Development and characterisation of SiAlON composites with TiB2, TiN, TiC and TiCN

30 vol% of TiB₂, TiCN, TiN or TiC was added to a sialon matrix with an X-phase sialon (Si₁₂Al₁₈O₃₉N₈) and an Al₂O₃−Si₃N₄ (77/23 wt%) starting powder composition and hot pressed at 1650°C in vacuum. The microstructures of the obtained composites were characterised by means of X-ray diffraction and el...