PVA film with 10 % TA absorbed about 90 % less water and PVA film with 10 % CNF and 10 % TA absorbed about 80 % less water than the neat PVA film after the films were soaked in water for one hour. The better properties of the composite films produced are due to hydrogen and ester bonds between the components of the composite, which was confirmed by FT-IR spectroscopy. Antioxidant effective films were also obtained due to the biologically active TA to the PVA and PVA/CNF systems. [Display omitted]</description><subject>Biocomposite</subject><subject>Cellulose nanofibrils</subject><subject>PVA</subject><subject>Tannic acid</subject><issn>0141-8130</issn><issn>1879-0003</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2024</creationdate><recordtype>article</recordtype><recordid>eNqFkctuFDEQRS0EIkPgFyIvw6IHP7o77h1oxCNSJDbZW36UwSO33djugdnxD_lDvgSPJmHLqqSqW3V16yB0RcmWEjq-22_9Xvs0K7NlhPEtZaKfhmdoQ8XN1BFC-HO0IbSnnaCcXKBXpexbdxyoeIkuuCB8mAa-QQ-3scK3rKpPESeHf6ZkO60KWGzSvKQIsRb85_cD3kEIa0gFcFQxOa-zDwWraHFVMXqDlfEWd9jHmrDCSwrH64OPx4BVMOl7Cm_xrGr2v3Cb-3nJ6QDYrdGcrFXArbFArh7Ka_TCqVDgzWO9RPefPt7vvnR3Xz_f7j7cdaanY-2YHpgy2oBhveOUmp45RSij1jHd28n1XI9aO61Ne5EYxECo6I0dJtCjueGX6Pp8tjn_WKFUOftiWkoVIa1FMjGNgrbnTk06nqUmp1IyOLlkP6t8lJTIEw-5l0885ImHPPNoi1ePHquewf5bewLQBO_PAmhBDx6yLMZDNGB9BlOlTf5_Hn8BlCCjuA</recordid><startdate>202401</startdate><enddate>202401</enddate><creator>Osolnik, Urša</creator><creator>Vek, Viljem</creator><creator>Korošec, Romana Cerc</creator><creator>Oven, Primož</creator><creator>Poljanšek, Ida</creator><general>Elsevier B.V</general><scope>6I.</scope><scope>AAFTH</scope><scope>NPM</scope><scope>AAYXX</scope><scope>CITATION</scope><scope>7X8</scope></search><sort><creationdate>202401</creationdate><title>Integration of wood-based components – Cellulose nanofibrils and tannic acid - into a poly(vinyl alcohol) matrix to improve functional properties</title><author>Osolnik, Urša ; Vek, Viljem ; Korošec, Romana Cerc ; Oven, Primož ; Poljanšek, Ida</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c416t-2b52acbcec24f311c42fa0121df2b4d9f43b6bbfbbc20285850184cd59eb6c73</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2024</creationdate><topic>Biocomposite</topic><topic>Cellulose nanofibrils</topic><topic>PVA</topic><topic>Tannic acid</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Osolnik, Urša</creatorcontrib><creatorcontrib>Vek, Viljem</creatorcontrib><creatorcontrib>Korošec, Romana Cerc</creatorcontrib><creatorcontrib>Oven, Primož</creatorcontrib><creatorcontrib>Poljanšek, Ida</creatorcontrib><collection>ScienceDirect Open Access Titles</collection><collection>Elsevier:ScienceDirect:Open Access</collection><collection>PubMed</collection><collection>CrossRef</collection><collection>MEDLINE - Academic</collection><jtitle>International journal of biological macromolecules</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Osolnik, Urša</au><au>Vek, Viljem</au><au>Korošec, Romana Cerc</au><au>Oven, Primož</au><au>Poljanšek, Ida</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Integration of wood-based components – Cellulose nanofibrils and tannic acid - into a poly(vinyl alcohol) matrix to improve functional properties</atitle><jtitle>International journal of biological macromolecules</jtitle><addtitle>Int J Biol Macromol</addtitle><date>2024-01</date><risdate>2024</risdate><volume>256</volume><issue>Pt 2</issue><spage>128495</spage><epage>128495</epage><pages>128495-128495</pages><artnum>128495</artnum><issn>0141-8130</issn><eissn>1879-0003</eissn><abstract>Poly(vinyl alcohol) (PVA) biocomposite films reinforced with cellulose nanofibrils (CNF) and biologically active tannic acid (TA) were prepared. The influence of different concentrations of CNF and TA in the PVA polymer matrix was investigated in terms of mechanical properties, thermal properties and hydrophobicity improvement of the prepared films. The results showed that in all cases the addition of CNF and TA improved the values of tensile strength and elastic modulus. The PVA film with 10 % CNF exhibited a 30 % higher tensile strength, and the three-component PVA film with 2 % CNF and 10 % TA (P2C10T) exhibited a 40 % higher tensile strength compared to the neat PVA film. The thermal properties (Tg, Tonset) of the PVA biocomposite films were greatly improved, with a significant effect observed for the three-component PVA films. The Tg of the PVA film with 10 % CNF and 10 % TA was 87 °C, 12 °C higher than that of the neat PVA film. For three-component PVA biocomposites with 4 % and 6 % CNF and with all weight percentages of TA, the Tonset shifted to a higher temperature range by about 30 °C compared to the neat PVA film. The PVA film with 2 % CNF and 10 % TA exhibited about a 20° higher contact angle than the neat PVA film. Moreover, the addition of both fillers to the PVA matrix resulted in PVA biocomposites with lower water absorption. PVA film with 10 % TA absorbed about 90 % less water and PVA film with 10 % CNF and 10 % TA absorbed about 80 % less water than the neat PVA film after the films were soaked in water for one hour. The better properties of the composite films produced are due to hydrogen and ester bonds between the components of the composite, which was confirmed by FT-IR spectroscopy. Antioxidant effective films were also obtained due to the biologically active TA to the PVA and PVA/CNF systems. [Display omitted]</abstract><cop>Netherlands</cop><pub>Elsevier B.V</pub><pmid>38035953</pmid><doi>10.1016/j.ijbiomac.2023.128495</doi><tpages>1</tpages><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 0141-8130
ispartof International journal of biological macromolecules, 2024-01, Vol.256 (Pt 2), p.128495-128495, Article 128495
issn 0141-8130
1879-0003
language eng
recordid cdi_proquest_miscellaneous_2896810239
source ScienceDirect Journals (5 years ago - present)
subjects Biocomposite
Cellulose nanofibrils
PVA
Tannic acid
title Integration of wood-based components – Cellulose nanofibrils and tannic acid - into a poly(vinyl alcohol) matrix to improve functional properties
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T23%3A19%3A27IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Integration%20of%20wood-based%20components%20%E2%80%93%20Cellulose%20nanofibrils%20and%20tannic%20acid%20-%20into%20a%20poly(vinyl%20alcohol)%20matrix%20to%20improve%20functional%20properties&rft.jtitle=International%20journal%20of%20biological%20macromolecules&rft.au=Osolnik,%20Ur%C5%A1a&rft.date=2024-01&rft.volume=256&rft.issue=Pt%202&rft.spage=128495&rft.epage=128495&rft.pages=128495-128495&rft.artnum=128495&rft.issn=0141-8130&rft.eissn=1879-0003&rft_id=info:doi/10.1016/j.ijbiomac.2023.128495&rft_dat=%3Cproquest_cross%3E2896810239%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=2896810239&rft_id=info:pmid/38035953&rft_els_id=S0141813023053941&rfr_iscdi=true