Characterization of Martensitic Transformation in Ferromagnetic Shape Memory Alloys Co-Ni-Ga Melt-Spun Ribbons

The martensitic transformation in Co50Ni20Ga30 ribbon has been characterized in detail by means of X-ray diffraction and magnetic measurements. The sample showed a structural transition from the body-centered cubic with indexed lattice parameters of a=5.743 Å to martensite with a tetragonal structur...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials science forum 2005-01, Vol.475-479, p.2033-2036
Hauptverfasser: Li, Yang Xian, Liu, G.D., Dai, X.F., Qu, J.P., Liu, H.Y., Meng, F.B., Zhang, M., Liu, Z.H., Wu, G.H., Chen, J.L.
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 2036
container_issue
container_start_page 2033
container_title Materials science forum
container_volume 475-479
creator Li, Yang Xian
Liu, G.D.
Dai, X.F.
Qu, J.P.
Liu, H.Y.
Meng, F.B.
Zhang, M.
Liu, Z.H.
Wu, G.H.
Chen, J.L.
description The martensitic transformation in Co50Ni20Ga30 ribbon has been characterized in detail by means of X-ray diffraction and magnetic measurements. The sample showed a structural transition from the body-centered cubic with indexed lattice parameters of a=5.743 Å to martensite with a tetragonal structure with lattice parameters of a=b=5.422 Å and c=6.401 Å. (c/a>1). By comparing the results of the diffraction intensity and the magnetic susceptibility measurements, we found that the proceeding of the martensitic transformation can be divided into several different steps during cooling from 283 K to 213 K. During heating from 673 K to 833 K, the peak width became very wide and the intensity became very low. It reveals an order-disorder transformation.
doi_str_mv 10.4028/www.scientific.net/MSF.475-479.2033
format Article
fullrecord <record><control><sourceid>proquest_cross</sourceid><recordid>TN_cdi_proquest_miscellaneous_28471680</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>28471680</sourcerecordid><originalsourceid>FETCH-LOGICAL-c304t-1459dbf9d9af3e6d45ea81f8e4768236259d0659a660fb89705174d1e7f2be243</originalsourceid><addsrcrecordid>eNqVkEFrGzEQhUVoIG6a_7CnXorWklbS7h7DYruBuIHaOQvtehQr7EquJGOcX18ZB3ruYRiY93jD-xD6QUnJCWvmp9OpjIMFl6yxQ-kgzdebZclrgXndloxU1Q2aUSkZbmvBvqAZYUJgwWt5h77G-E5IRRsqZ8h1ex30kCDYD52sd4U3xVqHBC7aZIdiG7SLxofpqlpXLCEEP-m3_DXrm70-QLGGyYdz8TiO_hyLzuNfFq90Po8Jbw5HV_y2fe9d_IZujR4jPHzue_S6XGy7n_j5ZfXUPT7joSI8YcpFu-tNu2u1qUDuuADdUNNALtCwSrIsEylaLSUxfdPWRNCa7yjUhvXAeHWPvl9zD8H_OUJMarJxgHHUDvwxKtbwmsqGZGN3NQ7BxxjAqEOwkw5nRYm6sFaZtfrHWuXWKrNWmXWeVl1Y55TFNSVdaCUY9urdH4PLFf8r5y9Wk5Pn</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>28471680</pqid></control><display><type>article</type><title>Characterization of Martensitic Transformation in Ferromagnetic Shape Memory Alloys Co-Ni-Ga Melt-Spun Ribbons</title><source>Scientific.net Journals</source><creator>Li, Yang Xian ; Liu, G.D. ; Dai, X.F. ; Qu, J.P. ; Liu, H.Y. ; Meng, F.B. ; Zhang, M. ; Liu, Z.H. ; Wu, G.H. ; Chen, J.L.</creator><creatorcontrib>Li, Yang Xian ; Liu, G.D. ; Dai, X.F. ; Qu, J.P. ; Liu, H.Y. ; Meng, F.B. ; Zhang, M. ; Liu, Z.H. ; Wu, G.H. ; Chen, J.L.</creatorcontrib><description>The martensitic transformation in Co50Ni20Ga30 ribbon has been characterized in detail by means of X-ray diffraction and magnetic measurements. The sample showed a structural transition from the body-centered cubic with indexed lattice parameters of a=5.743 Å to martensite with a tetragonal structure with lattice parameters of a=b=5.422 Å and c=6.401 Å. (c/a&gt;1). By comparing the results of the diffraction intensity and the magnetic susceptibility measurements, we found that the proceeding of the martensitic transformation can be divided into several different steps during cooling from 283 K to 213 K. During heating from 673 K to 833 K, the peak width became very wide and the intensity became very low. It reveals an order-disorder transformation.