Optimal Operational Conditions during Production of Lead-Calcium-Tin Anodes for Improve Their Mechanical Properties

Previous works have shown that a minimum yield strength s0 of 58 MPa for leadcalcium- tin anodes of 6 mm thickness and a nominal composition of 0.7% Ca and 1.3% Sn are required to avoid early deformations and distortions during their operation in copper electrowinning cell. This s0 value for the ano...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials science forum 2005-01, Vol.475-479, p.2631-2634