</description><identifier>ISSN: 0255-5476</identifier><identifier>ISSN: 1662-9752</identifier><identifier>EISSN: 1662-9752</identifier><identifier>DOI: 10.4028/www.scientific.net/MSF.475-479.2033</identifier><language>eng</language><publisher>Trans Tech Publications Ltd</publisher><ispartof>Materials science forum, 2005-01, Vol.475-479, p.2033-2036</ispartof><rights>2005 Trans Tech Publications Ltd</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c304t-1459dbf9d9af3e6d45ea81f8e4768236259d0659a660fb89705174d1e7f2be243</citedby><cites>FETCH-LOGICAL-c304t-1459dbf9d9af3e6d45ea81f8e4768236259d0659a660fb89705174d1e7f2be243</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Uhttps://www.scientific.net/Image/TitleCover/510?width=600</thumbnail><link.rule.ids>314,780,784,27924,27925</link.rule.ids></links><search><creatorcontrib>Li, Yang Xian</creatorcontrib><creatorcontrib>Liu, G.D.</creatorcontrib><creatorcontrib>Dai, X.F.</creatorcontrib><creatorcontrib>Qu, J.P.</creatorcontrib><creatorcontrib>Liu, H.Y.</creatorcontrib><creatorcontrib>Meng, F.B.</creatorcontrib><creatorcontrib>Zhang, M.</creatorcontrib><creatorcontrib>Liu, Z.H.</creatorcontrib><creatorcontrib>Wu, G.H.</creatorcontrib><creatorcontrib>Chen, J.L.</creatorcontrib><title>Characterization of Martensitic Transformation in Ferromagnetic Shape Memory Alloys Co-Ni-Ga Melt-Spun Ribbons</title><title>Materials science forum</title><description>The martensitic transformation in Co50Ni20Ga30 ribbon has been characterized in detail by means of X-ray diffraction and magnetic measurements. The sample showed a structural transition from the body-centered cubic with indexed lattice parameters of a=5.743 Å to martensite with a tetragonal structure with lattice parameters of a=b=5.422 Å and c=6.401 Å. (c/a&gt;1). By comparing the results of the diffraction intensity and the magnetic susceptibility measurements, we found that the proceeding of the martensitic transformation can be divided into several different steps during cooling from 283 K to 213 K. During heating from 673 K to 833 K, the peak width became very wide and the intensity became very low. It reveals an order-disorder transformation.</description><issn>0255-5476</issn><issn>1662-9752</issn><issn>1662-9752</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2005</creationdate><recordtype>article</recordtype><recordid>eNqVkEFrGzEQhUVoIG6a_7CnXorWklbS7h7DYruBuIHaOQvtehQr7EquJGOcX18ZB3ruYRiY93jD-xD6QUnJCWvmp9OpjIMFl6yxQ-kgzdebZclrgXndloxU1Q2aUSkZbmvBvqAZYUJgwWt5h77G-E5IRRsqZ8h1ex30kCDYD52sd4U3xVqHBC7aZIdiG7SLxofpqlpXLCEEP-m3_DXrm70-QLGGyYdz8TiO_hyLzuNfFq90Po8Jbw5HV_y2fe9d_IZujR4jPHzue_S6XGy7n_j5ZfXUPT7joSI8YcpFu-tNu2u1qUDuuADdUNNALtCwSrIsEylaLSUxfdPWRNCa7yjUhvXAeHWPvl9zD8H_OUJMarJxgHHUDvwxKtbwmsqGZGN3NQ7BxxjAqEOwkw5nRYm6sFaZtfrHWuXWKrNWmXWeVl1Y55TFNSVdaCUY9urdH4PLFf8r5y9Wk5Pn</recordid><startdate>20050115</startdate><enddate>20050115</enddate><creator>Li, Yang Xian</creator><creator>Liu, G.D.</creator><creator>Dai, X.F.</creator><creator>Qu, J.P.</creator><creator>Liu, H.Y.</creator><creator>Meng, F.B.</creator><creator>Zhang, M.</creator><creator>Liu, Z.H.</creator><creator>Wu, G.H.</creator><creator>Chen, J.L.</creator><general>Trans Tech Publications Ltd</general><scope>AAYXX</scope><scope>CITATION</scope><scope>7TB</scope><scope>8BQ</scope><scope>8FD</scope><scope>FR3</scope><scope>JG9</scope></search><sort><creationdate>20050115</creationdate><title>Characterization of Martensitic Transformation in Ferromagnetic Shape Memory Alloys Co-Ni-Ga Melt-Spun Ribbons</title><author>Li, Yang Xian ; Liu, G.D. ; Dai, X.F. ; Qu, J.P. ; Liu, H.Y. ; Meng, F.B. ; Zhang, M. ; Liu, Z.H. ; Wu, G.H. ; Chen, J.L.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c304t-1459dbf9d9af3e6d45ea81f8e4768236259d0659a660fb89705174d1e7f2be243</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2005</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Li, Yang Xian</creatorcontrib><creatorcontrib>Liu, G.D.</creatorcontrib><creatorcontrib>Dai, X.F.</creatorcontrib><creatorcontrib>Qu, J.P.</creatorcontrib><creatorcontrib>Liu, H.Y.</creatorcontrib><creatorcontrib>Meng, F.B.</creatorcontrib><creatorcontrib>Zhang, M.</creatorcontrib><creatorcontrib>Liu, Z.H.</creatorcontrib><creatorcontrib>Wu, G.H.</creatorcontrib><creatorcontrib>Chen, J.L.</creatorcontrib><collection>CrossRef</collection><collection>Mechanical &amp; Transportation Engineering Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Engineering Research Database</collection><collection>Materials Research Database</collection><jtitle>Materials science forum</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Li, Yang Xian</au><au>Liu, G.D.</au><au>Dai, X.F.</au><au>Qu, J.P.</au><au>Liu, H.Y.</au><au>Meng, F.B.</au><au>Zhang, M.</au><au>Liu, Z.H.</au><au>Wu, G.H.</au><au>Chen, J.L.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Characterization of Martensitic Transformation in Ferromagnetic Shape Memory Alloys Co-Ni-Ga Melt-Spun Ribbons</atitle><jtitle>Materials science forum</jtitle><date>2005-01-15</date><risdate>2005</risdate><volume>475-479</volume><spage>2033</spage><epage>2036</epage><pages>2033-2036</pages><issn>0255-5476</issn><issn>1662-9752</issn><eissn>1662-9752</eissn><abstract>The martensitic transformation in Co50Ni20Ga30 ribbon has been characterized in detail by means of X-ray diffraction and magnetic measurements. The sample showed a structural transition from the body-centered cubic with indexed lattice parameters of a=5.743 Å to martensite with a tetragonal structure with lattice parameters of a=b=5.422 Å and c=6.401 Å. (c/a&gt;1). By comparing the results of the diffraction intensity and the magnetic susceptibility measurements, we found that the proceeding of the martensitic transformation can be divided into several different steps during cooling from 283 K to 213 K. During heating from 673 K to 833 K, the peak width became very wide and the intensity became very low. It reveals an order-disorder transformation.</abstract><pub>Trans Tech Publications Ltd</pub><doi>10.4028/www.scientific.net/MSF.475-479.2033</doi><tpages>4</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0255-5476
ispartof Materials science forum, 2005-01, Vol.475-479, p.2033-2036
issn 0255-5476
1662-9752
1662-9752
language eng
recordid cdi_proquest_miscellaneous_28471680
source Scientific.net Journals
title Characterization of Martensitic Transformation in Ferromagnetic Shape Memory Alloys Co-Ni-Ga Melt-Spun Ribbons
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-20T12%3A20%3A24IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Characterization%20of%20Martensitic%20Transformation%20in%20Ferromagnetic%20Shape%20Memory%20Alloys%20Co-Ni-Ga%20Melt-Spun%20Ribbons&rft.jtitle=Materials%20science%20forum&rft.au=Li,%20Yang%20Xian&rft.date=2005-01-15&rft.volume=475-479&rft.spage=2033&rft.epage=2036&rft.pages=2033-2036&rft.issn=0255-5476&rft.eissn=1662-9752&rft_id=info:doi/10.4028/www.scientific.net/MSF.475-479.2033&rft_dat=%3Cproquest_cross%3E28471680%3C/proquest_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=28471680&rft_id=info:pmid/&rfr_iscdi=true